Fretting wear of carburized titanium alloy against ZrO2 under serum lubrication

被引:5
|
作者
Luo, Yong [1 ]
Ge, Shirong [1 ]
Zhang, Dekun [1 ]
Wang, Qingliang [1 ]
Liu, Hongtao [1 ]
机构
[1] China Univ Min & Technol, Sch Mat Sci & Engn, Inst Tribol & Reliabil Engn, Xuzhou 221008, Jiangsu, Peoples R China
关键词
Fretting wear; Titanium alloys; Carburization; Artificial joints; CARBIDE; BEHAVIOR;
D O I
10.1016/j.triboint.2010.10.036
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Fretting wear of carburized titanium alloys was investigated on the universal multifunctional tester (UMT) with the ball-on-fiat fretting style under bovine serum lubrication. The tangential load and friction coefficient during the fretting process were analyzed, and the evolution of fretting log during the fretting process was investigated to understand the wear mechanism of the titanium alloy and carburized titanium alloy. Furthermore, the wear scar was examined using a SEM and three-dimension surface profiler. It was found that the friction coefficient of the titanium alloy increased faster than that of carburized titanium alloy in the first stage under serum lubrication, and then remained steady with a similar value in the second stage. The Ft-D curve indicated that there was wear mechanism transition from gross slip to mixed stick and slip. Finally, it was observed that there was a slight damage of the titanium alloy and carburized titanium alloy showed excellent performance during the fretting wear process under serum lubrication. All of the results suggested that carburized titanium alloy was a potential candidate for the stem material in artificial joints. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1471 / 1475
页数:5
相关论文
共 50 条
  • [21] In Situ XPS Analysis of Tribo-chemical Behavior in Titanium Alloy Exposed to Fretting Wear Under the Vacuum Environments
    Long, Jianjun
    Wei, Xuejiao
    Dong, Yiting
    Cheng, Xixi
    Li, Hao
    Xu, Xiaojun
    Zhu, Minhao
    TRIBOLOGY LETTERS, 2024, 72 (02)
  • [22] Study on the Effect of Normal Loads on the Fretting Wear Performance of Zr-4 Alloy Tubes Under Three Fretting Modes
    Xie, Wenxin
    Ding, Siyuan
    Rong, Bin
    Wang, Xizhang
    Xu, Lei
    Peng, Jingfang
    TRIBOLOGY LETTERS, 2025, 73 (01)
  • [23] Influence of phase composition on the sliding wear of composites in the system CaZrO3-MgO-ZrO2 against ZrO2 and steel
    Silva, Abilio
    Booth, Fernando
    Garrido, Liliana
    Aglietti, Esteban
    Pena, Pilar
    Baudin, Carmen
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2016, 85 : 125 - 133
  • [24] Effect of DLC film on fretting wear behavior of TC4 titanium alloy
    Jing P.-F.
    Yu S.-R.
    Song W.
    Chen Q.
    Zhang K.-F.
    Surface Technology, 2021, 50 (02): : 261 - 270
  • [25] Fretting wear and mechanical properties of surface-nanostructural titanium alloy bone plate
    Wang, Gaoqi
    Wang, Shouren
    Yang, Xuefeng
    Yu, Xiuchun
    Wen, Daosheng
    Chang, Zhengqi
    Zhang, Mingyuan
    SURFACE & COATINGS TECHNOLOGY, 2021, 405
  • [26] Microstructural evolution and oxidation in α/β titanium alloy under fretting fatigue loading
    Hanqing Liu
    Xiaohong Shao
    Kai Tan
    Zhenjie Teng
    Yaohan Du
    Lang Li
    Qingyuan Wang
    Qiang Chen
    Friction, 2023, 11 : 1906 - 1921
  • [27] Microstructural evolution and oxidation in α/β titanium alloy under fretting fatigue loading
    Liu, Hanqing
    Shao, Xiaohong
    Tan, Kai
    Teng, Zhenjie
    Du, Yaohan
    Li, Lang
    Wang, Qingyuan
    Chen, Qiang
    FRICTION, 2023, 11 (10) : 1906 - 1921
  • [28] Study of seizure of coated and treated titanium alloy under fretting conditions
    Njankeu, G. R. Yantio
    Paris, J. -Y.
    Denape, J.
    Pichon, L.
    Riviere, J. -P.
    TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1052 - 1059
  • [29] Subsurface deformation mechanism and the interplay relationship between strength-ductility and fretting wear resistance during fretting of a high-strength titanium alloy
    Tong, Yanlin
    Hua, Ke
    Xie, Haoyang
    Cao, Yue
    Huang, Zhuobin
    Liang, Zhenpeng
    Li, Xiaolin
    Wu, Hongxing
    Wang, Haifeng
    FRICTION, 2024, 12 (10) : 2259 - 2280
  • [30] The damage mechanism of Alloy 690TT against Alloy 600 caused by fretting wear in room temperature pure water
    Xin, Long
    Huang, Qian
    Han, Yongming
    Lu, Yonghao
    Zhang, Weidong
    Shoji, Tetsuo
    MATERIALS CHARACTERIZATION, 2020, 161 (161)