Effects of Solute and Second-Phase Particles on the Texture of Nd-Containing Mg Alloys

被引:121
作者
Hadorn, Jason P. [1 ]
Hantzsche, Kerstin [2 ]
Yi, Sangbong [2 ]
Bohlen, Jan [2 ]
Letzig, Dietmar [2 ]
Agnew, Sean R. [1 ]
机构
[1] Univ Virginia, Dept Mat Sci & Engn, Charlottesville, VA 22904 USA
[2] Helmholtz Ctr Geesthacht, Magnesium Innovat Ctr MagIC, D-21502 Geesthacht, Germany
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2012年 / 43A卷 / 04期
基金
美国国家科学基金会;
关键词
MAGNESIUM SINGLE-CRYSTALS; FOIL THICKNESS MEASUREMENTS; BEAM DIFFRACTION PATTERNS; ABNORMAL GRAIN-GROWTH; DYNAMIC RECRYSTALLIZATION; Y ALLOYS; DEFORMATION MICROSTRUCTURES; MISORIENTATION AXES; PRISMATIC GLIDE; ALUMINUM;
D O I
10.1007/s11661-011-1018-z
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot-rolled, binary Mg-Nd alloys with compositions >= 0.095 at. pct undergo the texture weakening phenomenon that has been reported in a number of Mg-rare earth (RE) alloys. However, alloys with compositions <= 0.01 at. pct retain a strong basal texture typical of pure Mg and other Mg alloys. Measurements of intragranular misorientation axes obtained using electron backscatter diffraction (EBSD) show that more dilute alloys contain predominantly basal < a > dislocations, while richer alloys contain primarily prismatic < a > dislocations. It is suggested that this change in dislocation content is related to a change in the dynamic recrystallization (DRX) mechanism. Metastable second-phase MgxNd1-x intermetallic particles are present within the alloys, and an annealing study indicates that the alloys undergoing texture weakening have grain sizes well predicted by classical Zener drag theory. Even though the more dilute alloys also contain second-phase particles, they are not sufficient to induce pinning. The promotion of nonbasal slip and the reduction in grain boundary mobility due to Zener drag are suggested as controlling mechanisms that promote the observed texture weakening phenomena.
引用
收藏
页码:1363 / 1375
页数:13
相关论文
共 72 条
[21]   AN INSITU STUDY OF PRISMATIC GLIDE IN MAGNESIUM .2. MICROSCOPIC ACTIVATION PARAMETERS [J].
COURET, A ;
CAILLARD, D .
ACTA METALLURGICA, 1985, 33 (08) :1455-1462
[22]   AN INSITU STUDY OF PRISMATIC GLIDE IN MAGNESIUM .1. THE RATE CONTROLLING MECHANISM [J].
COURET, A ;
CAILLARD, D .
ACTA METALLURGICA, 1985, 33 (08) :1447-1454
[23]  
Dunn C.G., 1966, RECRYSTALLIZATION GR, P461
[24]   The roles of oriented nucleation and oriented growth on recrystallization textures in commercial purity aluminium [J].
Engler, O ;
Vatne, HE ;
Nes, E .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 205 (1-2) :187-198
[25]  
Fultz B., 2002, TRANSMISSION ELECT M
[26]   Correlation of plastic deformation and dynamic recrystallization in magnesium alloy Zk60 [J].
Galiyev, A ;
Kaibyshev, R ;
Gottstein, G .
ACTA MATERIALIA, 2001, 49 (07) :1199-1207
[27]   ON THEORY OF EFFECT OF PRECIPITATE PARTICLES ON GRAIN GROWTH IN METALS [J].
GLADMAN, T .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1966, 294 (1438) :298-&
[28]   A thermodynamic assessment of the Mg-Nd binary system using random solution and associate models for the liquid phase [J].
Gorsse, S ;
Hutchinson, CR ;
Chevalier, B ;
Nie, JF .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 392 (1-2) :253-262
[29]  
GRAHAM CD, 1956, T AM I MIN MET ENG, V206, P517
[30]  
Grewen J., 1978, Recrystallization of Metallic Materials, P111