Deformation microstructures as well as strengthening and toughening mechanisms of low-density high Mn steels for cryogenic applications

被引:24
作者
Chen, Jun [1 ]
Ren, Jia-kuan [1 ]
Liu, Zhen-yu [1 ]
机构
[1] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2021年 / 13卷
基金
国家重点研发计划;
关键词
High Mn steel; Low density; Planar defects; Strength; Cryogenic impact toughness; CHARPY IMPACT TOUGHNESS; TEMPERATURE BRITTLE-FRACTURE; FATIGUE-CRACK-PROPAGATION; INDUCED PLASTICITY STEELS; STACKING-FAULT ENERGY; HIGH-MANGANESE; GRAIN-SIZE; TWIN INTERACTIONS; AUSTENITIC STEEL; AL ADDITION;
D O I
10.1016/j.jmrt.2021.05.018
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The three Al-bearing high Mn steels were prepared to investigate the effect of Al on microstructures as well as tensile and cryogenic impact properties. The Al addition leads to three strengthening modes of solid-solution, grain refinement and delta-ferrite. The former two strengthening modes can increase yield strength from 406 to 467 MPa with increasing Al content from similar to 3.0 to similar to 5.0 wt%. Once the Al content reaches similar to 8.0 wt%, the yield strength reaches 588 MPa owing to the formation of delta-ferrite. The changes in major deformation mechanisms are sufficient twinning plus deformation bands -> a little twinning plus deformation bands -> nearly no twinning plus highly dense dislocation walls as the Al content increases from similar to 3.0 to similar to 8.0 wt%. A loss in total elongation is mainly due to the suppression of twinning in the 5Al and 8Al steels. However, under an impact loading at similar to 196 degrees C, the major deformation mechanisms are cross twinning and highly dense dislocation walls in the 3Al and 5Al steels, leading to ductile dimpled fracture as well as high impact absorbed energies of similar to 122 and similar to 138 J for the 3Al and 5Al steels, respectively. The toughening modes contain high angle grain boundaries induced deflections of a crack, cross planar defects induced tortuousness of a crack in grain interior and a large plastic deformation dissipating energy. In addition, it is due to the formation of delta-ferrite that the 8Al steel becomes a brittle material at similar to 196 degrees C. The delta-ferrite induced cryogenic brittlement (delta-ICB) effect was sufficiently discussed. (C) 2021 The Author(s). Published by Elsevier B.V.
引用
收藏
页码:947 / 961
页数:15
相关论文
共 62 条
  • [1] Room-temperature cleavage fracture of FeMnAIC steels
    Acselrad, O
    Dille, J
    Pereira, LC
    Delplancke, JL
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (12): : 3863 - 3866
  • [2] The influence of rolling practice on notch toughness and texture development in high-strength linepipe
    Baczynski, GJ
    Jonas, JJ
    Collins, LE
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (12): : 3045 - 3054
  • [3] In situ observations of transgranular crack propagation in high-manganese steel
    Baik, Sung-Il
    Ahn, Tae-Young
    Hong, Woong-Pyo
    Jung, Yeon-Seung
    Lee, Young-Kook
    Kim, Young-Woon
    [J]. SCRIPTA MATERIALIA, 2015, 100 : 32 - 35
  • [4] High Manganese and Aluminum Steels for the Military and Transportation Industry
    Bartlett, Laura
    Van Aken, David
    [J]. JOM, 2014, 66 (09) : 1770 - 1784
  • [5] Hardening by slip-twin and twin-twin interactions in FeMnNiCoCr
    Bonisch, M.
    Wu, Y.
    Sehitoglu, H.
    [J]. ACTA MATERIALIA, 2018, 153 : 391 - 403
  • [6] High manganese austenitic twinning induced plasticity steels: A review of the microstructure properties relationships
    Bouaziz, O.
    Allain, S.
    Scott, C. P.
    Cugy, P.
    Barbier, D.
    [J]. CURRENT OPINION IN SOLID STATE & MATERIALS SCIENCE, 2011, 15 (04) : 141 - 168
  • [7] Interpretation of significant decrease in cryogenic-temperature Charpy impact toughness in a high manganese steel
    Chen, Jun
    Ren, Jia-kuan
    Liu, Zhen-yu
    Wang, Guo-dong
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 737 : 158 - 165
  • [8] Influence of Heat Treatments on the Microstructural Evolution and Resultant Mechanical Properties in a Low Carbon Medium Mn Heavy Steel Plate
    Chen, Jun
    Lv, Meng-Yang
    Liu, Zhen-Yu
    Wang, Guo-Dong
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (05): : 2300 - 2312
  • [9] Current state of Fe-Mn-Al-C low density steels
    Chen, Shangping
    Rana, Radhakanta
    Haldar, Arunansu
    Ray, Ranjit Kumar
    [J]. PROGRESS IN MATERIALS SCIENCE, 2017, 89 : 345 - 391
  • [10] Extra strengthening and work hardening in gradient nanotwinned metals
    Cheng, Zhao
    Zhou, Haofei
    Lu, Qiuhong
    Gao, Huajian
    Lu, Lei
    [J]. SCIENCE, 2018, 362 (6414) : 559 - +