Deformation microstructures as well as strengthening and toughening mechanisms of low-density high Mn steels for cryogenic applications

被引:24
作者
Chen, Jun [1 ]
Ren, Jia-kuan [1 ]
Liu, Zhen-yu [1 ]
机构
[1] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2021年 / 13卷
基金
国家重点研发计划;
关键词
High Mn steel; Low density; Planar defects; Strength; Cryogenic impact toughness; CHARPY IMPACT TOUGHNESS; TEMPERATURE BRITTLE-FRACTURE; FATIGUE-CRACK-PROPAGATION; INDUCED PLASTICITY STEELS; STACKING-FAULT ENERGY; HIGH-MANGANESE; GRAIN-SIZE; TWIN INTERACTIONS; AUSTENITIC STEEL; AL ADDITION;
D O I
10.1016/j.jmrt.2021.05.018
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The three Al-bearing high Mn steels were prepared to investigate the effect of Al on microstructures as well as tensile and cryogenic impact properties. The Al addition leads to three strengthening modes of solid-solution, grain refinement and delta-ferrite. The former two strengthening modes can increase yield strength from 406 to 467 MPa with increasing Al content from similar to 3.0 to similar to 5.0 wt%. Once the Al content reaches similar to 8.0 wt%, the yield strength reaches 588 MPa owing to the formation of delta-ferrite. The changes in major deformation mechanisms are sufficient twinning plus deformation bands -> a little twinning plus deformation bands -> nearly no twinning plus highly dense dislocation walls as the Al content increases from similar to 3.0 to similar to 8.0 wt%. A loss in total elongation is mainly due to the suppression of twinning in the 5Al and 8Al steels. However, under an impact loading at similar to 196 degrees C, the major deformation mechanisms are cross twinning and highly dense dislocation walls in the 3Al and 5Al steels, leading to ductile dimpled fracture as well as high impact absorbed energies of similar to 122 and similar to 138 J for the 3Al and 5Al steels, respectively. The toughening modes contain high angle grain boundaries induced deflections of a crack, cross planar defects induced tortuousness of a crack in grain interior and a large plastic deformation dissipating energy. In addition, it is due to the formation of delta-ferrite that the 8Al steel becomes a brittle material at similar to 196 degrees C. The delta-ferrite induced cryogenic brittlement (delta-ICB) effect was sufficiently discussed. (C) 2021 The Author(s). Published by Elsevier B.V.
引用
收藏
页码:947 / 961
页数:15
相关论文
共 62 条
  • [51] Effect of Al addition on low-cycle fatigue properties of hydrogen charged high-Mn TWIP steels
    Song, Seok Weon
    Kwon, Young Jin
    Lee, Taekyung
    Lee, Chong Soo
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 677 : 421 - 430
  • [52] FRACTURE PROCESS OF A LOW-CARBON LOW-ALLOY STEEL RELEVANT TO CHARPY TOUGHNESS AT DUCTILE-BRITTLE FRACTURE TRANSITION REGION
    TANI, T
    NAGUMO, M
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (02): : 391 - 399
  • [53] CLEAVAGE-LIKE FRACTURE ALONG SLIP PLANES IN FE-18CR-3NI-13MN-0.37N AUSTENITIC STAINLESS-STEEL AT LIQUID-HELIUM TEMPERATURE
    TOBLER, RL
    MEYN, D
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (06): : 1626 - 1631
  • [54] Mechanism of low temperature brittle fracture in high nitrogen bearing austenitic steels
    Tomota, Y
    Xia, Y
    Inoue, K
    [J]. ACTA MATERIALIA, 1998, 46 (05) : 1577 - 1587
  • [55] New twinning route in face-centered cubic nanocrystalline metals
    Wang, Lihua
    Guan, Pengfei
    Teng, Jiao
    Liu, Pan
    Chen, Dengke
    Xie, Weiyu
    Kong, Deli
    Zhang, Shengbai
    Zhu, Ting
    Zhang, Ze
    Ma, Evan
    Chen, Mingwei
    Han, Xiaodong
    [J]. NATURE COMMUNICATIONS, 2017, 8
  • [56] Evading the strength- ductility trade-off dilemma in steel through gradient hierarchical nanotwins
    Wei, Yujie
    Li, Yongqiang
    Zhu, Lianchun
    Liu, Yao
    Lei, Xianqi
    Wang, Gang
    Wu, Yanxin
    Mi, Zhenli
    Liu, Jiabin
    Wang, Hongtao
    Gao, Huajian
    [J]. NATURE COMMUNICATIONS, 2014, 5
  • [57] Influence of Al content on the strain-hardening behavior of aged low density Fe-Mn-Al-C steels with high Al content
    Wu, Z. Q.
    Ding, H.
    An, X. H.
    Han, D.
    Liao, X. Z.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 639 : 187 - 191
  • [58] Relationships among crystallographic texture, fracture behavior and Charpy impact toughness in API X100 pipeline steel
    Yang, Xiao-Long
    Xu, Yun-Bo
    Tan, Xiao-Dong
    Wu, Di
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 641 : 96 - 106
  • [59] Origin of Extended Tensile Ductility of a Fe-28Mn-10Al-1C Steel
    Yoo, J. D.
    Hwang, S. W.
    Park, K. -T.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (07): : 1520 - 1523
  • [60] Effect of stacking faults on the ductility of Fe-18Mn-1.5Al-0.6C twinning-induced plasticity steel at low temperatures
    Yoo, Joon
    Choi, Kayoung
    Zargaran, A.
    Kim, Nack J.
    [J]. SCRIPTA MATERIALIA, 2017, 137 : 18 - 21