Effect of Ceramic Surface Treatment and Adhesive Systems on Bond Strength of Metallic Brackets

被引:8
|
作者
Juntavee, Patrapan [1 ]
Kumchai, Hattanas [1 ]
Juntavee, Niwut [2 ]
Nathanson, Dan [1 ]
机构
[1] Boston Univ, Goldman Sch Dent Med, Dept Restorat Sci & Biomat, Boston, MA 02215 USA
[2] Khon Kaen Univ, Dept Prosthodont, Fac Dent, Khon Kaen, Thailand
关键词
PORCELAIN; RESIN; ACID;
D O I
10.1155/2020/7286528
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. This study evaluated the effect of ceramic surface treatments on bond strength of metal brackets to machinable ceramics and veneering porcelain using different adhesive resins. Materials and methods. Machined ceramic specimens (10 x 10 x 2 mm) were prepared from Vitablocs mark II (Vita) and IPS e.max (R) CAD (Ivoclar). Layered porcelain fused to metal (IPS d.Sign (R), Ivoclar) was used to fabricate PFM specimens (n = 60/group). Half of specimens were etched (9.6% HF, 15 sec), and the rest were nonetched. Three resin bonding systems were used for attaching metal brackets (Victory series (TM) APC II, 3M) to each group (n = 10): Transbond (TM) XT (3M), Light Bond (TM) (Reliance), or Blugloo (TM) (Ormco), all cured with LED curing unit (Bluephase G1600, Vivadent) for 50 s each. Specimens were immersed in deionized water at 37 degrees C for 24 hours prior to shear bond testing (Instron) at crosshead speed of 0.5 mm/min. Debond surface of ceramic and bracket base was examined for failure mode (FM), Ceramic Damage Index (CDI), and Adhesive Remnant Index (ARI). ANOVA and post hoc multiple comparisons were used to analyze the differences in bond strength. The chi-squared test was used to determine significance effect of FM, CDI, and ARI. Results. Significant differences in shear bond strength among group were found (p <= 0.05) related to ceramic, surface treatment, and resin cement. Conclusion. Bond strength of bracket to ceramic is affected by type of ceramic, resin cement, and ceramic surface conditioning. Etching ceramic surface enhanced ceramic-bracket bond strength. However, bond strengths in nontreated ceramic surface groups were still higher than bond strength required for bonding in orthodontic treatment.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Effects of surface-conditioning methods on shear bond strength of brackets bonded to different all-ceramic materials
    Sarac, Y. Sinasi
    Kulunk, Tolga
    Elekdag-Turk, Selma
    Sarac, Duygu
    Turk, Tamer
    EUROPEAN JOURNAL OF ORTHODONTICS, 2011, 33 (06) : 667 - 672
  • [42] Effect of DPSS laser on the shear bond strength of orthodontic brackets
    Park, Soo-Byung
    Kang, Eun-Hee
    Son, Woo-Sung
    Ko, Ching-Chang
    Kim, Hyung-Il
    Kwon, Yong Hoon
    AMERICAN JOURNAL OF DENTISTRY, 2010, 23 (04) : 205 - 207
  • [43] Influence of surface treatments on the shear bond strength of orthodontic brackets to porcelain
    Wang, Cong
    Zeng, Jishan
    Wang, Shaoan
    Yang, Zheng
    Huang, Qian
    Chen, Pixiu
    Zhou, Shujuan
    Liu, Xiaoqing
    APPLIED SURFACE SCIENCE, 2008, 255 (02) : 416 - 418
  • [44] The effect of enamel bleaching on the shear bond strengths of metal and ceramic brackets
    Oztas, E.
    Bagdelen, G.
    Kilicoglu, H.
    Ulukapi, H.
    Aydin, I.
    EUROPEAN JOURNAL OF ORTHODONTICS, 2012, 34 (02) : 232 - 237
  • [45] The Influence of Hydrofluoric Acid Temperature and Application Technique on Ceramic Surface Texture and Shear Bond Strength of an Adhesive Cement
    Cuzic, Cristiana
    Jivanescu, Anca
    Negru, Radu Marcel
    Hulka, Iosif
    Rominu, Mihai
    MATERIALS, 2023, 16 (12)
  • [46] Assessment the Bond Strength of Ceramic Brackets to CAD/CAM Nanoceramic Composite and Interpenetrating Network Composite after Different Surface Treatments
    Ozarslan, Mustafa Mehmet
    Ustun, Ozlem
    Buyukkaplan, Ulviye Sebnem
    Barutcigil, Cagatay
    Turker, Nurullah
    Barutcigil, Kubilay
    BIOMED RESEARCH INTERNATIONAL, 2018, 2018
  • [47] Effect of Galardin and its Solvents on the Microtensile Bond Strength of Different Adhesive Systems to Dentin
    Chaharom, Mohammad Esmaeel Ebrahimi
    Bahari, Mahmoud
    Rahbar, Mahdi
    Golbaz, Sepideh
    PESQUISA BRASILEIRA EM ODONTOPEDIATRIA E CLINICA INTEGRADA, 2019, 19 (01):
  • [48] Does surface priming increase the bond strength of orthodontic brackets? An experimental study
    Al Taweel, Sara M.
    Zinelis, Spiros
    Sofyan, Arif
    Al Jabbari, Youssef S.
    CLINICAL AND EXPERIMENTAL DENTAL RESEARCH, 2024, 10 (03):
  • [49] Halloysite nanotube incorporation into adhesive systems-effect on bond strength to human dentin
    Alkatheeri, Mohammed S.
    Palasuk, Jadesada
    Eckert, George J.
    Platt, Jeffrey A.
    Bottino, Marco C.
    CLINICAL ORAL INVESTIGATIONS, 2015, 19 (08) : 1905 - 1912
  • [50] Comparative Evaluation of Shear Bond Strength of Brackets Bonded with self Etch Primer/Adhesive and Conventional Etch/Primer and Adhesive System
    Bhattacharjee, Debarshi
    Sharma, Kanchan
    Rajalaxmi, Sahu
    Neha, Komal
    Kumari, Archana
    Rai, Anurag
    JOURNAL OF PHARMACY AND BIOALLIED SCIENCES, 2021, 13 (06): : S1168 - S1173