Effect of ceramic waste powder on alkali-activated slag pastes cured in hot weather after exposure to elevated temperature

被引:109
作者
Rashad, Alaa M. [1 ,2 ]
Essa, Ghada M. F. [1 ]
机构
[1] Housing & Bldg Natl Res Ctr, Bldg Mat Res & Qual Control Inst, HBRC, Cairo, Egypt
[2] Shaqra Univ, Coll Engn, Civil Engn Dept, Shaqraa, Saudi Arabia
关键词
Activated slag; Recycled ceramic powder; Water absorption; Compressive strength; High temperature; Hot weather; BLAST-FURNACE SLAG; MECHANICAL-PROPERTIES; COMPRESSIVE STRENGTH; MORTARS; GEOPOLYMERS; BINDERS; MICROSTRUCTURE; PERFORMANCE; DURABILITY; RESISTANCE;
D O I
10.1016/j.cemconcomp.2020.103617
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Extensive amounts of ceramic and slag wastes are produced every year by ceramic and iron industries. Recycling of these wastes are one of the operational solutions to eliminate their disposal. It is appropriate to employ these wastes as a binder material in the field of construction to save the virgin natural raw materials and limit environmental pollution problems. This work aims to incorporate ceramic waste powder (C-W-P) into alkali-activated slag (AAS) pastes activated with sodium silicate. The specimens were cured at a high ambient temperature of 45 degrees C to simulate curing in hot weather. Slag was partially replaced with C-W-P in the range of 5-50%, by weight. The effect of C-W-P on the workability, water absorption and compressive strength were measured. After 91 curing days, some specimens were subjected to elevated temperatures in the range of 200-1000 degrees C with a step of 200 degrees C for 2 h and the residual compressive strength was monitored. The results were analyzed by X-ray diffraction (XRD), thermogravimetric analysis and its derivative (TGA/DTG) as well as scanning electron microscopy (SEM). The results revealed that C-W-P has a negative effect on the workability, whilst it has a positive effect on the water absorption as well as the compressive strength before and after exposure to elevated temperatures.
引用
收藏
页数:10
相关论文
共 68 条
  • [11] Mechanical and thermal characterisation of geopolymers based on silicate-activated metakaolin/slag blends
    Bernal, Susan A.
    Rodriguez, Erich D.
    Mejia de Gutierrez, Ruby
    Gordillo, Marisol
    Provis, John L.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2011, 46 (16) : 5477 - 5486
  • [12] Evolution of binder structure in sodium silicate-activated slag-metakaolin blends
    Bernal, Susan A.
    Provis, John L.
    Rose, Volker
    Mejia de Gutierrez, Ruby
    [J]. CEMENT & CONCRETE COMPOSITES, 2011, 33 (01) : 46 - 54
  • [13] Influence of admixtures on the properties of alkali-activated slag mortars subjected to different curing conditions
    Bilim, Cahit
    Karahan, Okan
    Atis, Cengiz Duran
    Ilkentapar, Serhan
    [J]. MATERIALS & DESIGN, 2013, 44 : 540 - 547
  • [14] Influence of the long term curing temperature on the hydration of alkaline binders of blast furnace slag-metakaolin
    Burciaga-Diaz, Oswaldo
    Gomez-Zamorano, Lauren Y.
    Ivan Escalante-Garcia, Jose
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2016, 113 : 917 - 926
  • [15] Statistical Analysis of Strength Development as a Function of Various Parameters on Activated Metakaolin/Slag Cements
    Burciaga-Diaz, Oswaldo
    Ivan Escalante-Garcia, Jose
    Arellano-Aguilar, Raul
    Gorokhovsky, Alexander
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (02) : 541 - 547
  • [16] Mechanical and microstructural properties of alkali-activated slag and slag plus fly ash mortars exposed to high temperature
    Celikten, Serhat
    Saridemir, Mustafa
    Deneme, Ibrahim Ozgur
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2019, 217 : 50 - 61
  • [17] Fire-resistant geopolymer produced by granulated blast furnace slag
    Cheng, TW
    Chiu, JP
    [J]. MINERALS ENGINEERING, 2003, 16 (03) : 205 - 210
  • [18] Test research on effects of waste ceramic polishing powder on the permeability resistance of concrete
    Cheng, Yun-hong
    Huang, Fei
    Liu, Rui
    Hou, Jian-long
    Li, Guang-lu
    [J]. MATERIALS AND STRUCTURES, 2016, 49 (03) : 729 - 738
  • [20] Thermo-mechanical characteristics of geopolymer mortar
    Chithambaram, S. Jeeva
    Kumar, Sanjay
    Prasad, M. M.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2019, 213 : 100 - 108