Adaptation and self-healing effect of tribo-oxidizing in high-speed sliding friction on ZrB2-SiC ceramic composite

被引:33
作者
Savchenko, N. L. [1 ]
Mirovoy, Yu A. [1 ,2 ]
Buyakov, A. S. [1 ,2 ]
Burlachenko, A. G. [1 ]
Rudmin, M. A. [2 ]
Sevostyanova, I. N. [1 ]
Buyakova, S. P. [1 ,2 ,3 ]
Tarasov, S. Yu [1 ,2 ]
机构
[1] Inst Strength Phys & Mat Sci, Tomsk, Russia
[2] Natl Res Tomsk Polytech Univ, Tomsk, Russia
[3] Natl Res Tomsk State Univ, Tomsk, Russia
基金
俄罗斯科学基金会;
关键词
ZrB2-SiC; Sliding friction; Wear rate; Tribofilm; Worn surface analysis; Self-healing; TRIBOLOGICAL PROPERTIES; THERMAL-CONDUCTIVITY; MAGNETIC-PROPERTIES; ABLATION BEHAVIOR; SILICON-CARBIDE; WEAR; TEMPERATURE; OXIDATION; STEEL; COATINGS;
D O I
10.1016/j.wear.2020.203204
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The objective of this work was to study adaptive mechanisms and behavior of ZrB2-20 vol% SiC ultra high-temperature ceramics in low-speed and high-speed sliding against a high-carbon steel disk. The worn surfaces of ceramic samples were examined and characterized for chemical composition and mechanical properties. Intense tribooxidation of the composite components as well as transfer layer generation was observed at sliding speeds as high as 11 m/s, 22 m/s and 37 m/s with the formation of at least two subsurface layers. The first one was a mechanically mixed (transfer) layer composed of an iron-containing borosilicate glass mixed with the tribooxidation products resulted from oxidizing both ceramics and steel components. The second underlying layer was a partially oxidized zirconium diboride. Such a combination of quasi-viscous transfer layer and partially ductile underlying layer allowed reducing friction, forming a smooth worn surface and protecting the ceramics against brittle subsurface fracture. Also the effect of self-healing of the subsurface defects by means of liquid bomsilicate glass was observed during sliding friction. The results obtained were discussed in comparison to other adaptation mechanisms found in different materials during friction.
引用
收藏
页数:17
相关论文
共 68 条
  • [21] HOT HARDNESS OF SELECTED BORIDES OXIDES AND CARBIDES TO 1900 DEGREES C
    KOESTER, RD
    MOAK, DP
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1967, 50 (06) : 290 - &
  • [22] Texture formation on the friction surface in transformation-toughened ceramics
    Korolev, PV
    Savchenko, NL
    Kul'kov, SN
    [J]. TECHNICAL PHYSICS LETTERS, 2004, 30 (01) : 12 - 14
  • [23] THE STRUCTURAL ENERGETIC CONCEPT IN THE THEORY OF FRICTION AND WEAR - (SYNERGISM AND SELF-ORGANIZATION)
    KOSTETSKY, BI
    [J]. WEAR, 1992, 159 (01) : 1 - 15
  • [24] KOVALCHUK VV, 1992, SOV POWDER METALL+, V31, P183
  • [25] Crystal structure and elastic properties of ZrB compared with ZrB2: A first-principles study
    Li, Hui
    Zhang, Litong
    Zeng, Qingfeng
    Wang, Junjie
    Cheng, Laifei
    Ren, Haitao
    Guan, Kang
    [J]. COMPUTATIONAL MATERIALS SCIENCE, 2010, 49 (04) : 814 - 819
  • [26] Control of the thermal conductivity of SiC by modifying the polymer precursor
    Li, Zhenbao
    Wang, Yiguang
    An, Linan
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (01) : 61 - 67
  • [27] Effect of high-temperature aging on the thermal conductivity of nanocrystalline tetragonal yttria-stabilized zirconia
    Limarga, Andi M.
    Shian, Samuel
    Baram, Mor
    Clarke, David R.
    [J]. ACTA MATERIALIA, 2012, 60 (15) : 5417 - 5424
  • [28] Friction, wear and mechanical behavior of nano-objects on the nanoscale
    Maharaj, Dave
    Bhushan, Bharat
    [J]. MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2015, 95 : 1 - 43
  • [29] Micro pop-in issues in nanoindentation behaviour of 10 ZTA ceramics
    Maiti, Payel
    Eqbal, Ammar
    Bhattacharya, Manjima
    Das, Pradip Sekhar
    Ghosh, Jiten
    Mukhopadhyay, Anoop Kumar
    [J]. CERAMICS INTERNATIONAL, 2019, 45 (07) : 8204 - 8215
  • [30] MAKRAM H, 1971, J CRYST GROWTH, V13, P585