Hot -cracking resistivity of dissimilar clads using Inconel 52 and 308L stainless steel on carbon steel

被引:9
|
作者
Kim, Yookyung [1 ,2 ]
Nam, Hyunbin [2 ]
Lee, Junghun [2 ]
Park, Chulho [3 ]
Moon, Byungrok [2 ]
Nam, Dae-Geun [4 ]
Lee, Seung Hwan [5 ]
Kang, Namhyun [2 ]
机构
[1] Nucl Power Plant BG, Doosan Heavy Ind, Chang Won, South Korea
[2] Pusan Natl Univ, Dept Mat Sci & Engn, Busan 46241, South Korea
[3] Chosun Univ, Dept Welding & Joining Sci Engn, Gwanju 61452, South Korea
[4] Korea Inst Ind Technol, Dongnam Reg Div, Busan 46, South Korea
[5] Korea Aerosp Univ, Sch Aerosp & Mech Engn, Goyang Si 10540, Gyeonggi Do, South Korea
基金
新加坡国家研究基金会;
关键词
Hot-cracking resistivity; Inconel; 52; Stainless steel 308L; Laves phase; Transition zone; Delta-ferrite; SOLIDIFICATION CRACKING; MECHANICAL-PROPERTIES; WELD METALS; ALLOY; NB; WELDABILITY; MICROSTRUCTURE; PHASE; SIGMA;
D O I
10.1016/j.jnucmat.2020.152103
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigates the effect of a built-up sequence on the hot-cracking resistivity of dissimilar clads. Dissimilar clads of Inconel 52 and austenitic stainless steel (STS) 308L were produced using submerged arc-welding of the carbon steel. Hot-cracking occurred near the fusion boundary when the STS 308L was cladded to the buffer layer of Inconel 52 (STS 308L/Inconel 52 clad). Causative factors were identified as: (i) the wide transition zone in the interface between the dissimilar clads, and (ii) the eutectic-type Laves phase having a high level of S and P contents and a continuous geometry of thin films formed along the grain boundary. Hot cracks did not appear when Inconel 52 was cladded to the buffer layer of 308L stainless steel (Inconel 52/STS 308L clad). Hot-cracking resistivity was significantly improved by forming d-ferrite in the interfacial boundary for the Inconel 52/STS 308 L clad. (c) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:6
相关论文
共 50 条
  • [31] Microstructures and hot cracking formed at the interface of Zircaloy-4/stainless-steel-304L junctions
    Lebaili, Abdelatif
    CANADIAN METALLURGICAL QUARTERLY, 2023, 62 (04) : 690 - 700
  • [32] Efficiency of dissimilar friction welded 1045 medium carbon steel and 316L austenitic stainless steel joints
    Khidhir, Gawhar Ibraheem
    Baban, Sherko A.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (02): : 1926 - 1932
  • [33] Solid-state dissimilar joining of stainless steel 316L and Inconel 718 alloys by electrically assisted pressure joining
    Li, Yong-Fang
    Hong, Sung-Tae
    Choi, Howook
    Han, Heung Nam
    MATERIALS CHARACTERIZATION, 2019, 154 : 161 - 168
  • [34] Insight into the galvanic corrosion behaviour of low alloy steel A508/309 L/308 L stainless steel dissimilar metal weld at different temperatures.
    Okonkwo, Bright O.
    Ming, Hongliang
    Li, Zimin
    Li, Li
    Chen, Yimian
    Peng, Jiajing
    Wang, Jianqiu
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [35] Influence of Deposition Mode on Microstructural and Mechanical Properties of Wire Arc Additive Manufactured 308L Stainless Steel Structures
    Paul, Amrit Raj
    Mukherjee, Manidipto
    Singh, Dilpreet
    Raja, Manivannan
    Mondal, Manas Kumar
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (14) : 7345 - 7367
  • [36] Interactive effect of thermal aging and proton irradiation on microstructural evolution and hardening of 8-ferrite in 308L stainless steel weld metal
    Gao, Xiaodong
    Lin, Xiaodong
    Guo, Tao
    Xu, Lining
    Han, Yaolei
    Jiang, Baolong
    Mei, Xingyuan
    Peng, Qunjia
    Qiao, Lijie
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 170 : 140 - 155
  • [37] Influences of the process parameter and thermal cycles on the quality of 308L stainless steel walls produced by additive manufacturing utilizing an arc welding source
    Le, Van Thao
    Mai, Dinh Si
    Bui, Manh Cuong
    Wasmer, Kilian
    Nguyen, Van Anh
    Dinh, Duc Manh
    Nguyen, Van Canh
    Vu, Duong
    WELDING IN THE WORLD, 2022, 66 (08) : 1565 - 1580
  • [38] Dissimilar Friction Stir Welding of Carbon Steel and Stainless Steel: Some Observation on Microstructural Evolution and Stress Corrosion Cracking Performance
    Mohd Joharif Bin Matlan
    Hamed Mohebbi
    Srinivasa Rao Pedapati
    Mokhtar B. Awang
    Mokhtar Che Ismail
    Saeid Kakooei
    Nsikan Etim Dan
    Transactions of the Indian Institute of Metals, 2018, 71 : 2553 - 2564
  • [39] Microscale investigation of the correlation between microstructure and galvanic corrosion of low alloy steel A508 and its welded 309/308L stainless steel overlayer
    Okonkwo, Bright O.
    Ming, Hongliang
    Zhang, Zhiming
    Wang, Jianqiu
    Rahimi, Ehsan
    Hosseinpour, Saman
    Davoodi, Ali
    CORROSION SCIENCE, 2019, 154 : 49 - 60
  • [40] Solidification Cracking Susceptibility of Alloy 52 Weld Overlay on 316L Stainless Steel
    Chung, W. C.
    Tsay, L. W.
    Chen, C.
    PHYSICAL AND NUMERICAL SIMULATION OF MATERIAL PROCESSING VI, PTS 1 AND 2, 2012, 704-705 : 529 - +