Stressed-oxidation behavior of 2D CVI SiC/BN/SiC at elevated temperature in air

被引:6
|
作者
Han, Xiao [1 ,3 ]
Pan, Rong [5 ]
Shi, Jian [5 ]
Yu, Guoqiang [1 ,3 ]
Song, Fangxiao [1 ,3 ]
Gao, Xiguang [1 ,3 ]
Song, Yingdong [1 ,3 ,4 ]
Wang, Fang [2 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Key Lab Aeroengine Thermal Environm & Struct, Minist Ind & Informat Technol, Coll Energy & Power Engn, Nanjing 210016, Peoples R China
[2] Nanjing Forestry Univ, Coll Chem Engn, Nanjing 210016, Peoples R China
[3] Nanjing Univ Aeronaut & Astronaut, Coll Energy & Power Engn, Jiangsu Prov Key Lab Aerosp Power Syst, Nanjing 210016, Peoples R China
[4] Nanjing Univ Aeronaut & Astronaut, State Key Lab Mech & Control Mech Struct, Nanjing 210016, Peoples R China
[5] AECC Sichuan Gas Turbine Estab, Chengdu 610500, Peoples R China
关键词
SiC; BN; SiC composites; Intermediate temperature; Stressed-oxidation behavior; Strain-time curve; Failure mechanism; MATRIX COMPOSITES; BORON-NITRIDE; RUPTURE; MECHANISMS; LIFETIME; FIBERS; CARBON; DAMAGE;
D O I
10.1016/j.ceramint.2021.06.082
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The stressed-oxidation behaviors of 2D woven SiCf/BN/SiC composites were investigated at 950 degrees C and 1100 degrees C in air. The different proportions (60%-90%) of the ultimate tensile strength (UTS) at corresponding temperatures were chosen as constant stress. The stressed-oxidation experiments were taken to failure or interrupted (240h). The UTS decreases by 20.75% at 950 degrees C and 30.71% at 1100 degrees C. The composites did not fail during stressed oxidation when subjected to constant stress corresponding to the initial linear and the beginning of nonlinear segments of the tensile curve, above which the composites failed with a maximum failure life of about 10h. Fiber degradation due to the thermal exposure and the fiber cracks caused by the oxidation of BN interface coating and SiC fiber could be responsible for the strength degradation and failure of the composites during stressed oxidation.
引用
收藏
页码:28158 / 28166
页数:9
相关论文
共 50 条
  • [1] Tensile and stressed-oxidation behavior of 2D SiC/BN/SiC composites at Intermediate Temperatures in Air
    Han, Xiao
    Yu, Guoqiang
    Pan, Rong
    Shao, Hongyan
    Xie, Chuyang
    Zhang, Huajun
    Gao, Xiguang
    Song, Yingdong
    Wang, Fang
    CERAMICS INTERNATIONAL, 2022, 48 (01) : 1 - 9
  • [2] Oxidation behavior of SiC/SiC composites in air at high temperature
    Hong Zhi-liang
    Zhang Qiao-jun
    Li Kai-yuan
    Guo Hong-bao
    Zhang Cheng-yu
    Liu Yong-sheng
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2021, 49 (05): : 144 - 150
  • [3] Corrosion behavior of CVI 2D Cf/SiC composites under high temperature burner rig tests
    Yu, Jun
    Duan, Junjie
    Fan, Xiaomeng
    Xiao, Peng
    Chen, Pengju
    Tong, Yonggang
    Li, Yang
    CORROSION SCIENCE, 2022, 209
  • [4] A comparative study on high temperature oxidation behavior of SiC, SiC-BN and SiBCN monoliths
    Zhang, Meng
    Chen, Qingqing
    He, Yunpeng
    Hong, Yuzhe
    Li, Daxin
    Yang, Zhihua
    Jia, Dechang
    Cai, Delong
    Niu, Zibo
    Guan, Jingyi
    Wang, Bingzhu
    CORROSION SCIENCE, 2021, 192
  • [5] Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating
    Wu, SJ
    Cheng, LF
    Zhang, LT
    Xu, YD
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (14-15): : 4489 - 4492
  • [6] Dynamic fracture behavior on 2D SiC/SiC composites
    Shibayama, T
    Kayano, H
    SCIENCE REPORTS OF THE RESEARCH INSTITUTES TOHOKU UNIVERSITY SERIES A-PHYSICS CHEMISTRY AND METALLURGY, 1997, 45 (01): : 127 - 131
  • [7] High temperature oxidation behavior and mechanism of Ti3SiC2-SiC nanocomposites in air
    Zhang, Jianfeng
    Wang, Lianjun
    Jiang, Wan
    Chen, Lidong
    COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (06) : 1531 - 1538
  • [8] Effect of oxidation on the damping behavior of 2D C/SiC composites
    Zhang Qing
    Cheng Lai-fei
    Wang Fu-yuan
    Zhang Li-tong
    NEW CARBON MATERIALS, 2014, 29 (06) : 522 - 528
  • [9] Research on mechanical behavior of 2D C/SiC composites at elevated temperature under uniaxial compression
    Suo, Tao
    Li, Yu-Long
    Liu, Ming-Shuang
    Binggong Xuebao/Acta Armamentarii, 2010, 31 (04): : 516 - 520
  • [10] Oxidation behavior of CVI, MSI and CVI plus MSI C/SiC composites
    Yan Zhi-qiao
    Chen Feng
    Xiong Xiang
    Xiao Peng
    Zhang Hong-bo
    Huang Bai-yun
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (04) : 590 - 596