Visualization of strain distribution around fatigue crack developed by low cycle fatigue test in high-strength steels using digital image correlation method for replica films

被引:13
|
作者
Koga, Norimitsu [1 ]
Sakamaki, Yuta [2 ,7 ]
Kaseya, Akihiro [2 ,7 ]
Umezawa, Osamu [3 ,4 ]
Nakata, Hiroshi [5 ]
Toyoda, Shunsuke [6 ]
机构
[1] Kanazawa Univ, Fac Mech Engn, Inst Sci & Engn, Kakumamachi, Kanazawa, Ishikawa 9201192, Japan
[2] Yokohama Natl Univ, Grad Sch Engn, 79-5 Tokiwadai, Yokohama, Kanagawa 2408501, Japan
[3] Yokohama Natl Univ, Fac Engn, 79-5 Tokiwadai, Yokohama, Kanagawa 2408501, Japan
[4] Tech Univ Ostrava, Ctr Adv Innovat Technol, Vysoka Skola Banska, 17 Listopadu 15, Ostrava 70833, Czech Republic
[5] JFE Steel Corp, Kawasaki Ku, 1-1 Minamiwatarida Cho, Kawasaki, Kanagawa 2100855, Japan
[6] JFE Steel Corp, Chiyoda Ku, 2-2-3 Uchisaiwaicho, Tokyo 1000011, Japan
[7] JFE Steel Corp, Tokyo, Japan
关键词
High-strength steel; Low cycle fatigue; Crack initiation; Crack propagation; Strain distribution; Digital image correlation method; Replica method; INDUCED MARTENSITIC-TRANSFORMATION; BEHAVIOR; DEFORMATION; PHASE; ALLOYS; RANGE; MODEL;
D O I
10.1016/j.matchar.2022.111731
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Strain distributions around the fatigue crack during the low cycle fatigue of high-strength ferrite + martensite dual-phase (DP) and tempered martensite (Mt) steels were visualized during cycles from the initial state to the crack initiation and crack propagation using a digital image correlation analysis applied to replica films. The replica film successfully transcribed the microstructure on the specimen surface. Although both the DP and Mt. steels exhibited a high tensile strength, the work-hardening rate of the DP steel was higher than that of Mt. steel. Although the numbers of cycles to failure (Nf) in the DP and Mt. steels were almost the same at the total strain amplitudes (et) of 0.005-0.008 and 0.02-0.03, the Nf in the DP steel was higher than that in the Mt. steel at the et of 0.008-0.02. The cracks were generated and propagated along the high-tensile-strain regions in both steels and were initiated when the accumulated strain along the loading direction exceeded a critical value regardless of the value of et or the steel applied. The increment of the accumulated strain in the Mt. steel was higher than that of the DP steel at the et of 0.01, whereas it was almost the same between those at the et of 0.03. The inhomogeneity of the strain distribution, which was quantitatively evaluated from the histogram of the strain distribution, increased as the number of fatigue cycles increased. The strain was rather inhomogeneously introduced in the Mt. steel in comparison to the DP steel at the et of 0.01, whereas almost no difference in the inhomogeneity of the strain distribution was detected between the steels at the et of 0.03. Thus, the inhomogeneous strain distribution may promote crack initiation and propagation, resulting in a low Nf at the et of 0.008-0.02 in Mt. steel.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Biaxial High Cycle Fatigue of a type 304L stainless steel: Cyclic strains and crack initiation detection by digital image correlation
    Poncelet, M.
    Barbier, G.
    Raka, B.
    Courtin, S.
    Desmorat, R.
    Le-Roux, J. C.
    Vincent, L.
    EUROPEAN JOURNAL OF MECHANICS A-SOLIDS, 2010, 29 (05) : 810 - 825
  • [32] A general scenario of fish-eye crack initiation on the life of high-strength steels in the very high-cycle fatigue regime
    Wang, Chong
    Liu, Yongjie
    Nikitin, Alexander
    Wang, Qingyuan
    Zhou, Min
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (09) : 2183 - 2193
  • [33] High-Strength Reinforcing Steel Bars: Low Cycle Fatigue Behavior Using RGB Methodology
    Jorge E. Egger
    Fabian R. Rojas
    Leonardo M. Massone
    International Journal of Concrete Structures and Materials, 2021, 15
  • [34] High-Strength Reinforcing Steel Bars: Low Cycle Fatigue Behavior Using RGB Methodology
    Egger, Jorge E.
    Rojas, Fabian R.
    Massone, Leonardo M.
    INTERNATIONAL JOURNAL OF CONCRETE STRUCTURES AND MATERIALS, 2021, 15 (01)
  • [35] The correlation of fractal dimension to fracture surface slope for fatigue crack initiation analysis under bending-torsion loading in high-strength steels
    Macek, W.
    Branco, R.
    Podulka, P.
    Nejad, R. Masoudi
    Costa, J. D.
    Ferreira, J. A. M.
    Capela, C.
    MEASUREMENT, 2023, 218
  • [36] High resolution digital image correlation mapping of strain localization upon room and high temperature, high cycle fatigue of a TiAl intermetallic alloy
    Edwards, Thomas Edward James
    Di Gioacchino, Fabio
    Clegg, William John
    INTERNATIONAL JOURNAL OF FATIGUE, 2021, 142
  • [37] Crack closure effects during low cycle fatigue propagation in line pipe steel: An analysis with digital image correlation
    Rabbolini, S.
    Beretta, S.
    Foletti, S.
    Cristea, M. E.
    ENGINEERING FRACTURE MECHANICS, 2015, 148 : 441 - 456
  • [38] Low cycle fatigue life assessment of welded high-strength structural steels based on nominal and local design concepts
    Meoller, Benjamin
    Baumgartner, Joerg
    Wagener, Rainer
    Kaufmann, Heinz
    Melz, Tobias
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 101 : 192 - 208
  • [39] Low cycle fatigue test for solders using non-contact digital image measurement system
    Kanchanomai, C
    Yamamoto, S
    Miyashita, Y
    Mutoh, Y
    McEvily, AJ
    INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (01) : 57 - 67
  • [40] A damage coupled elasto-plastic constitutive model of marine high-strength steels under low cycle fatigue loadings
    Chen, Xipeng
    Yue, Jingxia
    Wu, Xuanfu
    Lei, Jiankang
    Fang, Xuan
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2023, 205