In situ crystallization of high performing WO3-based electrochromic materials and the importance for durability and switching kinetics
被引:82
作者:
Lin, Feng
[2
]
Cheng, Jifang
[1
]
Engtrakul, Chaiwat
[2
]
Dillon, Anne C.
[2
]
Nordlund, Dennis
[4
]
Moore, Rob G.
[4
]
Weng, Tsu-Chien
[4
]
Williams, S. K. R.
[1
]
Richards, Ryan M.
[1
,3
]
机构:
[1] Colorado Sch Mines, Dept Chem & Geochem, Golden, CO 80401 USA
[2] Natl Renewable Energy Lab, Golden, CO 80401 USA
[3] Colorado Sch Mines, Mat Sci Program, Golden, CO 80401 USA
[4] SLAC Natl Accelerator Lab, Menlo Pk, CA 94025 USA
基金:
美国国家科学基金会;
关键词:
WO3;
THIN-FILMS;
TUNGSTEN-OXIDE NANOPARTICLES;
CHEMICAL-VAPOR-DEPOSITION;
X-RAY-ABSORPTION;
ELECTRONIC-STRUCTURE;
CRYSTALLINITY;
PERIODICITY;
D O I:
10.1039/c2jm32742b
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
A chemical self-assembled synthesis was used to prepare disordered porous semicrystalline WO3-based cathodic electrochromic films. The resulting films were characterized with transmission electron microscopy (TEM), scanning electron microscopy (SEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), N-2 physisorption, Fourier transform infrared spectroscopy (FTIR) and near-edge X-ray absorption fine structure (NEXAFS). The electrochromic performance was evaluated in a Li-ion electrolyte (i. e., 1 M LiClO4 dissolved in propylene carbonate) with cyclic voltammetry (CV), galvanostatic cycling with potential limitation (GCPL) and chronoamperometry (CA) techniques. It is demonstrated that the crystallinity of WO3 thin films can be readily tuned with the variation of annealing temperatures and TiO2 addition. The results demonstrated excellent stability and durability (i. e., 1500 GCPL cycles in 32 days) for WO3 electrode annealed at 350 degrees C, ultrafast switching kinetics for WO3-TiO2 electrode (i. e., bleaching and coloration times are 5.5 s and 4.2 s, respectively) and excellent charge reversibility (% R approximate to 100%). Electrochemical, TEM and Raman spectroscopy studies suggest that a change in degree of crystallinity in WO3 occurs during the extended durability test, which then influences the durability and switching kinetics.