Interfacial Bond Behavior of High Strength Concrete Filled Steel Tube after Exposure to Elevated Temperatures and Cooled by Fire Hydrant

被引:9
作者
Chen, Zongping [1 ,2 ]
Tang, Jiyu [1 ]
Zhou, Xingyu [1 ]
Zhou, Ji [1 ]
Chen, Jianjia [1 ]
机构
[1] Guangxi Univ, Coll Civil Engn & Architecture, Nanning 530004, Peoples R China
[2] Guangxi Univ, Key Lab Disaster Prevent & Struct Safety, Chinese Minist Educ, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
elevated temperatures and water-cooling exposure; high-strength concrete; circular steel tube; bond strength; slip behavior;
D O I
10.3390/ma13010150
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
For the engineering structure in case of fire, a fire hydrant is generally used for extinguishing the fire. This paper presents an experimental investigation on interfacial bond behavior of high-strength concrete-filled steel tube (HSCFST) after exposure to elevated temperatures and cooled by fire hydrant using the pull-out test of 22 specimens. According to the experimental study, the failure mechanism of HSCFST exposed to elevated temperatures and water-cooling (ETWC) was revealed, the influence of various parameters on the bond behavior was analyzed, and the calculation formula of the bond strength of HSCFST subjected to ETWC was put forward. The results show that the load-slip curves of the loading end and the free end of the specimen are basically similar, and can be divided into three types of typical curves. In the push out test, the strain on the outer surface of the steel tube is exponentially distributed with its distance from the loading end. After ETWC exposure, the bond strength of the specimen is less affected by the concrete strength, which is inversely proportional to the anchorage length, and it is basically stable after the constant temperature duration is longer than 60 min. With the increase of the maximum temperature, the ultimate bond strength increases first, then decreases and then increases, and the residual bond strength increases first and then decreases. Besides, the study indicate that cooling method has significant influence on the bond behavior, compared with natural cooling specimens, the ultimate bond strength, residual bond strength, and shear bond stiffness of water-cooling specimens are smaller, and the interfacial energy dissipation capacity is larger.
引用
收藏
页数:23
相关论文
共 29 条
[1]   High temperature and residual properties of reactive powder concrete - A review [J].
Abid, Muhammad ;
Hou, Xiaomeng ;
Zheng, Wenzhong ;
Hussain, Raja Rizwan .
CONSTRUCTION AND BUILDING MATERIALS, 2017, 147 :339-351
[2]   High performance concrete under elevated temperatures [J].
Akca, Abdullah Huzeyfe ;
Zihnioglu, Nilufer Ozyurt .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 44 :317-328
[3]   Incremental collapse threshold for pushout resistance of circular concrete filled steel tubular columns [J].
Aly, T. ;
Elchalakani, M. ;
Thayalan, P. ;
Patnaikuni, I. .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2010, 66 (01) :11-18
[4]  
[Anonymous], 2014, GB509742014 MIN HOUS
[5]  
[Anonymous], 2011, GBT14682011 STAND AD
[6]  
[Anonymous], 2005, 5400252005 BS
[7]  
[Anonymous], 1997, AIJ REC DES CONSTR C
[8]  
[Anonymous], 2004, 13612004 DBJ
[9]  
[Anonymous], 1980, IABSE P
[10]  
[Anonymous], 2004, EUR 4 EC4 DES COMP S