Suppression of Phase Transformation in Nb-H Thin Films below Switchover Thickness

被引:26
作者
Burlaka, Vladimir [1 ]
Wagner, Stefan [1 ]
Hamm, Magnus [1 ]
Pundt, Astrid [1 ]
机构
[1] Univ Gottingen, Inst Mat Phys, Friedrich Hund Pl 1, D-37077 Gottingen, Germany
关键词
Thin films; hydrogen; phase transformation; STM; hydride phase; finite size effect; SIZE DEPENDENCE; HYDROGEN; NANOPARTICLES; SOLUBILITY; PD; NANOCRYSTALS; CLUSTERS; HYDRIDE; LAYERS;
D O I
10.1021/acs.nanolett.6b02467
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Hydrogen uptake in metal hydrogen (M-H) nanosized systems (e.g., thin films, clusters) is both a fundamental and a technologically relevant topic, which is becoming more important due to the recent developments of hydrogen sensors, purification membranes, and hydrogen storage solutions. It was recently shown that hydrogen (H) absorption in nanosized systems adhered to rigid substrates can lead to ultrahigh mechanical stress in the GPa range. About -10 GPa (compressive) stress were reported for hydrogen loaded niobium (Nb) thin films. Such high stresses can be achieved when conventional stress-release channels are closed, e.g., by reducing the system size. In this paper, we demonstrate that the high stress can be used to strongly modify the system's thermodynamics. In particular, a complete suppression of the phase transformation is achieved by reducing the film thickness below a switchover value d(so). Combined in situ scanning tunneling microscopy (STM) and in situ X-ray diffraction (XRD) measurements serve to determine the switchover thickness of epitaxial Nb/Al2O3 films in the thickness range from 55 to 5 rim. A switchover thickness d(so) = 9 +/- 1 nm is found at T = 294 K. This result is supported by complementary methods such as electromotive force (EMF), electrical resistance, and mechanical stress measurements in combination with theoretical modeling.
引用
收藏
页码:6207 / 6212
页数:6
相关论文
共 32 条
[1]   Influence of compressive biaxial strain on the hydrogen uptake of ultrathin single-crystal vanadium layers [J].
Andersson, G ;
Hjorvarsson, B ;
Isberg, P .
PHYSICAL REVIEW B, 1997, 55 (03) :1774-1781
[2]  
[Anonymous], 2008, Hydrogen as a Future Energy Carrier
[3]  
Baldi A, 2014, NAT MATER, V13, P1143, DOI [10.1038/NMAT4086, 10.1038/nmat4086]
[4]  
Bardhan R, 2013, NAT MATER, V12, P905, DOI [10.1038/NMAT3716, 10.1038/nmat3716]
[5]   Size effects on the hydrogen storage properties of nanostructured metal hydrides:: A review [J].
Berube, Vincent ;
Radtke, Gregg ;
Dresselhaus, Mildred ;
Chen, Gang .
INTERNATIONAL JOURNAL OF ENERGY RESEARCH, 2007, 31 (6-7) :637-663
[6]   Formation of Self-Assembled Nanoplates via Hydrogenation of Epitaxial Pd Film [J].
Boyerinas, Brad M. ;
Roythurd, Alexander L. ;
Bruck, Hugh A. .
NANO LETTERS, 2014, 14 (04) :1818-1822
[7]   In-situ STM and XRD studies on Nb-H films: Coherent and incoherent phase transitions [J].
Burlaka, Vladimir ;
Wagner, Stefan ;
Pundt, Astrid .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 645 :S388-S391
[8]   Review of hydrogen storage techniques for on board vehicle applications [J].
Durbin, D. J. ;
Malardier-Jugroot, C. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (34) :14595-14617
[9]   A fresh look at an old nano-technology: catalysis [J].
Freund, H. -J. ;
Nilius, N. ;
Risse, T. ;
Schauermann, S. .
PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2014, 16 (18) :8148-8167
[10]  
Fukai Y., 1993, Springer Series in Material Science, V21