Cracking Process in Delayed Fracture of High-Strength Steel after Long Atmospheric Exposure

被引:8
作者
Homma, Tomoka [1 ]
Chiba, Takahiro [1 ]
Takai, Kenichi [2 ]
Akiyama, Eiji [3 ]
Oshikawa, Wataru [4 ]
Nagumo, Michihiko [5 ]
机构
[1] Sophia Univ, Grad Sch, Chiyoda Ku, 7-1 Kioi Cho, Tokyo 1028544, Japan
[2] Sophia Univ, Dept Engn & Appl Sci, Chiyoda Ku, 7-1 Kioi Cho, Tokyo 1028544, Japan
[3] Tohoku Univ, Inst Mat Res, Aoba Ku, Katahira 2-1-1, Sendai, Miyagi 9808577, Japan
[4] Univ Ryukyus, Fac Engn, Nakagami, Okinawa 9030213, Japan
[5] Waseda Univ, Lab Mat Sci & Technol, Shinjuku Ku, NishiWaseda 2-8-26, Tokyo 1690051, Japan
关键词
hydrogen embrittlement; delayed fracture; high-strength steel; atmospheric exposure; fractography; cracking; ENHANCED LOCALIZED PLASTICITY; HYDROGEN-RELATED FRACTURE; MARTENSITIC STEEL; DUCTILE FRACTURE; EMBRITTLEMENT; FAILURE; SUSCEPTIBILITY; DEFORMATION; MECHANISM; BEHAVIOR;
D O I
10.2355/isijinternational.ISIJINT-2021-238
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper is the first microscopic observation of the entire cracking process in delayed fracture of high-strength steel bolt after long-term atmospheric exposure. A sufficiently fresh fracture surface exhibits the initiation of the propagating crack in a thin zone beneath the screw groove, resulting from the merging of multiple cracks nucleated therein. The fracture morphology is initially intergranular, exhibiting the three-dimensional shape of prior austenite grains, but the stress and strain states at the nucleation sites are not uniquely specified. The fracture morphology alters as the crack extends from intergranular to quasi-cleavage and fine dimples, associated with increasing stress intensity under a constant-displacement condition. The change from inter- to trans-granular fracture is continuous, implying affinity among different morphologies associated with the increased density and the distribution of potential crack nucleation sites in the crack front. The crack propagation in the quasi-cleavage and fine dimple regions is step-wise of about 50 mu m per step. Recent studies about the function of hydrogen in embrittlement are referred to in respect of the accumulation of strain-induced damage. The enhanced generation of strain-induced vacancies is the presumable function of hydrogen compatible with the present findings.
引用
收藏
页码:776 / 787
页数:12
相关论文
共 62 条
  • [1] [Anonymous], 1995, B1186 JIS, P23
  • [2] [Anonymous], 2010, 91 JSSC
  • [3] BEACHEM CD, 1972, METALL TRANS, V3, P437
  • [4] Birnbaum H.K., 1990, HYDROGEN EFFECTS MAT, P639
  • [5] HYDROGEN-ENHANCED LOCALIZED PLASTICITY - A MECHANISM FOR HYDROGEN-RELATED FRACTURE
    BIRNBAUM, HK
    SOFRONIS, P
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 176 (1-2): : 191 - 202
  • [6] Void growth in single crystal Copper-an atomistic modeling and statistical analysis study
    Chandra, S.
    Samal, M. K.
    Chavan, V. M.
    Raghunathan, S.
    [J]. PHILOSOPHICAL MAGAZINE, 2018, 98 (07) : 577 - 604
  • [7] Ductile fracture by vacancy condensation in FCC single crystals
    Cuitino, AM
    Ortiz, M
    [J]. ACTA MATERIALIA, 1996, 44 (02) : 427 - 436
  • [8] Das T., 2017, MAT PERFORMANCE HYDR, P132
  • [9] Dieudonne T., 2017, MAT PERFORMANCE HYDR, P114
  • [10] Hydrogen-enhanced lattice defect formation and hydrogen embrittlement of cyclically prestressed tempered martensitic steel
    Doshida, T.
    Nakamura, M.
    Saito, H.
    Sawada, T.
    Takai, K.
    [J]. ACTA MATERIALIA, 2013, 61 (20) : 7755 - 7766