Effect of vibratory weld conditioning on valve residual stress and fracture toughness

被引:0
|
作者
Lu, Qinghua [1 ]
Chen, Ligong [1 ]
Ni, Chunzhen [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai 200030, Peoples R China
来源
PROCEEDINGS OF THE INTERNATIONAL CONFERENCE ON MECHANICAL ENGINEERING AND MECHANICS 2007, VOLS 1 AND 2 | 2007年
关键词
vibratory weld conditioning; residual stress; fracture toughness;
D O I
暂无
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
In the present work the effects of vibratory weld conditioning (VWC) on residual stress and fracture toughness of full welded valve have been investigated. The experiment results show that vibration reduces residual deformation and stress generally. Fracture test is carried out using single edge notch bend (SENB) specimens. The fracture surfaces of failed weld metal (WM) specimens are characterized by dimple-like structures. The depth and density of these dimples increase with vibration applied in welding. While the fracture characteristic of the heat-affected zone (HAZ) is river marking, indicating brittle fracture mode. The possible solidification behaviour in VWC is discussed in this paper.
引用
收藏
页码:1044 / 1048
页数:5
相关论文
共 50 条
  • [11] Vibratory weld conditioning: treatment of specimens during cooling
    Munsi, ASMY
    Waddell, AJ
    Walker, CA
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2000, 214 (L3) : 129 - 138
  • [12] Effect of fracture path on the toughness of weld metal
    Gubeljak, N
    Legat, J
    Koçak, M
    INTERNATIONAL JOURNAL OF FRACTURE, 2002, 115 (04) : 343 - 359
  • [13] Effect of Trace Element on Microstructure and Fracture Toughness of Weld Metal
    Xu, Ke
    Fang, Tao
    Zhao, Longfei
    Cui, Haichao
    Lu, Fenggui
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2020, 33 (03) : 425 - 436
  • [14] Effect of fracture path on the toughness of weld metal
    N. Gubeljak
    J. Legat
    M. Koçak
    International Journal of Fracture, 2002, 115 : 343 - 359
  • [15] RESIDUAL STRESS AND FRACTURE TOUGHNESS OF PIRAC TITANIUM NITRIDE COATINGS
    Wu, Siyuan
    Zhang, Guoyun
    Wu, Shoujun
    Su, Yu
    SURFACE REVIEW AND LETTERS, 2017, 24 (04)
  • [16] Effects of vibratory weld conditioning on residual stresses and transverse contraction distortions in multipass welding
    Xu, J. J.
    Chen, L. G.
    Ni, C. Z.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2006, 11 (04) : 374 - 378
  • [17] Effect of residual stress on cleavage fracture toughness by using cohesive zone model
    Ren, X. B.
    Zhang, Z. L.
    Nyhus, B.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2011, 34 (08) : 592 - 603
  • [18] Effect of Process Induced Residual Stress on Interlaminar Fracture Toughness on Hybrid Composites
    Werner, Brian T.
    Nelson, Kevin
    Nelson, Ciji
    MECHANICS OF COMPOSITE, HYBRID AND MULTIFUNCTIONAL MATERIALS, VOL 5, 2019, : 307 - 310
  • [19] Vibratory weld conditioning - the effect of rigid body motion vibration during welding
    Munsi, A. S. M. Y.
    Waddell, A. J.
    Walker, C. A.
    STRAIN, 1999, 35 (04) : 139 - 143
  • [20] Vibratory weld conditioning process for thick plate welding
    Lu, Q.H.
    Zhang, J.
    Chen, X.
    Guo, C.
    Materials Research Innovations, 2015, 19 : S988 - S990