Understanding the synergistic effect of CO2, H2S and fluid flow towards carbon steel corrosion

被引:25
作者
Zhang, Shaohua [1 ]
Li, Yanrui [1 ]
Liu, Baosheng [1 ]
Mou, Liming [1 ]
Yu, Shuo [1 ]
Zhang, Yuezhong [1 ]
Yan, Xiaoyan [1 ]
机构
[1] Taiyuan Univ Sci & Technol, Coll Mat Sci & Engn, Taiyuan 030024, Shanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
Synergistic mechanism; Carbon steel; CO2; H2S; Fluid flow; HYDROGEN-SULFIDE; HIGH-TEMPERATURE; STAINLESS-STEEL; IRON; BEHAVIOR; MECHANISM; PRODUCTS; KINETICS; XPS; ENVIRONMENTS;
D O I
10.1016/j.vacuum.2021.110790
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The synergistic effect of CO2, H2S and fluid flow towards carbon steel pipelines was studied by systematically evaluating the corrosion response of AISI 1020 carbon steel in aqueous solutions containing CO2 and CO2/H2S at various contents under the static and dynamic conditions at 60 degrees C. The results have revealed that the dissolved H2S can impede the formation of FeCO3 crystals by the preferential adsorption process of FeHSads+ to form the porous iron sulfide scale, through which the corrosive species, especially in dissolved CO2, can easily reach the steel/scale interface and accelerate the dissolution of steel matrix. On the other hand, the limited adsorption process of FeHSads+, enhanced mass transport of corrosive species/Fe2+ along with easy spalling of iron sulfide scale with poor adhesion are expected under the action of fluid flow, ultimately aggravating the localized and general corrosion of carbon steel.
引用
收藏
页数:14
相关论文
共 69 条
[1]   New insights on the role of CO2 in the mechanism of carbon steel corrosion [J].
Almeida, Tatiana das Chagas ;
Elaine Bandeira, Merlin Cristina ;
Moreira, Rogaciano Maia ;
Mattos, Oscar Rosa .
CORROSION SCIENCE, 2017, 120 :239-250
[2]  
[Anonymous], 2004, ASTM Standard G31-72
[3]   The impact-abrasive wear behavior of high wear resistance filling pipeline with explosion treatment [J].
Ba, Lei ;
Gao, Qian ;
Cen, Wang ;
Wang, Jing ;
Wen, Zhenjiang .
VACUUM, 2021, 192
[4]   Initiation and developmental stages of steel corrosion in wet H2S environments [J].
Bai, Pengpeng ;
Zhao, Hui ;
Zheng, Shuqi ;
Chen, Changfeng .
CORROSION SCIENCE, 2015, 93 :109-119
[5]   Investigations of the diverse corrosion products on steel in a hydrogen sulfide environment [J].
Bai, Pengpeng ;
Zheng, Shuqi ;
Zhao, Hui ;
Ding, Yu ;
Wu, Jian ;
Chen, Changfeng .
CORROSION SCIENCE, 2014, 87 :397-406
[6]   A review of iron carbonate (FeCO3) formation in the oil and gas industry [J].
Barker, Richard ;
Burkle, Daniel ;
Charpentier, Thibaut ;
Thompson, Harvey ;
Neville, Anne .
CORROSION SCIENCE, 2018, 142 :312-341
[7]   Reaction pathways in the Fe-S system below 100°C [J].
Benning, LG ;
Wilkin, RT ;
Barnes, HL .
CHEMICAL GEOLOGY, 2000, 167 (1-2) :25-51
[8]  
Bockris J.O.M., 1961, ELECTROCHIM ACTA, V4, P325, DOI [10.1016/0013-4686(61)80026-1, DOI 10.1016/0013-4686(61)80026-1]
[9]  
Bockris JOM, 1962, Electrochim Acta, V3, P293, DOI [10.1016/0013-4686(62)87007-8, DOI 10.1016/0013-4686(62)87007-8]
[10]   XPS study of the silica-supported Fe-containing catalysts for deep or partial H2S oxidation [J].
Bukhtiyarova, GA ;
Bukhtiyarov, VI ;
Sakaeva, NS ;
Kaichev, VV ;
Zolotovskii, BP .
JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 2000, 158 (01) :251-255