摘要
As the regularity of strength of C/SiC composites with elevating temperature is obscure, the mini-composite C/SiC is applied in present investigation for this purpose. The C/SiC mini-composite specimen is fabricated with T300PAN carbon fiber, its work section contains one fiber yam tow and the other part six tows. The tensile experiments of mini-composites are carried out in vacuum around 10(-5) torr from room temperature to 1700 degrees C. Tensile strength of mini-composites in the range around 900-1300 degrees C is higher than that at other temperature. In strong interface bonding condition, fibers' strength decrement of mini-composite mainly attributes to the internal thermo-stress induced by expansion coefficient mismatch between carbon fiber and SiC matrix, and the stress concentration generated by SiC matrix crack. The stress concentration coefficient is 3.59 by matrix crack for C/SiC mini-composites. At 1300 degrees C, mini-composite's strength Weibull modulus is 3.65. In the fracture surface of mini-composite, the fiber fracture mirror has not been found very clear.
引用
收藏
页码:435 / 439
页数:5
相关论文
共 50 条
  • [31] Test of mechanical properties of C/SiC composites at elevated temperature air
    Chen, Weihua
    Wang, Liyan
    Zhang, Hanyi
    Ji, Nizhi
    Li, Guanshu
    Ma, Jing
    Guofang Keji Daxue Xuebao/Journal of National University of Defense Technology, 2021, 43 (06): : 26 - 32
  • [32] Fracture Characteristics of C/SiC Composites for Rocket Nozzle at Elevated Temperature
    Yoon, Dong Hyun
    Lee, Jeong Won
    Kim, Jae Hoon
    Sihn, Ihn Cheol
    Lim, Byung Joo
    TRANSACTIONS OF THE KOREAN SOCIETY OF MECHANICAL ENGINEERS A, 2016, 40 (11) : 927 - 933
  • [33] Effect of porosity on the tensile strength and Micromechanisms of laminated stitched C/C-SiC composites
    Song, Zhuoyu
    Xiao, Kaiyin
    Xiao, Shijian
    Du, Kaifan
    Mao, Zebei
    Li, Tong
    Wang, Bo
    MATERIALS & DESIGN, 2024, 247
  • [34] Tensile strength at elevated temperature and its applicability as an accelerated testing methodology for unidirectional composites
    Koyanagi, Jun
    Nakada, Masayuki
    Miyano, Yasushi
    MECHANICS OF TIME-DEPENDENT MATERIALS, 2012, 16 (01) : 19 - 30
  • [35] Tensile strength at elevated temperature and its applicability as an accelerated testing methodology for unidirectional composites
    Jun Koyanagi
    Masayuki Nakada
    Yasushi Miyano
    Mechanics of Time-Dependent Materials, 2012, 16 : 19 - 30
  • [36] Influence of heat treatment on microstructure and mechanical properties of Cansas-II SiC/PyC/CVI-SiC mini-composites
    Han, Xiao
    Chen, Xihui
    Ding, Junjie
    Wu, Weijing
    Sun, Zhigang
    Song, Yingdong
    CERAMICS INTERNATIONAL, 2022, 48 (01) : 1077 - 1089
  • [37] Detailed study of interphase degradation in SiC/BN/SiC ceramic matrix composites after elevated temperature tensile testing
    Toller-Nordstrom, L. R. M.
    Gavalda-Diaz, O.
    Gale, L.
    Armstrong, D. E. J.
    Nicholls, R. J.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (04)
  • [38] Intermediate temperature strength degradation in SiC/SiC composites
    Morscher, GN
    Cawley, JD
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (14-15) : 2777 - 2787
  • [39] Tensile behavior of 2D-C/SiC composites at elevated temperatures: Experiment and modeling
    Yang, C. -P.
    Zhang, L.
    Wang, B.
    Huang, T.
    Jiao, G. -Q.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (04) : 1281 - 1290
  • [40] Gas leak tightness of SiC/SiC composites at elevated temperature
    Hayasaka, Daisuke
    Park, Joon-Soo.
    Kishimoto, Hirotatsu
    Kohyama, Akira
    FUSION ENGINEERING AND DESIGN, 2016, 109 : 1498 - 1501