Flashover behavior of ceramic and non-ceramic insulators under switching impulse stress at different climatic conditions

被引:0
作者
Elsässer, O [1 ]
Feser, K [1 ]
机构
[1] Univ Stuttgart, Inst Power Transmiss & High Voltage Technol, D-7000 Stuttgart, Germany
来源
1998 ANNUAL REPORT CONFERENCE ON ELECTRICAL INSULATION AND DIELECTRIC PHENOMENA, VOLS 1 AND 2 | 1998年
关键词
D O I
暂无
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Composite insulators became more and more common in service to replace porcelain insulators, because of their outstanding surface characteristics in polluted areas. Many investigations have been carried out on their behavior under AC and DC stress. Little data is available for impulse stress. Therefore the flashover behavior of a ceramic and a composite insulator were investigated under different climatic conditions and switching impulse (SI) stress. The temperature was varied between 10 degrees C and 40 degrees C. The relative humidity was ranged between 10% and 90%. All tests took place in an environmental chamber. The insulators were manufactured with the same profile of the electrodes and had the same number of sheds to get results which were easy to compare. The tests were performed with clean insulators. The influence of the relative and absolute humidity on the flashover voltage were evaluated with respect to the different insulator materials. The results were compared to those obtained in the pure air gap. Special attention was paid to the statistical analyses of the data, which means how to calculate errorbars and confidential intervals.
引用
收藏
页码:88 / 91
页数:4
相关论文
共 50 条
[41]   Causes and potential remedies of brittle fracture failure of composite (non-ceramic) insulators [J].
Kumosa, M ;
Kumosa, L ;
Armentrout, D .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2004, 11 (06) :1037-1048
[42]   Influence of non-ceramic insulators' shed inclination on their long-term behaviour in cyclic rain and fog conditions [J].
Bretuj, W. ;
Fleszynski, J. ;
Wieczorek, K. .
2007 IEEE INTERNATIONAL CONFERENCE ON SOLID DIELECTRICS, VOLS 1 AND 2, 2007, :126-129
[43]   Analysis of Stress Control on 33-kV Non-ceramic Insulators Using Finite-element Method [J].
Natarajan, Murugan ;
Basharan, Vigneshwaran ;
Pillai, Kannayeram Ganapathya ;
Velayutham, Maheswari Ramasamy ;
Silluvairaj, Willjuice Iruthayarajan Maria .
ELECTRIC POWER COMPONENTS AND SYSTEMS, 2015, 43 (05) :566-577
[44]   Electrical performance of non-ceramic insulators in artificial contamination tests - Role of resting time [J].
delaO, A ;
Gorur, RS ;
Burnham, JT .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 1996, 3 (06) :827-835
[45]   Optimized Design of Electric Field Grading Systems in 115 kV Non-Ceramic Insulators [J].
Cruz Dominguez, D. ;
Espino-Cortes, F. P. ;
Gomez, P. .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2013, 20 (01) :63-70
[46]   Electrical performance of non-ceramic insulators in artificial contamination tests role of resting time [J].
Arizona State Univ, Tempe, United States .
IEEE Trans Dielectr Electr Insul, 6 (827-835)
[47]   Brittle fracture of non-ceramic suspension insulators with epoxy cone end-fittings [J].
Kumosa, M ;
Narayan, HS ;
Qiu, Q ;
Bansal, A .
COMPOSITES SCIENCE AND TECHNOLOGY, 1997, 57 (07) :739-751
[48]   Quality Analysis of Ceramic Insulators Under Steep Front Impulse Voltage [J].
Marimuthu, K. ;
Vynatheya, S. ;
Vasudev, N. ;
Raja, P. .
2018 20TH NATIONAL POWER SYSTEMS CONFERENCE (NPSC), 2018,
[49]   Moisture absorption properties of unidirectional glass/polymer composites used in composite (non-ceramic) insulators [J].
Kumosa, L ;
Benedikt, B ;
Armentrout, D ;
Kumosa, M .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2004, 35 (09) :1049-1063
[50]   Diagnostic of non-ceramic insulators aged in a salt fog chamber by using electric field sensor [J].
Ramírez-Vázquez, I ;
Hernández-Corona, R ;
Montoya-Tena, G .
CONFERENCE RECORD OF THE 2004 IEEE INTERNATIONAL SYMPOSIUM ON ELECTRICAL INSULATION, 2004, :471-474