Properties of cubic boron nitride thin films deposited by a hybrid RF-PLD-technique

被引:4
作者
Klotzbucher, T
Mergens, M
Wesner, DA
Kreutz, EW
机构
[1] Rhein Westfal TH Aachen, Lehrstuhl Lasertech, D-52074 Aachen, Germany
[2] Fraunhofer Inst Lasertech, D-52074 Aachen, Germany
关键词
cubic boron nitride; pulsed layer deposition; RF-bias; compressive stress;
D O I
10.1016/S0257-8972(97)00654-3
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the hybrid RF-PLD-technique pulsed laser deposition is combined with an additional RF-discharge resulting in ion bombardment of the growing film due to DC-self-biasing of the substrate electrode. The DC-bins voltage is in the order of some hundreds of volts, leading to ion energies in the order of some hundreds of electron volts. The ion current to the substrate is typically in the order of 10 mu A/cm(2) as determined by the Langmuir probe technique. FTIR (Fourier transform infrared) spectroscopy reveals that the cubic phase is formed only in regions on the film surface where an ion-to-atom arrival ratio of about 0.5 is present. Maximum cubic boron nitride (c-BN) contents of about 60% have been achieved and a layered structure [hexagonal boron nitride (h-BN) interlayer between substrate and c-BN film] typical for c-BN film deposition, was observed. The films are nearly stoichiometric with little boron enrichment as determined by XPS analysis. Using pure argon discharges without any molecular nitrogen leads to boron-rich films and suppression of the cubic phase. High compressive stress is present in regions of c-BN formation. leading to partial delamination and cracking of the films. Micro-Raman analysis showed only peaks characteristic for h-BN, even in regions of c-BN growth, indicating that c-BN is nanocrystalline, which is confirmed by XRD measurements. (C) 1998 Elsevier Science S.A.
引用
收藏
页码:388 / 392
页数:5
相关论文
共 50 条
  • [41] Effect of heat treatment on the stress and structure evolution of plasma deposited boron nitride thin films
    Anutgan, T. Aliyeva
    Anutgan, M.
    Wdemir, O.
    Atilgan, I.
    Katircioglu, B.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2008, 202 (13) : 3058 - 3066
  • [42] Studies on the stress in cubic boron nitride films by infrared spectroscopy
    Zhao, YN
    Zou, GT
    Wang, B
    He, Z
    Zhu, PW
    Tao, YC
    [J]. CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 1998, 19 (07): : 1136 - 1139
  • [43] Removal of sp2-boron nitride transition layer in the growth of cubic boron nitride films
    Wong, SF
    Ong, CW
    Pang, GKH
    Li, Q
    Lau, WM
    [J]. DIAMOND AND RELATED MATERIALS, 2004, 13 (09) : 1632 - 1637
  • [44] Formation of boron nitride films with various amounts of the cubic phase
    Ullmann, J
    Heyden, D
    Schwarz, G
    Wolf, GK
    Baba, K
    Hatada, R
    [J]. SURFACE & COATINGS TECHNOLOGY, 1997, 97 (1-3) : 281 - 290
  • [45] Adhesion improvement of cubic boron nitride films by in situ annealing
    Yu, J
    Song, SH
    Weng, LQ
    [J]. SURFACE & COATINGS TECHNOLOGY, 2006, 200 (16-17) : 4737 - 4740
  • [46] Stress reduction of cubic boron nitride films by oxygen addition
    Ye, J.
    Ulrich, S.
    Zlebert, C.
    Stueber, M.
    [J]. THIN SOLID FILMS, 2008, 517 (03) : 1151 - 1155
  • [47] Characterisation of cubic boron nitride films at different stages of deposition
    Jiang, LD
    Fitzgerald, AG
    Rose, MJ
    Lousa, A
    Gimeno, S
    [J]. APPLIED SURFACE SCIENCE, 2000, 167 (1-2) : 89 - 93
  • [48] Deposition of thick cubic boron nitride films - Mechanisms and concepts
    Kulisch, Wilhelm
    Freudenstein, Regine
    [J]. THIN SOLID FILMS, 2007, 516 (2-4) : 216 - 222
  • [49] Preparation and thermophysical properties of hexagonal boron nitride-cubic boron nitride/epoxy composites
    Gao L.
    Li X.
    Zhang X.
    Hu Z.
    Yang X.
    [J]. Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 2022, 39 (06): : 2599 - 2606
  • [50] Stress measurement and stress relaxation during magnetron sputter deposition of cubic boron nitride thin films
    Abendroth, B
    Gago, R
    Kolitsch, A
    Möller, W
    [J]. THIN SOLID FILMS, 2004, 447 : 131 - 135