Corrosion rate of pure copper in an oxic bentonite/saline groundwater environment

被引:14
|
作者
Rosborg, B. [1 ]
Kranjc, A. [2 ]
Kuhar, V. [2 ]
Legat, A. [2 ]
机构
[1] Royal Inst Technol, Div Surface & Corros Sci, SE-10044 Stockholm, Sweden
[2] Slovenian Natl Bldg & Civil Engn Inst, SI-1000 Ljubljana, Slovenia
关键词
Pure copper; Bentonite clay; Saline groundwater; Long term exposure; Electrical resistance sensor; Corrosion rate; BEHAVIOR;
D O I
10.1179/1743278210Y.0000000015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The principal strategy for high level radioactive waste disposal in Sweden is to enclose the spent fuel in copper canisters that are embedded in bentonite clay similar to 500 m down in the Swedish bedrock. At this depth, the groundwater is reducing. However, oxic conditions are initially established in the repository during emplacement. The corrosion rate of pure copper in an oxic bentonite/saline groundwater environment has been followed by thin electrical resistance sensors placed in a bentonite test package that was kept at room temperature for 3 years. The corrosion potentials of the sensors have verified oxic conditions in the test package. The corrosion rate of pure copper in this environment has been found to slowly decrease to quite low but measurable values; from above 15 mu m/year down to similar to 1 mu m/year after 3 years of exposure. The measurements have verified a desired behaviour of copper in the environment.
引用
收藏
页码:148 / 152
页数:5
相关论文
共 50 条
  • [1] Copper corrosion in bentonite/saline groundwater solution: Effects of solution and bentonite chemistry
    Kosec, T.
    Qin, Z.
    Chen, J.
    Legat, A.
    Shoesmith, D. W.
    CORROSION SCIENCE, 2015, 90 : 248 - 258
  • [2] An electrochemical impedance spectroscopy study of copper in a bentonite/saline groundwater environment
    Rosborg, Bo
    Pan, Jinshan
    ELECTROCHIMICA ACTA, 2008, 53 (25) : 7556 - 7564
  • [3] Tafel slopes used in monitoring of copper corrosion in a bentonite/groundwater environment
    Rosborg, B
    Pan, JS
    Leygraf, C
    CORROSION SCIENCE, 2005, 47 (12) : 3267 - 3279
  • [4] Electrochemical impedance spectroscopy of pure copper exposed in bentonite under oxic conditions
    Rosborg, Bo
    Kosec, Tadeja
    Kranjc, Andrej
    Pan, Jinshan
    Legat, Andraz
    ELECTROCHIMICA ACTA, 2011, 56 (23) : 7862 - 7870
  • [5] Effect of Sulfide Addition on the Corrosion Mechanism of Copper in Saline Groundwater Solution
    Bojinov, Martin
    Goel, Sneha
    Ikaelaeinen, Tiina
    Saario, Timo
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2024, 171 (04)
  • [6] Influence of temperature on corrosion rate and porosity of corrosion products of carbon steel in anoxic bentonite environment
    Stoulil, J.
    Kanok, J.
    Kouril, M.
    Parschova, H.
    Novak, P.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 443 (1-3) : 20 - 25
  • [7] Cation exchange capacity of bentonite in a saline environment
    Bohac, Peter
    Delavernhe, Laure
    Zervas, Erik
    Koeniger, Franz
    Schuhmann, Rainer
    Emmerich, Katja
    APPLIED GEOCHEMISTRY, 2019, 100 : 407 - 413
  • [8] Influence of Watermelon Seed Extract on the Electrochemical Corrosion Protection of Copper in the Saline Environment
    Maurya, Ravi
    Kumar, Sangam
    Pal, Shivam Kumar
    Ji, Gopal
    Rastogi, Chandresh Kumar
    Journal of Solid Waste Technology and Management, 2024, 50 (03): : 602 - 613
  • [9] Exploring the inhibitory performance of expired moxifloxacin and norfloxacin on copper corrosion in saline environment
    Toghan, Arafat
    Alduaij, Omar K.
    Attia, Azza
    Al Bahir, Areej
    Masoud, Emad M.
    Alhussain, Hanan
    Eldesoky, Ahmed M.
    Farag, Ahmed A.
    Fawzy, Ahmed
    JOURNAL OF ELECTROCHEMICAL SCIENCE AND ENGINEERING, 2025,
  • [10] Stress corrosion cracking of copper in swollen bentonite simulating nuclear waste disposal environment
    Fujimoto, Shinji
    Tsuchiya, Hiroaki
    Ogawa, Soma
    Iida, Yoshihisa
    Taniguchi, Naoki
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2021, 72 (1-2): : 333 - 338