Hot -cracking resistivity of dissimilar clads using Inconel 52 and 308L stainless steel on carbon steel

被引:9
|
作者
Kim, Yookyung [1 ,2 ]
Nam, Hyunbin [2 ]
Lee, Junghun [2 ]
Park, Chulho [3 ]
Moon, Byungrok [2 ]
Nam, Dae-Geun [4 ]
Lee, Seung Hwan [5 ]
Kang, Namhyun [2 ]
机构
[1] Nucl Power Plant BG, Doosan Heavy Ind, Chang Won, South Korea
[2] Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
[3] Chosun Univ, Dept Welding & Joining Sci Engn, Gwanju 61452, South Korea
[4] Korea Inst Ind Technol, Dongnam Reg Div, Busan 46, South Korea
[5] Korea Aerosp Univ, Sch Aerosp & Mech Engn, Goyang Si 10540, Gyeonggi Do, South Korea
基金
新加坡国家研究基金会;
关键词
Hot-cracking resistivity; Inconel; 52; Stainless steel 308L; Laves phase; Transition zone; Delta-ferrite; SOLIDIFICATION CRACKING; MECHANICAL-PROPERTIES; WELD METALS; ALLOY; NB; WELDABILITY; MICROSTRUCTURE; PHASE; SIGMA;
D O I
10.1016/j.jnucmat.2020.152103
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigates the effect of a built-up sequence on the hot-cracking resistivity of dissimilar clads. Dissimilar clads of Inconel 52 and austenitic stainless steel (STS) 308L were produced using submerged arc-welding of the carbon steel. Hot-cracking occurred near the fusion boundary when the STS 308L was cladded to the buffer layer of Inconel 52 (STS 308L/Inconel 52 clad). Causative factors were identified as: (i) the wide transition zone in the interface between the dissimilar clads, and (ii) the eutectic-type Laves phase having a high level of S and P contents and a continuous geometry of thin films formed along the grain boundary. Hot cracks did not appear when Inconel 52 was cladded to the buffer layer of 308L stainless steel (Inconel 52/STS 308L clad). Hot-cracking resistivity was significantly improved by forming d-ferrite in the interfacial boundary for the Inconel 52/STS 308 L clad. (c) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:6
相关论文
共 50 条
  • [41] A study on wire arc additive manufacturing of 308L austenitic stainless steel cylindrical components: Optimisation, microstructure and mechanical properties
    Nagasai, Bellamkonda Prasanna
    Malarvizhi, Sudersanan
    Balasubramanian, Visvalingam
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2023, 237 (09) : 1391 - 1404
  • [42] Effect of post-irradiation annealing on microstructure and corrosion of proton-irradiated 308L stainless steel weld metal
    Lin, Xiaodong
    Han, En-Hou
    Peng, Qunjia
    Ke, Wei
    Jiao, Zhijie
    CORROSION SCIENCE, 2020, 175
  • [43] Stress-assisted oxidation behaviour of inconel 52M/316 austenitic stainless-steel dissimilar weld joints in a simulated pressurised water reactor
    Xu, Youwei
    Yang, Binhui
    Shi, Yu
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2022, 54 (10) : 3778 - 3787
  • [44] Evolutions of microstructure and mechanical property of 308L stainless steel repaired by the local dry underwater wire arc additive manufacturing
    Liao, Haipeng
    Wang, Zhenmin
    Chi, Peng
    Zhang, Bin
    Ding, Tao
    Zhang, Qin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 898
  • [45] Experimental investigation of the effect of laser parameters on the weld bead shape and temperature distribution during dissimilar laser welding of stainless steel 308 and carbon steel St 37
    Dong, Xinmin
    Wang, Guofang
    Ghaderi, Mohammad
    INFRARED PHYSICS & TECHNOLOGY, 2021, 116
  • [46] The Effect of Welding Parameters on Joining Dissimilar Low Carbon Steel and 3CR12 Ferritic Stainless Steel by GTAW with ER308L Filler Metal
    Luijan, Jinkamon
    Surin, Prayoon
    Eidhed, Krittee
    4TH INTERNATIONAL CONFERENCE ON MECHANICAL, AERONAUTICAL AND AUTOMOTIVE ENGINEERING (ICMAA 2020), 2020, 1519
  • [47] Fabrication and characterization of stainless steel 308 L/Inconel 625 functionally graded material with continuous change in composition by dual-wire arc additive manufacturing
    Li, Tianxu
    Wang, Zhijiang
    Yang, Zhenwen
    Shu, Xinxin
    Xu, Jun
    Wang, Ying
    Hu, Shengsun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 915
  • [48] Mitigation of hot cracking of alloy 52M overlay on cast stainless steel CF8A
    Shih, Y. -J.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2013, 18 (07) : 566 - 572
  • [49] Investigation of ER308L and ER309L filler wires on dissimilar metals between carbon steel and 3CR12 ferritic stainless steel by GTAW through boiler fabrication in a sugar factory
    Luijan, Jinkamon
    Surin, Prayoon
    Eidhed, Kittee
    MATERIALS RESEARCH EXPRESS, 2023, 10 (12)
  • [50] A Study on Dissimilar Welding of AISI 1020 Carbon Steel and AISI 201 Stainless Steel Using Flux Core Arc Welding Processes
    Abbas, Mahmoud
    Bastawesy, Gamal
    Abdel-Aleem, Hamed A.
    EGYPTIAN JOURNAL OF CHEMISTRY, 2025, 68 (04): : 75 - 89