Phase transformation of Ni/Si thin films induced by nanoindentation and annealing

被引:5
|
作者
Lee, Woei-Shyan [1 ]
Chen, Tao-Hsing [2 ]
Lin, Chi-Feng [3 ]
Chen, Jyun-Ming [1 ]
机构
[1] Natl Cheng Kung Univ, Dept Mech Engn, Tainan 701, Taiwan
[2] Natl Cheng Kung Univ, Ctr Micro Nano Sci & Technol, Tainan 701, Taiwan
[3] Natl Ctr High Performance Comp, Hsin Shi 744, Tainan County, Taiwan
来源
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING | 2010年 / 100卷 / 04期
关键词
NICKEL SILICIDE; MECHANICAL-PROPERTIES; INDENTATION; SUBSTRATE; HARDNESS; NISI; STABILITY; THICKNESS; CONTACT; CMOS;
D O I
10.1007/s00339-010-5706-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Thin Ni/Si films are prepared by depositing a Ni layer with a thickness of 100 nm on a Si (100) substrate. The as-deposited thin-film specimens are indented to a maximum depth of 500 nm using a nanoindentation technique and are then annealed at temperatures of 200A degrees C, 300A degrees C, 500A degrees C and 800A degrees C for 2 min. The microstructural changes and phases induced in the various specimens are observed using transmission electron microscopy (TEM) and micro-Raman scattering spectroscopy (RSS). Based on the load-displacement data obtained in the nanoindentation tests, the hardness and Young's modulus of the as-deposited specimens are found to be 13 GPa and 177 GPa, respectively. The microstructural observations reveal that the nanoindentation process prompts the transformation of the indentation-affected zone of the silicon substrate from a diamond cubic structure to a mixed structure comprising amorphous phase and metastable Si III and Si XII phases. Following annealing at temperatures of 200 similar to 500A degrees C, the indented zone contains either a mixture of amorphous phase and Si III and Si XII phases, or Si III and Si XII phases only, depending on the annealing temperature. In addition, the annealing process prompts the formation of nickel silicide phases at the Ni/Si interface or within the indentation zone. The composition of these phases depends on the annealing temperature. Specifically, Ni(2)Si is formed at a temperature of 200A degrees C, NiSi is formed at a temperature of 300A degrees C and 500A degrees C, and NiSi(2) is formed at 800A degrees C.
引用
收藏
页码:1089 / 1096
页数:8
相关论文
共 50 条
  • [41] Study on annealing effects of Au thin films on Si
    Young, TF
    Chang, JF
    Ueng, HY
    THIN SOLID FILMS, 1998, 322 (1-2) : 319 - 322
  • [42] AES and USXES investigations of the phase transformation in the surface layers of V-Si/SiO2/Si thin films structure stimulated by oxygen annealing
    Domashevskaya, EP
    Yurakov, YA
    Veligura, GA
    Bocharov, SA
    JOURNAL OF ELECTRON SPECTROSCOPY AND RELATED PHENOMENA, 1995, 76 : 511 - 516
  • [43] Annealing effect on the photoluminescence of Si nanocrystallites thin films
    Jeon, KA
    Kim, JH
    Choi, JB
    Han, KB
    Lee, SY
    MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2003, 23 (6-8): : 1017 - 1019
  • [44] Electron microscopy study of Ni induced crystallization in amorphous Si thin films
    Radnoczi, G. Z.
    Dodony, E.
    Battistig, G.
    Vouroutzis, N.
    Stoemenos, J.
    Frangis, N.
    Kovacs, A.
    Pecz, B.
    INTERNATIONAL CONFERENCES AND EXHIBITION ON NANOTECHNOLOGIES & ORGANIC ELECTRONICS (NANOTEXNOLOGY 2014), 2015, 1646 : 31 - 37
  • [45] Magnetic field induced phase transformation in polycrystalline NiCoMnAl thin films
    Rios, S.
    Bufford, D.
    Karaman, I.
    Wang, H.
    Zhang, X.
    APPLIED PHYSICS LETTERS, 2013, 103 (13)
  • [46] UV-Induced Ferroelectric Phase Transformation in PVDF Thin Films
    Almadhoun, Mahmoud N.
    Khan, Mohammad A.
    Raab, Karam
    Park, Ji Hoon
    Buriak, Jillian M.
    Alshareef, Husain N.
    ADVANCED ELECTRONIC MATERIALS, 2019, 5 (01)
  • [47] Nanoindentation behaviour and microstructural evolution of Au/Cr/Si thin films
    Department of Mechanical Engineering, National Cheng Kung University, Tainan 701, Taiwan, Taiwan
    不详
    Mater. Trans., 7 (1768-1777):
  • [48] Nanoindentation Behaviour and Microstructural Evolution of Au/Cr/Si Thin Films
    Lee, Woei-Shyan
    Liu, Te-Yu
    Chen, Tao-Hsing
    MATERIALS TRANSACTIONS, 2009, 50 (07) : 1768 - 1777
  • [49] NANOINDENTATION OF ZnSnO/Si THIN FILMS PREPARED BY AEROSOL SPRAY PYROLYSIS
    Morar, V
    Pyrtsac, C.
    Curmei, N.
    Grabco, D.
    Rusu, E., V
    Ursachi, V. V.
    Tiginyanu, I. M.
    ROMANIAN JOURNAL OF PHYSICS, 2021, 66 (3-4):
  • [50] A Critical Appraisal of the Nanoindentation Creep 'Nose' Effect in Ni Thin Films
    Ma, Zengsheng
    Zhou, Yichun
    Long, Shiguo
    Pan, Yong
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2012, 12 (02) : 955 - 958