High temperature corrosion properties of SiNx and CrNx coatings deposited by IBAD method

被引:9
作者
Pitter, J
Cerny, F
Cizner, J
Suchanek, J
Tischler, D
机构
[1] ATG Ltd, Prague 19902, Czech Republic
[2] Czech Tech Univ, Fac Mech Engn, Dept Phys, Prague, Czech Republic
[3] SVUM Corp, Res Ctr Bechovice, Prague, Czech Republic
[4] Czech Tech Univ, Fac Mech Engn, Dept Mfg Technol, Prague, Czech Republic
关键词
chromium nitride; silicon nitride; MAD coating; high temperature corrosion;
D O I
10.1016/j.surfcoat.2005.02.059
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiNx and CrNx coatings (thickness 1-2 mu m) were deposited by IBAD method at a nitrogen ions energy of 90 keV on low-alloy, AISI 310 and 316 substrate. The samples were subjected to long-term high temperature corrosion tests at cycled reducing-oxidizing atmosphere and in air. Corrosion rate was evaluated gravimetrically. The corrosion rate of coated alloy steels was significantly decreased at temperatures up to 800 degrees C. At 900 degrees C exposure the nitrides were subjected to fast decomposition and oxidation. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:73 / 76
页数:4
相关论文
共 6 条
[1]   Protective behaviour against high temperature oxidation of silicon nitride films synthesized by ion-beam-assisted deposition [J].
Chen, Yuanru ;
Liu, Shikai ;
Liu, Xianghuai ;
Zou, Shichang ;
Shang, Zhenkui ;
Xu, Chuntong ;
Zheng, Yan .
Surface and Coatings Technology, 1992, 51 (1-3) :227-231
[2]  
LIU XH, 1991, SURF COAT TECH, V46, P227, DOI 10.1016/0257-8972(91)90165-S
[3]  
Scharf TW, 2000, J INF STOR PROC SYST, V2, P185
[4]   Metallization of CVD diamond films by ion beam assisted deposition [J].
Tjong, SC ;
Wong, NB ;
Li, G ;
Lee, ST .
MATERIALS CHEMISTRY AND PHYSICS, 2000, 62 (03) :241-246
[5]   PREPARATION OF HARD COATINGS BY ION-BEAM METHODS [J].
WEISSMANTEL, C ;
REISSE, G ;
ERLER, HJ ;
HENNY, F ;
BEWILOGUA, K ;
EBERSBACH, U ;
SCHURER, C .
THIN SOLID FILMS, 1979, 63 (02) :315-325
[6]  
XU D, 1994, SURF COAT TECH, V66, P486