The mechanical properties and microstructure of nitrided tetragonal zirconia polycrystals doped with yttria (Y-TZP) have been evaluated. It has been established that a surface layer is formed during nitriding at 1650 degreesC for 5 min, 1 and 2 h. Such layer exhibits a gradient in grain size, which results in a variation in the capacity of the material to undergo a stress assisted tetragonal to monoclinic (t-m) phase transformation together with a build up of residual stresses. After nitriding for 1 h, the outer surface forms non-transformable t' phase, which protects the material from low temperature ageing degradation. It is shown that, in contrast with the original Y-TZP, the nitrided surface does not transform in the presence of water at 100 degreesC during time periods of up to 900 h. By contrast, nitrided Y-TZP is not stable after exposure in air at temperatures of 600 and 800 degreesC, since t-m transformation Occurs in a subsurface layer of the nitrided rods, and this induces high internal stresses. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2955 / 2962
页数:8
相关论文
共 16 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]   On the transformation toughening of Y-ZrO2 ceramics with mixed Y-TZP/PSZ microstructures [J].
Casellas, D ;
Cumbrera, FL ;
Sánchez-Bajo, F ;
Forsling, W ;
Llanes, L ;
Anglada, M .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2001, 21 (06) :765-777
[3]   Fracture toughness and mechanical strength of Y-TZP/PSZ ceramics [J].
Casellas, D ;
Feder, A ;
Llanes, L ;
Anglada, M .
SCRIPTA MATERIALIA, 2001, 45 (02) :213-220
[4]   ROLE OF ANION VACANCIES IN NITROGEN-STABILIZED ZIRCONIA [J].
CHENG, YB ;
THOMPSON, DP .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (03) :683-688
[5]  
Chung TJ, 1997, J AM CERAM SOC, V80, P2607, DOI 10.1111/j.1151-2916.1997.tb03163.x
[6]   NITRIDE-STABILIZED CUBIC ZIRCONIA [J].
CLAUSSEN, N ;
WAGNER, R ;
GAUCKLER, LJ ;
PETZOW, G .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1978, 61 (7-8) :369-370
[7]   Microstructural study of silica-doped zirconia ceramics [J].
Gremillard, L ;
Epicier, T ;
Chevalier, J ;
Fantozzi, G .
ACTA MATERIALIA, 2000, 48 (18-19) :4647-4652
[8]   LOW-TEMPERATURE AGING OF T'-ZIRCONIA - THE ROLE OF MICROSTRUCTURE ON PHASE-STABILITY [J].
JUE, JF ;
CHEN, J ;
VIRKAR, AV .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (08) :1811-1820
[9]   INDENTATION STUDIES ON Y2O3-STABILIZED ZRO2 .1. DEVELOPMENT OF INDENTATION-INDUCED CRACKS [J].
KALISZEWSKI, MS ;
BEHRENS, G ;
HEUER, AH ;
SHAW, MC ;
MARSHALL, DB ;
DRANSMANN, GW ;
STEINBRECH, RW ;
PAJARES, A ;
GUIBERTEAU, F ;
CUMBRERA, FL ;
DOMINGUEZRODRIGUEZ, A .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (05) :1185-1193
[10]   MECHANICS OF TRANSFORMATION-TOUGHENING IN BRITTLE MATERIALS [J].
MCMEEKING, RM ;
EVANS, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1982, 65 (05) :242-246