Mechanical and microstructural characterization of Ti-SiC reinforced AA5083 surface composites fabricated via friction stir process

被引:3
|
作者
Rahman, Md Ziyaur [1 ]
Khan, Zahid A. [1 ]
Siddiquee, Arshad Noor [1 ]
Abidi, Mustufa Haider [2 ]
Aboudaif, Mohamed K. [2 ]
Al-Ahmari, Abdulrahman [2 ,3 ]
机构
[1] Jamia Millia Islamia, Dept Mech Engn, Fac Engn & Technol, New Delhi 110025, India
[2] King Saud Univ, Adv Mfg Inst, Raytheon Chair Syst Engn, Riyadh 11421, Saudi Arabia
[3] King Saud Univ, Coll Engn, Ind Engn Dept, Riyadh 11421, Saudi Arabia
关键词
metal matrix composites (MMC); friction stir processing (FSP); microstructure investigation; mechanical characterization; TOOL GEOMETRY; ALLOY; PARAMETERS; NANO-ZRO2; TOUGHNESS;
D O I
10.1088/2053-1591/ac433b
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A mixture of Titanium and silicon-carbide powders was embedded in the AA5083 matrix by Friction Stir Processing (FSP). Experiments were performed as per Taguchi L8 orthogonal array, and the effect of reinforcement on hot strength (at 100 degrees C), processed zone (PZ) geometry, and microstructure were investigated. The effect of PZ geometry on the surface properties was also analyzed. The effect of heating the tensile test specimens to 540 degrees C on the strength at 100 degrees C was also separately investigated. It was observed that surface hardness was significantly enhanced by FSP, and the highest mean hardness of 90.4 HV was observed. Furthermore, it was observed that the surface properties also significantly depend on PZ geometry. From experimental results, it was found that the specimens with the lowest width to depth ratio bears the highest hardness and vice versa. A clear effect of parameters was evident on the geometry of processed zones with a deep bowl, and shallow cup-shaped zones were formed with smaller and larger shoulder diameters, respectively. The samples were processed at 355 rpm, 63 mm min(-1), 17 mm shoulder, and 355 rpm, 80 mm min(-1). The 20 mm shoulder showed high tensile strength 292 MPa and 294 Mpa, respectively. The strength of these samples did not reduce much even after heating to 540 degrees C.
引用
收藏
页数:14
相关论文
共 50 条
  • [11] Influence of SiC Content on Microstructure and Tribological Properties of Friction Stir-Processed SiC/AA5083 Surface Composites
    Vikram Kumar S. Jain
    S. Muthukumaran
    Metallurgical and Materials Transactions A, 2019, 50 : 2933 - 2944
  • [12] Microstructure, Mechanical and Sliding Wear Behavior of AA5083–B4C/SiC/TiC Surface Composites Fabricated Using Friction Stir Processing
    Vikram Kumar S. Jain
    P. M. Muhammed
    S. Muthukumaran
    S. P. Kumaresh Babu
    Transactions of the Indian Institute of Metals, 2018, 71 : 1519 - 1529
  • [13] Mechanical and microstructural properties of friction stir welded AA5083 and AA5754 aluminium alloys
    Tolun, F.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2021, 59 (03): : 149 - 160
  • [14] Effect of process parameters of mechanical studies on friction stir welded AA5083 by GRA
    Kumar Gummadi A.
    Amudha K.
    Srinivasa Rao M.S.
    Sharma P.
    Shalini S.
    Kumarnath J.
    Materials Today: Proceedings, 2023, 77 : 540 - 544
  • [15] Mechanical and Microstructural Characterization of Hybrid Cu-SiC-Zn Composites Fabricated Via Friction Stir Processing
    Barmouz, Mohsen
    Zall, Vahid
    Pashazadeh, Hamed
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2016, 19 (06): : 1292 - 1298
  • [16] Investigation of process parameters and tool design on friction stir channeling (FSC) of AA5083 monolithic plates and microstructural characterization
    Ioannis Papantoniou
    Panagiotis Karmiris-Obratański
    Dimitrios Manolakos
    The International Journal of Advanced Manufacturing Technology, 2022, 121 : 981 - 992
  • [17] Investigation of process parameters and tool design on friction stir channeling (FSC) of AA5083 monolithic plates and microstructural characterization
    Papantoniou, Ioannis
    Karmiris-Obratanski, Panagiotis
    Manolakos, Dimitrios
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 121 (1-2): : 981 - 992
  • [18] Influence of friction stir processing on wear behavior of nanosized SiC reinforced AA5083 nanocomposites developed by stir casting
    Rajan, Gaurav
    Kumar, Atul
    Mula, Suhrit
    JOURNAL OF MANUFACTURING PROCESSES, 2025, 141 : 1631 - 1649
  • [19] Investigation on the machinability of Biochar reinforced AA5083 Metal Matrix composites fabricated by stir casting technique
    Praveen, K.
    Raja, R.
    Jannet, Sabitha
    George, Lijin
    ENGINEERING RESEARCH EXPRESS, 2024, 6 (01):
  • [20] Mechanical properties of cryogenically treated AA5083 friction stir welds
    Vasudevan, Neelamegam
    Bhaskar, Govindasamy Bhavani
    Rao, Tadivaka Srinivasa
    Mohandass, Muthukrishnan
    MATERIALS TESTING, 2019, 61 (12) : 1129 - 1134