Effect of sol aging time on the wear properties of TiO2-SiO2 composite films prepared by a sol-gel method

被引:31
作者
Yazici, M. [1 ]
Comakli, O. [2 ]
Yetim, T. [3 ]
Yetim, A. F. [4 ]
Celik, A. [2 ]
机构
[1] Erzurum Tech Univ, High Technol Res Ctr, Erzurum, Turkey
[2] Ataturk Univ, Fac Engn, Dept Mech Engn, Erzurum, Turkey
[3] Erzurum Tech Univ, Fac Engn & Architecture, Dept Chem Engn, Erzurum, Turkey
[4] Erzurum Tech Univ, Fac Engn & Architecture, Dept Mech Engn, Erzurum, Turkey
关键词
Sol-gel; Composite film; Sol aging time; TiO2-SiO2; coating; ZNO THIN-FILMS; TRIBOLOGICAL PROPERTIES; OPTICAL-PROPERTIES; TITANIUM-ALLOYS; COATINGS; BEHAVIOR; TIO2;
D O I
10.1016/j.triboint.2016.08.041
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
TiO2-SiO2 composite films were deposited on commercially pure titanium (Cp-Ti) substrate with composite sols of different aging times (unaged, 1, 3,10 weeks) by a sol gel method. The effects of aging time on the structural, mechanical and wear properties of composite coatings were investigated using pin-on-disk tribotester. The structure of composite coatings was analyzed with XRD and SEM. The wear volume of TiO2-SiO2 composite films were investigated with 3D profilometer. Tribological properties of the composite films were significantly influenced by aging time. Composite coatings prepared from unaged sol showed the best wear resistance. This may be attributed to their high surface hardness, low surface roughness and self-lubricant phase structure. It was observed that increasing aging time led to increase the grain size. It was obtained that the wear volume values increased with increasing aging time. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:175 / 182
页数:8
相关论文
共 32 条
  • [1] [Anonymous], 2010, G99 ASTM INT
  • [2] Surface modification of titanium alloys for combined improvements in corrosion and wear resistance
    Bloyce, A
    Qi, PY
    Dong, H
    Bell, T
    [J]. SURFACE & COATINGS TECHNOLOGY, 1998, 107 (2-3) : 125 - 132
  • [3] TRIBOLOGICAL PROPERTIES OF TITANIUM-ALLOYS
    BUDINSKI, KG
    [J]. WEAR, 1991, 151 (02) : 203 - 217
  • [4] Failure mode maps in the thin film scratch adhesion test
    Bull, SJ
    [J]. TRIBOLOGY INTERNATIONAL, 1997, 30 (07) : 491 - 498
  • [5] The effect of calcination temperatures on wear properties of TiO2 coated CP-Ti
    Comakli, O.
    Yetim, T.
    Celik, A.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 246 : 34 - 39
  • [6] The evolution of 'sol-gel' chemistry as a technique for materials synthesis
    Danks, A. E.
    Hall, S. R.
    Schnepp, Z.
    [J]. MATERIALS HORIZONS, 2016, 3 (02) : 91 - 112
  • [7] Formation of Al3Ti and Al2O3 from an Al-TiO2 system for preparing in-situ aluminium matrix composites
    Feng, CF
    Froyen, L
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2000, 31 (04) : 385 - 390
  • [8] Sol-gel derived TiO2 coating on plasma nitrided 316L stainless steel
    Fu, T.
    Wen, C. S.
    Lu, J.
    Zhou, Y. M.
    Ma, S. G.
    Dong, B. H.
    Liu, B. G.
    [J]. VACUUM, 2012, 86 (09) : 1402 - 1407
  • [9] Experimental study of plasma nitriding dental implant surfaces
    Guerra Neto, C. L. B.
    da Silva, M. A. M.
    Alves, C., Jr.
    [J]. SURFACE ENGINEERING, 2009, 25 (06) : 430 - 433
  • [10] Kerkwijk B., 1999, WEAR FRICTION NANOST