Effects of Melt Superheating on the Microstructure and Tensile Properties of a Ternary Al-15 Wt Pct Si-1.5 Wt Pct Mg Alloy

被引:12
|
作者
Kakitani, Rafael [1 ]
Reyes, Rodrigo V. [2 ]
Garcia, Amauri [1 ]
Cheung, Noe [1 ]
Spinelli, Jose E. [2 ]
机构
[1] Univ Estadual Campinas, UNICAMP, Dept Mfg & Mat Engn, BR-13083860 Campinas, SP, Brazil
[2] Univ Fed Sao Carlos, Dept Mat Engn, BR-13565905 Sao Carlos, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
MECHANICAL-PROPERTIES; DIRECTIONAL SOLIDIFICATION; DENDRITIC MICROSTRUCTURE; SI ALLOYS; COMPOSITE; PARTICLES; ALUMINUM; IMPACT; PHASE; MG2SI;
D O I
10.1007/s11661-018-5058-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Unsteady solidified microstructures of the Al-15 wtpct Si-1.5 wtpct Mg alloy under two degrees of melt superheating are examined: 4 and 21pct above the alloy liquidus temperature. The dendritic array and the eutectic mixture have been investigated, which are affected not only by the solidification kinetics but also by the melt superheating. The directional solidification experiments permitted that aligned Al-rich dendrites could be formed for both high- and low-melt superheatings. These dendrites appear as islands' isolated from each other and dispersed within the -Al+Si+Mg2Si eutectic matrix. Such configuration arises in samples under the entire range of examined cooling rates, i.e., from 0.5 to 50 K/s. Directionally solidified samples having different -Al dendrite interphase spacings have been characterized and subjected to tensile tests. Such microstructural spacings translate the effectiveness in blocking the dislocations motion during loading, which is promoted mainly by the dendritic/eutectic boundaries. This mechanism is especially operative since the applied tensile load is perpendicular to the dendritic growth path. As such, the evolution of tensile properties as a function of these spacings was assessed. Both elongation () and the ultimate strength (sigma(u)) are enhanced nearly by 40pct due to the reduction in the dendrite interphase spacing. The highest properties (sigma(u): 310MPa and : 7pct) are associated with a microstructure formed by aligned dendrites with 70m in spacing embedded in a eutectic mixture. Three factors appear to contribute to the higher strength values observed for the alloy processed under lower-melt superheating, i.e., higher fraction of dendrites, solid solution strengthening of Mg in -Al, and finer eutectic Si spacing.
引用
收藏
页码:1308 / 1322
页数:15
相关论文
共 50 条
  • [21] An observation on microstructure of a casting Zn-40 Wt pct al alloy
    Xiaolei Xu
    Zhiwei Yu
    Yaqin Shi
    Yongqing Ma
    Zukun Hei
    Metallurgical and Materials Transactions A, 1998, 29 : 2477 - 2481
  • [22] EFFECT OF MELT CLEANLINESS ON THE PROPERTIES OF AN AL-10 WT PCT SI-10 VOL PCT SIC(P) COMPOSITE
    SAMUEL, FH
    LIU, H
    SAMUEL, AM
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (07): : 1631 - 1645
  • [23] Microstructures and tensile properties of an A1-12 wt pct Si alloy produced by reciprocating extrusion
    Yeh, JW
    Yuan, SY
    Peng, CH
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (09): : 2503 - 2512
  • [24] Microstructures and tensile properties of an A1-12 wt pct Si alloy produced by reciprocating extrusion
    Jien-Wei Yeh
    Shi-Ying Yuan
    Chao-Hung Peng
    Metallurgical and Materials Transactions A, 1999, 30 : 2503 - 2512
  • [25] EFFECT OF HEAT-TREATMENT ON THE MICROSTRUCTURE, TENSILE PROPERTIES, AND FRACTURE-BEHAVIOR OF PERMANENT-MOLD AL-10 WT PCT SI-0.6 WT PCT MG/SIC/10(P), COMPOSITE CASTINGS
    SAMUEL, FH
    SAMUEL, AM
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (10): : 2247 - 2263
  • [26] Effect of dendritic arm spacing on mechanical properties and corrosion resistance of Al 9 Wt Pct Si and Zn 27 Wt Pct Al alloys
    Wislei R. Osorio
    Pedro R. Goulart
    Amauri Garcia
    Givanildo A. Santos
    Carlos Moura Neto
    Metallurgical and Materials Transactions A, 2006, 37 : 2525 - 2538
  • [27] Effect of dendritic arm spacing on mechanical properties and corrosion resistance of Al 9 Wt Pct Si and Zn 27 Wt Pct Al alloys
    Osorio, Wislei R.
    Goulart, Pedro R.
    Santos, Givanildo A.
    Moura Neto, Carlos
    Garcia, Amauri
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (08): : 2525 - 2538
  • [28] Effect of silicon particles on the fatigue crack growth characteristics of Al-12 wt pct Si-0.35 wt pct Mg-(0 to 0.02) wt pct Sr casting alloys
    NatSteel Ltd, Singapore, Singapore
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1995, 26 A (06): : 1553 - 1570
  • [29] INFLUENCE OF QUENCHING ON SEGREGATION OF MAGNESIUM TO GRAIN-BOUNDARIES IN AN AL-5.9 WT PCT ZN-3.2 WT PCT MG ALLOY
    DOIG, P
    EDINGTON, JW
    METALLURGICAL TRANSACTIONS, 1975, A 6 (04): : 943 - 945
  • [30] INTERMETALLIC PHASES FORMED DURING DC-CASTING OF AN AL-0.25 WT PCT FE-0.13 WT PCT SI ALLOY
    SKJERPE, P
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1987, 18 (02): : 189 - 200