Fabrication, microstructural characterization and mechanical properties evaluation of Ti/TiB/TiB2 composite coatings deposited on Ti6Al4V alloy by electro-spark deposition method

被引:30
作者
Shafyei, Hassan [1 ]
Salehi, Mehdi [2 ]
Bahrami, Abbas [2 ]
机构
[1] Isfahan Univ Technol, Pardis Coll, Mat Engn Grp, Esfahan 8415683111, Iran
[2] Isfahan Univ Technol, Dept Mat Engn, Esfahan 8415683111, Iran
关键词
Ti/TiB/TiB2 MMC coating; Microstructural; Mechanical properties; Electro-spark deposition; SHS process; Ti6Al4V; TITANIUM-ALLOY; WEAR BEHAVIOR; TIB2;
D O I
10.1016/j.ceramint.2020.03.068
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, briquettes of Ti-TiB-TiB2 composite were produced by mixing Ti and B powders, performing self-propagating high-temperature synthesis process and by applying hydrostatic pressure on the reaction products with a high-capacity press. Ti-TiB-TiB2 was then coated to Ti6Al4V substrate by Electro-Spark Deposition (ESD) technique under two atmospheres of air and argon, single and double-layer coatings and in two energy levels of 40 W and 110 W as input powers. Coatings microstructure were examined by Scanning Electron Microscope (SEM) equipped with Energy Dispersive Spectroscopy (EDS) analyzer. Comparison of the coatings microstructure with the electrode microstructure shows that the coatings have a much finer microstructure than that of the electrode due mainly to the high solidification rate in the ESD process. Microstructural observations also revealed that the main phases in the coatings are needle-shaped TiB and particle-shaped TiB2 in the Ti matrix. The coating microstructure was much finer due to an increase in solidification rate by reducing the input power from 110 to 40 W. In such a situation, two phases of TiB2 and TiB with nanometer sizes were scattered in the Ti matrix. Also, due to the trapping of the gases in low input power of 40 W, a limited number of very small gas pores was created in the microstructure. Interface examination of the coating and the substrate by the Line Scan and X-ray Image show a good coherence of the coating with the substrate. Adhesion results showed that the bond strength between the coating and the substrate was higher than 50 MPa in all coatings. No crack was observed in the coatings after bending tests which were performed, in accordance with the intended standard, on the samples around a mandrel. The hardness of all coatings was increased with decreasing the input energy from 110 to 40 W.
引用
收藏
页码:15276 / 15284
页数:9
相关论文
共 29 条
[1]  
Amuda MOH, 2017, MATER TODAY-PROC, V4, P763, DOI 10.1016/j.matpr.2017.01.084
[2]  
[Anonymous], 1992, ASM Handbook, V3, P324
[3]   Synthesis and sintering of TiB2 and TiB2-TiC composite under high pressure [J].
Bhaumik, SK ;
Divakar, C ;
Singh, AK ;
Upadhyaya, GS .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 279 (1-2) :275-281
[4]   Formation of amorphous Zr41.2Ti13.8Ni10Cu12.5Be22.5 coatings via the ElectroSpark Deposition process [J].
Cadney, S. ;
Brochu, M. .
INTERMETALLICS, 2008, 16 (04) :518-523
[5]   The transformation of an Al-based crystalline electrode material to an amorphous deposit via the electrospark welding process [J].
Cadney, S. ;
Goodall, G. ;
Kim, G. ;
Moran, Angela ;
Brochu, M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 476 (1-2) :147-151
[6]   Wear behaviour of coated carbide tools during machining of Ti6Al4V aerospace alloy associated with strong built up edge formation [J].
Chowdhury, M. S. I. ;
Chowdhury, S. ;
Yamamoto, K. ;
Beake, B. D. ;
Bose, B. ;
Elfizy, A. ;
Cavelli, D. ;
Dosbaeva, G. ;
Aramesh, M. ;
Fox-Rabinovich, G. S. ;
Veldhuis, S. C. .
SURFACE & COATINGS TECHNOLOGY, 2017, 313 :319-327
[7]   Biotribological properties of Ti/TiB2 multilayers in simulated body solution [J].
Ding, Hongyan ;
Zhou, Guanghong ;
Liu, Tao ;
Xia, Mujian ;
Wang, Xiangming .
TRIBOLOGY INTERNATIONAL, 2015, 89 :62-66
[8]   Production of amorphous and nanocrystalline iron based coatings by electro-spark deposition process [J].
Hasanabadi, M. Fakoori ;
Ghaini, F. Malek ;
Ebrahimnia, M. ;
Shahverdi, H. R. .
SURFACE & COATINGS TECHNOLOGY, 2015, 270 :95-101
[9]   Development of a nanostructure microstructure in the Al-Ni system using the electrospark deposition process [J].
Heard, D. W. ;
Brochu, M. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2010, 210 (6-7) :892-898
[10]   Effects of process parameters on microstructure and wear resistance of TiN coatings deposited on TC11 titanium alloy by electrospark deposition [J].
Hong, Xiang ;
Feng, Ke ;
Tan, Ye-fa ;
Wang, Xiao-long ;
Tan, Hua .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (08) :1767-1776