On the mechanical performance of K- and Na-based strain-hardening geopolymer composites (SHGC) reinforced with PVA fibers

被引:46
作者
Constancio Trindade, Ana Carolina [1 ]
Curosu, Iurie [2 ]
Liebscher, Marco [2 ]
Mechtcherine, Viktor [2 ]
Silva, Flavio de Andrade [1 ]
机构
[1] Pontificia Univ Catolica Rio de Janeiro PUC Rio, Dept Civil & Environm Engn, Rio De Janeiro 22451900, RJ, Brazil
[2] Tech Univ Dresden, Inst Construct Mat, Dresden 01062, Germany
关键词
Geopolymer; Fiber reinforcement; PVA fiber; Strain-hardening; ductility; Aggregates; Pullout test; CEMENT-BASED COMPOSITES; FLY-ASH; FRACTURE-TOUGHNESS; TENSILE BEHAVIOR; MATRIX DESIGN; METAKAOLIN; SHCC; MICROSTRUCTURE; REPAIR; MODEL;
D O I
10.1016/j.conbuildmat.2020.118558
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Strain-hardening cementitious composites (SHCC) are known by their high deformation capacity due to a multiple cracking tolerance under increasing tensile loading. While SHCC have been well investigated, the design of geopolymer (GP) composites in the same context is not sufficiently understood, mainly due to varying precursor materials used in previous studies. In this work, two metakaolin-based GP mixtures were produced, using K and Na as alkali sources. The incorporation of fine-grained sand was extensively investigated to evaluate its compatibility with both strain-hardening geopolymer composites (SHGC) reinforced with short polyvinyl-alcohol (PVA) fibers. Their mechanical properties were analyzed by means of compression, bending, and tension tests. Digital Image Correlation (DIC) was used to evaluate the fracture mechanisms under uniaxial tension. Particle size distribution (PSD), X-ray diffraction (XRD), Thermogravimetric analysis (TGA) and mercury intrusion porosimetry (MIP) were conducted. Additionally, single-fiber pullout tests with subsequent Environmental Scanning Electron Microscopy (ESEM) were carried out. NaGP composites, reinforced with fine-grained sand, yielded improved mechanical responses, reaching a strain capacity of approximately 4.5%, with enhanced multiple cracking, as opposed to the lower performance observed for KGP composites, that did not present a typical strain-hardening curve when in presence of fine-grained sand, but a strain-softening one. When compared to typical SHCC responses, Na-based SHGC showed a mechanically improved multiple cracking behavior, indicating the potential of this material for a wide range of applications, such as dynamic loading and requirements of long-term durability. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:16
相关论文
共 68 条
[1]  
4A STM International, 2015, ASTM C1437-15, P7
[2]   The effect of matrix composition and calcium content on the sulfate durability of metakaolin and metakaolin/slag alkali-activated mortars [J].
Alcamand, Himad A. ;
Borges, Paulo H. R. ;
Silva, Flavio A. ;
Trindade, Ana Carolina C. .
CERAMICS INTERNATIONAL, 2018, 44 (05) :5037-5044
[3]  
[Anonymous], ADV CIVIL ENG MAT
[4]  
[Anonymous], 19612016 BS EN
[5]  
[Anonymous], 2002, ACI Symposium Publication, DOI DOI 10.14359/12264
[6]  
[Anonymous], 2018, THESIS TU DRESDEN
[7]  
[Anonymous], 2009, D6910D6910M09 ASTM I
[8]  
[Anonymous], ENGINEERED CEMENTITI
[9]  
ASTM, 2014, C230C230M14 ASTM INT
[10]  
ASTM International, 2017, C138C138M17A ASTM IN