Properties of cubic boron nitride thin films deposited by a hybrid RF-PLD-technique

被引:4
|
作者
Klotzbucher, T
Mergens, M
Wesner, DA
Kreutz, EW
机构
[1] Rhein Westfal TH Aachen, Lehrstuhl Lasertech, D-52074 Aachen, Germany
[2] Fraunhofer Inst Lasertech, D-52074 Aachen, Germany
关键词
cubic boron nitride; pulsed layer deposition; RF-bias; compressive stress;
D O I
10.1016/S0257-8972(97)00654-3
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the hybrid RF-PLD-technique pulsed laser deposition is combined with an additional RF-discharge resulting in ion bombardment of the growing film due to DC-self-biasing of the substrate electrode. The DC-bins voltage is in the order of some hundreds of volts, leading to ion energies in the order of some hundreds of electron volts. The ion current to the substrate is typically in the order of 10 mu A/cm(2) as determined by the Langmuir probe technique. FTIR (Fourier transform infrared) spectroscopy reveals that the cubic phase is formed only in regions on the film surface where an ion-to-atom arrival ratio of about 0.5 is present. Maximum cubic boron nitride (c-BN) contents of about 60% have been achieved and a layered structure [hexagonal boron nitride (h-BN) interlayer between substrate and c-BN film] typical for c-BN film deposition, was observed. The films are nearly stoichiometric with little boron enrichment as determined by XPS analysis. Using pure argon discharges without any molecular nitrogen leads to boron-rich films and suppression of the cubic phase. High compressive stress is present in regions of c-BN formation. leading to partial delamination and cracking of the films. Micro-Raman analysis showed only peaks characteristic for h-BN, even in regions of c-BN growth, indicating that c-BN is nanocrystalline, which is confirmed by XRD measurements. (C) 1998 Elsevier Science S.A.
引用
收藏
页码:388 / 392
页数:5
相关论文
共 50 条
  • [21] Effects of Si impurity on the nucleation and growth of cubic boron nitride thin films
    Oba, H.
    Nose, K.
    Yoshida, T.
    SURFACE & COATINGS TECHNOLOGY, 2007, 201 (9-11) : 5502 - 5505
  • [22] Vibrational spectroscopy of mixed hexagonal-cubic boron nitride thin films
    Beghi, MG
    Bottani, CE
    Miotello, A
    Ossi, PM
    THIN SOLID FILMS, 1997, 308 : 107 - 112
  • [23] FORMATION OF CUBIC BORON-NITRIDE FILMS ON DIAMOND BY PLASMA CVD TECHNIQUE
    OKAMOTO, M
    UTSUMI, Y
    OSAKA, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 1990, 29 (06): : L1004 - L1006
  • [24] Synthesis and mechanical properties of cubic boron nitride/nanodiamond composite films
    Chong, YM
    Ma, KL
    Leung, KM
    Chan, CY
    Ye, Q
    Bello, I
    Zhang, WJ
    Lee, ST
    CHEMICAL VAPOR DEPOSITION, 2006, 12 (01) : 33 - 38
  • [25] General stress reduction mechanisms for the deposition of cubic boron nitride thin films
    Ulrich, S
    Ehrhardt, H
    Schwan, J
    Donner, W
    Dosch, H
    Widmayer, P
    Ziemann, P
    SURFACE & COATINGS TECHNOLOGY, 1999, 116 : 269 - 273
  • [26] Microstructure and mechanical properties of pulsed laser deposited boron nitride films
    Weissmantel, S
    Reisse, G
    Keiper, B
    Schulze, S
    DIAMOND AND RELATED MATERIALS, 1999, 8 (2-5) : 377 - 381
  • [27] C-BN thin film formation in a hybrid rf-PLD technique
    Klotzbucher, T
    Mergens, M
    Wesner, DA
    Kreutz, EW
    DIAMOND AND RELATED MATERIALS, 1997, 6 (5-7) : 599 - 603
  • [28] Cubic boron nitride films for industrial applications
    Bello, I
    Chong, YM
    Leung, KM
    Chan, CY
    Ma, KL
    Zhang, WJ
    Lee, ST
    Layyous, A
    DIAMOND AND RELATED MATERIALS, 2005, 14 (11-12) : 1784 - 1790
  • [29] Preparation of cubic boron nitride films by radio frequency sputtering
    Tian Ling
    Ding Yi
    Chen Hao
    Liu Jun-Kai
    Deng Jin-Xiang
    He De-Yan
    Chen Guang-Hua
    ACTA PHYSICA SINICA, 2006, 55 (10) : 5441 - 5443
  • [30] Cubic boron nitride films by dc and rf magnetron sputtering: Layer characterization and process diagnostics
    Hahn, J
    Friedrich, M
    Pintaske, R
    Schaller, M
    Kahl, N
    Zahn, DRT
    Richter, F
    DIAMOND AND RELATED MATERIALS, 1996, 5 (10) : 1103 - 1112