Influence of Controlled Acidity of Hole-Collecting Buffer Layers on the Performance and Lifetime of Polymer:Fullerene Solar Cells

被引:73
作者
Kim, Hwajeong [3 ,5 ]
Nam, Sungho [3 ]
Lee, Hyena [3 ]
Woo, Sungho [3 ,6 ]
Ha, Chang-Sik [4 ]
Ree, Moonhor [1 ,2 ]
Kim, Youngkyoo [3 ]
机构
[1] Pohang Univ Sci & Technol POSTECH, Ctr Electrophoto Behav Adv Mol Syst, Div Adv Mat Sci, Dept Chem,BK Sch Mol Sci, Pohang 790784, South Korea
[2] Pohang Univ Sci & Technol POSTECH, Polymer Res Inst, Pohang 790784, South Korea
[3] Kyungpook Natl Univ, Dept Chem Engn, Organ Nanoelect Lab, Taegu 702701, South Korea
[4] Pusan Natl Univ, Dept Polymer Sci & Engn, Pusan 609735, South Korea
[5] Kyungpook Natl Univ, Res Inst Adv Energy Technol, Prior Res Ctr, Taegu 702701, South Korea
[6] Daegu Gyeongbuk Inst Sci & Technol DGIST, Green Energy Res Div, Taegu 711873, South Korea
基金
新加坡国家研究基金会;
关键词
FULLERENE; FILMS; POLY(3-HEXYLTHIOPHENE); DEGRADATION; MORPHOLOGY; BLENDS; PSS; ITO;
D O I
10.1021/jp2028615
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
We report the influence of the controlled acidity of the hole-collecting buffer layer, poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS), on the performance and lifetime of polymer:fullerene solar cells. The acidity was controlled by adding a strong base (NaOH) to the pristine PEDOT:PSS solutions. The NaOH-modified PEDOT:PSS layers were used for fabricating polymer:fullerene solar cells with active layers made from blend films of poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl-C-61-butyric acid methyl ester (PC61BM). The results showed that a small addition of NaOH (0.2 molar ratio) removed 23% of the sulfonic acid groups but did not change the device performance, even though further NaOH addition degraded the, device performance owing to an increased sheet resistance and lowered work function, as well as a changed surface morphology. Storage lifetime tests showed that the device with the modified PEDOT:PSS layer (0.2 molar ratio NaOH) was almost not degraded, whereas the pristine PEDOT:PSS layer might affect the deterioration at the interface with the active layer (P3HT: PCBM). Under 1 sun illumination for 10 h, the modified PEDOT:PSS layer (0.2 molar ratio NaOH) resulted in similar to 25% improved lifetime, which is in excellent agreement with the extent of reduction of the sulfonic acid groups (similar to 23%).
引用
收藏
页码:13502 / 13510
页数:9
相关论文
共 35 条
[31]  
Skotheim T.A., 2007, Handbook of Conducting Polymers, VThird
[32]   Long-term operational lifetime and degradation analysis of P3HT: PCBM photovoltaic cells [J].
Voroshazi, Eszter ;
Verreet, Bregt ;
Aernouts, Tom ;
Heremans, Paul .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2011, 95 (05) :1303-1307
[33]   Effect of solvent on PEDOT/PSS nanometer-scaled thin films: XPS and STEM/AFM studies [J].
Yan, Hu ;
Okuzaki, Hidenori .
SYNTHETIC METALS, 2009, 159 (21-22) :2225-2228
[34]   POLYMER PHOTOVOLTAIC CELLS - ENHANCED EFFICIENCIES VIA A NETWORK OF INTERNAL DONOR-ACCEPTOR HETEROJUNCTIONS [J].
YU, G ;
GAO, J ;
HUMMELEN, JC ;
WUDL, F ;
HEEGER, AJ .
SCIENCE, 1995, 270 (5243) :1789-1791
[35]   Electrochemical and XPS studies toward the role of monomeric and polymeric sulfonate counterions in the synthesis, composition, and properties of poly(3,4-ethylenedioxythiophene) [J].
Zotti, G ;
Zecchin, S ;
Schiavon, G ;
Louwet, F ;
Groenendaal, L ;
Crispin, X ;
Osikowicz, W ;
Salaneck, W ;
Fahlman, M .
MACROMOLECULES, 2003, 36 (09) :3337-3344