Pure copper components fabricated by cold spray (CS) and selective laser melting (SLM) technology

被引:88
作者
Huang, Jian [1 ]
Yan, Xingchen [1 ,2 ]
Chang, Cheng [3 ]
Xie, Yingchun [1 ]
Ma, Wenyou [1 ]
Huang, Renzhong [1 ]
Zhao, Ruimin [4 ]
Li, Shunhua [4 ]
Liu, Min [1 ]
Liao, Hanlin [2 ]
机构
[1] Guangdong Inst New Mat, Natl Engn Lab Modern Mat Surface Engn Technol, Key Lab Guangdong Modern Surface Engn Technol, Guangzhou 510651, Peoples R China
[2] Univ Bourgogne Franche Comte, UTBM, CNRS, ICB,UMR 6303, F-90010 Belfort, France
[3] Univ Technol Troyes, CNRS, ICD LASMIS, UMR 6281, 12 Rue Marie Curie, F-10004 Troyes, France
[4] Yunnan Yunlu Yongxin Co Ltd, Honghe 654300, Peoples R China
关键词
Selective laser melting; Pure copper; Cold spraying; Microstructure evolution; Mechanical property; MICROSTRUCTURE CHARACTERIZATION; MECHANICAL-PROPERTIES; METAL-MATRIX; ATOMIZATION; COMPOSITES; DEPOSITION; STRENGTH;
D O I
10.1016/j.surfcoat.2020.125936
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To study effect of the different metal additive manufacturing techniques on microstructural evolution, phase constitution and the relationship between the microstructure and tensile behavior of pure Cu parts, components were manufactured by selective laser melting (SLM) technology and cold spraying (CS) technology, respectively. The microstructure of Cu parts was detected using an optical microscope (OM) and scanning electron microscopy (SEM). The XRD spectrum revealed that only Cu phase is formed in the SLM Cu and CS Cu samples. The microstructure of the SLM Cu samples is constituted by the polycrystalline grains with substructures including the columnar dendrites and the equiaxed structures. As for the CS Cu samples, only the equiaxed grains were detected. In terms of the main physical properties, the averaged electrical conductivity of SLM Cu sample is 41% IACS, while that of CS Cu sample is 73% IACS. For the microhardness, the mean microhardness value of the CS Cu and the SLM Cu samples is 144.2 +/- 4.3 HV0.05 and 83.6 +/- 5.2 HV0.05, respectively. With regard to the statistic mechanical properties, the yield strength (YS) and ultimate tensile strength (UTS) of the SLM Cu part is approximately 185.8 +/- 6.1 MPa and 242.2 +/- 8.2 MPa, respectively.
引用
收藏
页数:10
相关论文
共 41 条
  • [1] Alexander L., 1989, POWDER DIFFR, V4, P66, DOI [10.1017/S0885715600016432, DOI 10.1017/S0885715600016432]
  • [2] [Anonymous], 1990, ASM Handbook, V1, DOI [10.31399/asm.hb.v01.9781627081610, DOI 10.31399/ASM.HB.V01.9781627081610]
  • [3] [Anonymous], 1990, ASM HDB, DOI DOI 10.1007/S004310050884
  • [4] [Anonymous], COLD SPRAY TECHNOLOG
  • [5] [Anonymous], 2015, COPPER ELECT CONDUCT
  • [6] [Anonymous], ASM SPEC HDB COPP CO
  • [7] Cold spraying - A materials perspective
    Assadi, H.
    Kreye, H.
    Gaertner, F.
    Klassen, T.
    [J]. ACTA MATERIALIA, 2016, 116 : 382 - 407
  • [8] Design and analysis of additive manufactured bimodal structures obtained by cold spray deposition
    Bagherifard, Sara
    Astaraee, Asghar Heydari
    Locati, Matteo
    Nawaz, Ali
    Monti, Stefano
    Kondas, Jan
    Singh, Reeti
    Guagliano, Mario
    [J]. ADDITIVE MANUFACTURING, 2020, 33
  • [9] Influence of post-heat treatments on the mechanical properties of CX stainless steel fabricated by selective laser melting
    Chang, Cheng
    Yan, Xingchen
    Bolot, Rodolphe
    Gardan, Julien
    Gao, Shuohong
    Liu, Min
    Liao, Hanlin
    Chemkhi, Mandi
    Deng, Sihao
    [J]. JOURNAL OF MATERIALS SCIENCE, 2020, 55 (19) : 8303 - 8316
  • [10] Effects of substrate heat accumulation on the cold sprayed Ni coating quality: Microstructure evolution and tribological performance
    Chen, Chaoyue
    Xie, Yingchun
    Xie, Xinliang
    Yan, Xingchen
    Huang, Renzhong
    Wang, Jiang
    Ren, Zhongming
    Deng, Sihao
    Liao, Hanlin
    [J]. SURFACE & COATINGS TECHNOLOGY, 2019, 371 : 185 - 193