Metal dusting and coking of alloy 803

被引:0
|
作者
Han, GW [1 ]
Feng, D [1 ]
Deng, B [1 ]
机构
[1] Cent Iron & Steel Res Inst, Dept High Temp Mat Res, Beijing 100081, Peoples R China
关键词
superalloys; SEM; metal dusting; coking;
D O I
10.1016/S0010-938X(03)00147-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Investigation was made by SEM examination on metal dusting and coking behaviours of alloy 803 in a flowing gas mixture of H-2-CO-H2O, It was found that an oxide scale arisen on the sample surface at the beginning of exposure, Metal dusting started when graphite deposition occurred earlier at the local defects in the oxide settle than the defects were repaired by enough supply of chromium from the interior of alloy matrix. Coke consisted of graphite filaments and metallic particles produced by disintegrating of alloy matrix, and grow up from the defects in the oxide scale with pit left in the sample surface, Increasing chromium content, doping a small amount of silicon and reducing grain size to create fast diffusion paths for chromium and silicon to alloy surface, all promote the formation of a dense oxide scale and favor early self-repairing or the defects in the oxide scale before occurrence of graphite deposition, The resistance of an alloy to metal dusting can be improved generally by means of these methods, (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:443 / 452
页数:10
相关论文
共 50 条
  • [21] Effect of Ni-Al Coating with and without Re Modification on Coking and Metal Dusting of Fe-Cr-Ni Alloy under Cyclic Condition at 600 °C
    Li, Meifeng
    Xie, Yun
    Grzesik, Zbigniew
    Liu, Famin
    Zhang, Jianqiang
    Zhou, Chungen
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2020, 167 (16)
  • [22] Inhibition of metal dusting of Alloy 800H by laser surface melting
    Voisey, KT
    Liu, Z
    Stott, FH
    APPLIED SURFACE SCIENCE, 2006, 252 (10) : 3658 - 3666
  • [23] Corrosion resistance of a high-silicon alloy in metal-dusting environments
    Chun, C. M.
    Ramanarayanan, T. A.
    OXIDATION OF METALS, 2007, 67 (3-4): : 215 - 234
  • [24] Pure bending testing of Cr-Mo alloy in metal dusting condition
    Xu, Tao
    Tu, Shan-Tung
    Song, Hong-Jian
    Gong, Jian-Ming
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 341 - 344
  • [25] Corrosion Resistance of a High-Silicon Alloy in Metal-Dusting Environments
    C. M. Chun
    T. A. Ramanarayanan
    Oxidation of Metals, 2007, 67 : 215 - 234
  • [26] Initiation of Metal-Dusting Pits and a Method to Mitigate Metal-Dusting Corrosion
    Z. Zeng
    K. Natesan
    Oxidation of Metals, 2006, 66 : 1 - 20
  • [27] Initiation of metal-dusting pits and a method to mitigate metal-dusting corrosion
    Zeng, Z.
    Natesan, K.
    OXIDATION OF METALS, 2006, 66 (1-2): : 1 - 20
  • [28] Resistance of Ni-Base Alloy UNS N06696 to Metal Dusting
    Kurihara, Shinnosuke
    Matsumoto, Satoshi
    Anada, Hiroyuki
    Ogawa, Hidenori
    Nishiyama, Yoshitaka
    Okada, Hirokazu
    Osuki, Takahiro
    MATERIALS PERFORMANCE, 2011, 50 (08) : 66 - 70
  • [29] Metal dusting reaction mechanisms
    Young, D. J.
    HIGH-TEMPERATURE OXIDATION AND CORROSION 2005, 2006, 522-523 : 15 - 26
  • [30] Metal dusting, carburization and nitridation
    Schütze, M
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2003, 54 (10): : 735 - 735