Thermal characterization of the interaction of poly(3-hydroxybutyrate) with maleic anhydride

被引:1
作者
Souza, J. L. [1 ]
Santos, A. F. [1 ]
Crespi, M. S. [1 ]
Ribeiro, C. A. [1 ]
机构
[1] Univ Estadual Paulista UNESP, Inst Quim, Araraquara, SP, Brazil
关键词
Transesterification reaction; Poly(3-hydroxybutyrate); Maleic anhydride; POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYHEXANOATE); DEGRADATION; PHB;
D O I
10.1007/s10973-011-1706-3
中图分类号
O414.1 [热力学];
学科分类号
摘要
Poly(3-hydroxybutyrate), PHB, has been structurally modified with maleic anhydride, MA, in the presence of triethylamine, TEA. Glass transition, melting, and crystallization temperature, obtained from DSC curves, and thermal degradation temperatures obtained from TG ones, were employed to evaluate the influence of the MA proportion on the modification in the PHB chain. According to the results, most of chain modification reactions are the 80/20 and 90/10 proportions. Observations suggest that most chain modification reactions occur when the ratio of PHB/MA is 80/20 or 90/10. This suggests that modifications of PHB in the presence of MA involve main chain scission.
引用
收藏
页码:453 / 458
页数:6
相关论文
共 23 条
[1]   Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide] [J].
Aoyagi, Y ;
Yamashita, K ;
Doi, Y .
POLYMER DEGRADATION AND STABILITY, 2002, 76 (01) :53-59
[2]  
Budavari S, 2001, MERCK INDEX NAB ENCY, P1552
[3]   Biodegradable polymers [J].
Chandra, R ;
Rustgi, R .
PROGRESS IN POLYMER SCIENCE, 1998, 23 (07) :1273-1335
[4]   Production and evaluation of biodegradable composites based on PHB-PHV copolymer [J].
Chen, LJ ;
Wang, M .
BIOMATERIALS, 2002, 23 (13) :2631-2639
[5]  
Dawes E. A., 1973, ROLE REGULATION ENER
[6]  
Gomez J. G. C., 1997, REV BRAS ENG QUIM, V17, P24
[7]   Crystallisation of poly(3-hydroxybutyrate)/polyvinyl acetate blends [J].
Hay, JN ;
Sharma, L .
POLYMER, 2000, 41 (15) :5749-5757
[8]   Thermal degradation of plasticized poly(3-hydroxybutyrate) investigated by DSC [J].
Janigová, I ;
Lacík, I ;
Chodák, I .
POLYMER DEGRADATION AND STABILITY, 2002, 77 (01) :35-41
[9]   DEVELOPMENT OF A DEGRADABLE COMPOSITE FOR ORTHOPEDIC USE - INVIVO BIOMECHANICAL AND HISTOLOGICAL-EVALUATION OF 2 BIOACTIVE DEGRADABLE COMPOSITES BASED ON THE POLYHYDROXYBUTYRATE POLYMER [J].
KNOWLES, JC ;
HASTINGS, GW ;
OHTA, H ;
NIWA, S ;
BOEREE, N .
BIOMATERIALS, 1992, 13 (08) :491-496
[10]   Mechanistic aspects of the thermal degradation of poly(lactic acid) and poly(beta-hydroxybutyric acid) [J].
Kopinke, FD ;
Mackenzie, K .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1997, 40-1 :43-53