Carbon anode materials from polysiloxanes for lithium ion batteries

被引:24
作者
Ning, LJ
Wu, YP
Wang, LZ
Fang, SB
Holze, R
机构
[1] Chinese Acad Sci, Inst Chem, Beijing 100080, Peoples R China
[2] Tech Univ, AG Elektrochem, Inst Chem, D-09111 Chemnitz, Germany
关键词
lithium ion battery; anode material; disordered carbon; polysiloxane;
D O I
10.1007/s10008-004-0616-8
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Three kinds of silicon-containing disordered carbons have been prepared by pyrolysis of polysiloxanes with different amounts of phenyl side groups. X-ray powder diffraction, X-ray photoelectron spectroscopy and electrochemical capacity measurements were performed to study their behaviors. Graphite crystallites, micropores, and silicon species affect their electrochemical performances. All of them present high reversible capacities, > 372 mAh/g. Since the graphite crystallites are very small, they contribute very little to reversible capacity. The number of micropores produced by gas emission during the heat-treatment process decides whether they exhibit reversible capacity. Si mainly exists in the form C-Si-O and influences the irreversible capacity. There is no evident capacity fading in the first ten cycles, indicating promising properties for these disordered carbons.
引用
收藏
页码:520 / 523
页数:4
相关论文
共 24 条
[1]   KINETICS OF PORE COARSENING IN GLASSY-CARBON [J].
BOSE, S ;
BRAGG, RH .
CARBON, 1981, 19 (04) :289-295
[2]   ALL-SOLID LITHIUM ELECTRODES WITH MIXED-CONDUCTOR MATRIX [J].
BOUKAMP, BA ;
LESH, GC ;
HUGGINS, RA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (04) :725-729
[3]   Electrochemical intercalation of lithium species into disordered carbon prepared by the heat-treatment of poly (p-phenylene) at 650°C for anode in lithium-ion battery [J].
Gong, JB ;
Wu, HQ .
ELECTROCHIMICA ACTA, 2000, 45 (11) :1753-1762
[4]   Si-containing disordered carbons prepared by pyrolysis of pitch polysilane blends: effect of oxygen and sulfur [J].
Larcher, D ;
Mudalige, C ;
George, AE ;
Porter, V ;
Gharghouri, M ;
Dahn, JR .
SOLID STATE IONICS, 1999, 122 (1-4) :71-83
[5]   CHARGE-DISCHARGE CHARACTERISTICS OF THE MESOCARBON MICROBEADS HEAT-TREATED AT DIFFERENT TEMPERATURES [J].
MABUCHI, A ;
TOKUMITSU, K ;
FUJIMOTO, H ;
KASUH, T .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (04) :1041-1046
[6]   New carbon electrodes for secondary lithium batteries [J].
Sandi, G ;
Winans, RE ;
Carrado, KA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (05) :L95-L98
[7]   A MECHANISM OF LITHIUM STORAGE IN DISORDERED CARBONS [J].
SATO, K ;
NOGUCHI, M ;
DEMACHI, A ;
OKI, N ;
ENDO, M .
SCIENCE, 1994, 264 (5158) :556-558
[8]   THERMODYNAMIC PROPERTIES OF LITHIUM-SILICON SYSTEM [J].
SHARMA, RA ;
SEEFURTH, RN .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (12) :1763-1768
[9]   Novel spherical microporous carbon as anode material for Li-ion batteries [J].
Wang, Q ;
Li, H ;
Chen, LQ ;
Huang, XJ .
SOLID STATE IONICS, 2002, 152 :43-50
[10]   LITHIUM INSERTION IN PYROLYZED SILOXANE POLYMERS [J].
WILSON, AM ;
REIMERS, JN ;
FULLER, EW ;
DAHN, JR .
SOLID STATE IONICS, 1994, 74 (3-4) :249-254