Tribological Characterization of SiC and B4C Manufactured by Plasma Pressure Compaction

被引:19
作者
Rubino, Felice [1 ]
Pisaturo, Mario [1 ]
Senatore, Adolfo [1 ]
Carlone, Pierpaolo [1 ]
Sudarshan, Tirumalai S. [2 ]
机构
[1] Univ Salerno, Dept Ind Engn, Via Giovanni Paolo 2, Fisciano, SA, Italy
[2] Mat Modificat Inc, 2809K Merrilee Dr, Fairfax, VA USA
关键词
boron carbide; coefficient of friction; silicon carbide; wear; SILICON-CARBIDE CERAMICS; BORON-CARBIDE; MECHANICAL-PROPERTIES; OXIDATION BEHAVIOR; FRACTURE-TOUGHNESS; HIGH-TEMPERATURE; GRAIN-GROWTH; WEAR; FRICTION; HARDNESS;
D O I
10.1007/s11665-017-3016-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The objective of the present study was to assess the tribological properties and the wear behavior of silicon carbide and boron carbide ceramics, produced by the plasma pressure compaction sintering process. Reciprocating sliding tests were executed to evaluate the tribological behavior of silicon carbide and boron carbide. Samples of each material with distinct values of surface roughness Ra were tested. Wear mass loss, coefficients of friction and wear mechanism of the boron carbide and silicon carbide were evaluated by means of microscopes and an energy-dispersive spectroscopy probe. The coefficient of friction of the evaluated boron carbide was found to be 0.8, and the surface roughness affects only the starting transient, while for silicon carbide the steady-state value ranges from 0.5 to 0.8 depending on the roughness value Ra.
引用
收藏
页码:5648 / 5659
页数:12
相关论文
共 57 条
[1]   PRESSURE-SINTERED SILICON CARBIDE [J].
ALLIEGRO, RA ;
COFFIN, LB ;
TINKLEPAUGH, JR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1956, 39 (11) :386-389
[2]  
Angers R., 1984, Ceramics International, V10, P49, DOI 10.1016/0272-8842(84)90025-7
[3]  
[Anonymous], 1995, 9832008 ISOIEC
[4]  
[Anonymous], 2016, G13305 ASTM
[5]   Microtribological modification of silicon carbide surface by laser irradiation [J].
Aono, Yuko ;
Ando, Shotaro ;
Hirata, Atsushi .
PRECISION ENGINEERING-JOURNAL OF THE INTERNATIONAL SOCIETIES FOR PRECISION ENGINEERING AND NANOTECHNOLOGY, 2016, 43 :270-276
[6]  
ASTM, G9917 ASTM
[7]   Mechanical behaviour at high temperature of spark plasma sintered boron carbide ceramics [J].
Belon, R. ;
Antou, G. ;
Pradeilles, N. ;
Maitre, A. ;
Gosset, D. .
CERAMICS INTERNATIONAL, 2017, 43 (08) :6631-6635
[8]   Design of Experiment Approach for Sintering Study of Nanocrystalline SiC Fabricated Using Plasma Pressure Compaction [J].
Bothara, M. G. ;
Vijay, P. ;
Atre, S. V. ;
Park, S. -J. ;
German, R. M. ;
Sudarshan, T. S. ;
Radhakrishnan, R. .
SCIENCE OF SINTERING, 2009, 41 (02) :125-133
[9]   Sintering Behavior of Nanocrystalline Silicon Carbide Using a Plasma Pressure Compaction System: Master Sintering Curve Analysis [J].
Bothara, Manish G. ;
Atre, Sundar V. ;
Park, Seong-Jin ;
German, Randall M. ;
Sudarshan, T. S. ;
Radhakrishnan, R. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (12) :3252-3261
[10]  
Cengiz M., 2014, ACTA PHYS POLONICA A, V125