Suppression of pesting failure in MoSi2 film by doping of Si

被引:8
作者
Yu, Xiuhan [1 ]
Li, Fengji [1 ]
Shi, Xunwang [1 ]
Sun, Deen [1 ]
Wang, Jinbiao [2 ]
Zhang, Sam [1 ]
机构
[1] Southwest Univ, Ctr Adv Thin Films & Devices, Sch Mat & Energy, 2 Tiansheng Rd, Chongqing 400715, Peoples R China
[2] Chongqing Univ Arts & Sci, Chongqing Key Lab Mat Surface & Interface Sci, Chongqing 402160, Peoples R China
关键词
Pesting; Oxidation; Magnetron sputtering; Thermal annealing; Silicon dioxides; HIGH-TEMPERATURE OXIDATION; COMPOSITE COATINGS; BEHAVIOR; MICROSTRUCTURE; RESISTANCE; DEPOSITION; MECHANISM; CR2ALC;
D O I
10.1016/j.surfcoat.2021.128016
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
MoSi2 usually suffers pesting failure at 400- 700 degrees C due to severe oxidation of Mo, which has been a great hindrance for industrial applications. To address this issue, this work grew MoSi2(Si) thin films via magnetron cosputtering of a Si single element target and a MoSi2 compound target on Si wafer substrates at room temperature, followed by annealing at 950 degrees C in an argon atmosphere. The as-annealed thin films were heated in a muffle furnace at 700 degrees C in air to experience different duration of oxidation. After that, the oxidation resistance was evaluated by examining the thickness, morphology, structure and composition of the as-heated thin films using field emission scanning electron microscopy and X-ray diffraction, respectively. In comparison with the MoSi2 without doping of Si, the MoSi2(Si) film is denser and exhibits a C11b crystalline structure with a smaller crystal size of 30 nm. The oxidation of Mo is effectively inhibited. There is no big bulge on the film surface after 1 h oxidation. But the oxidation of Si is severe, resulting in the continuous growth of grey SiO2 layer which help preventing the further oxidation of Mo. SiO2 islands are observed after oxidation for 9 h. The early pesting sites gradually become healed by the grown SiO2 layer during oxidation for 60 h. The mechanism for suppressing the pesting failure of MoSi2 by Si doping is discussed in details. A model is developed to explain the process.
引用
收藏
页数:12
相关论文
共 32 条
[21]  
VASUDEVAN AK, 1992, MAT SCI ENG A-STRUCT, V155, pR5
[22]   A COMPARATIVE OVERVIEW OF MOLYBDENUM DISILICIDE COMPOSITES [J].
VASUDEVAN, AK ;
PETROVIC, JJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 155 (1-2) :1-17
[23]   A novel gradient SiC-ZrB2-MoSi2 coating for SiC coated C/C composites by supersonic plasma spraying [J].
Wang Lu ;
Fu Qian-gang ;
Zhao Feng-ling .
SURFACE & COATINGS TECHNOLOGY, 2017, 313 :63-72
[24]   The calibration of Debye-Scherrer x-ray powder cameras [J].
Wilson, AJC ;
Lipson, H .
PROCEEDINGS OF THE PHYSICAL SOCIETY, 1941, 53 :245-250
[25]   HIGH-TEMPERATURE OXIDATION OF MOLYBDENUM DISILICIDE [J].
WIRKUS, CD ;
WILDER, DR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1966, 49 (04) :173-&
[26]   Magnetron sputter deposition of zirconium-silicide coating for mitigating high temperature oxidation of zirconium-alloy [J].
Yeom, Hwasung ;
Maier, Benjamin ;
Mariani, Robert ;
Bai, David ;
Fronek, Steven ;
Xu, Peng ;
Sridharan, Kumar .
SURFACE & COATINGS TECHNOLOGY, 2017, 316 :30-38
[27]   Microstructure and oxidation protection of a MoSi2/SiO2-B2O3-Al2O3 coating for SiC-coated carbon/carbon composites [J].
Yong, Xiang ;
Cao, Liyun ;
Huang, Jianfeng ;
Kong, Weihua ;
Su, Jinbu ;
Li, Cuiyan ;
Ouyang, Haibo ;
Zhou, Lei ;
Liu, Jintao .
SURFACE & COATINGS TECHNOLOGY, 2017, 311 :63-69
[28]   Low-temperature cyclic oxidation behavior of MoSi2/Si3N4 nanocomposite coating formed on Mo substrate at 773 K [J].
Yoon, JK ;
Kim, GH ;
Han, JH ;
Shon, IJ ;
Doh, JM ;
Hong, KT .
SURFACE & COATINGS TECHNOLOGY, 2005, 200 (07) :2537-2546
[29]   Formation of MOSi2-SiC composite coatings by chemical vapor deposition of Si on the surface of MO2C layer formed by carburizing of Mo substrate [J].
Yoon, JK ;
Doh, JM ;
Byun, JY ;
Kim, GH ;
Lee, JK ;
Hong, KT .
SURFACE & COATINGS TECHNOLOGY, 2003, 173 (01) :39-46
[30]   Effect of mullite on the microstructure and oxidation behavior of thermal-sprayed MoSi2 coating at 1500 °C [J].
Zhang, Guangpeng ;
Sun, Jia ;
Fu, Qiangang .
CERAMICS INTERNATIONAL, 2020, 46 (08) :10058-10066