A new insight into high-temperature oxidation mechanism of super-austenitic stainless steel S32654 in air

被引:68
作者
Li, Huabing [1 ]
Zhang, Binbin [1 ]
Jiang, Zhouhua [1 ]
Zhang, Shucai [1 ]
Feng, Hao [1 ]
Han, Peide [2 ]
Dong, Nan [2 ]
Zhang, Wei [3 ]
Li, Guoping [3 ]
Fan, Guangwei [3 ]
Lin, Qizeng [3 ]
机构
[1] Northeastern Univ, Sch Met, Shenyang 110819, Peoples R China
[2] Taiyuan Univ Technol, Coll Materials Sci & Engn, Taiyuan 030024, Peoples R China
[3] Taiyuan Iron & Steel Grp Co Ltd, Ctr Technol, Taiyuan 030024, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
Super-austenitic stainless steel; High-temperature oxidation; MoO3; Cr2N; Synergistic effects; PHASE-TRANSFORMATION; CYCLIC DEFORMATION; PROCESSING MAP; BEHAVIOR; MO; MOLYBDENUM; RESISTANCE; MICROSTRUCTURE; CORROSION; ALLOYS;
D O I
10.1016/j.jallcom.2016.06.023
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
High temperature oxidation behavior and mechanisms for super-austenitic stainless steel S32654 were investigated at 900, 1000 and 1200 degrees C in air. The oxide layers were characterized by scanning electron microscopy with energy-dispersive spectroscopy (SEM-EDS), electron-probe microanalysis (EPMA), x-ray diffraction (XRD) and transmission electron spectroscopy (TEM). At 900 degrees C, oxidation follows parabolic law within the initial 10 h, and the external solid MnMoO4 molybdate oxide layer and the internal spinel oxide layer prevent oxygen or metal cations diffusion. The parabolic law then changes to a linear law due to the molten MnMoO4-MoO3 molybdate electrochemical reaction and oxide layer cracking. At 1000 and 1200 degrees C, oxidation follows linear law. The nitrogen in air plays a very important role in accelerating oxidation. The synergistic effects of the molten MnMoO4-MoO3 molybdate electrochemical reaction and discontinuous Cr2N precipitation strongly promote catastrophic oxidation. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:326 / 338
页数:13
相关论文
共 57 条
[1]   Microstructure and oxidation behavior of Nb-Mo-Si-B alloys [J].
Behrani, V ;
Thom, AJ ;
Kramer, MJ ;
Akinc, M .
INTERMETALLICS, 2006, 14 (01) :24-32
[2]  
Birks N., 2010, Introduction to high-temperature oxidation of metals
[3]   CATASTROPHIC OXIDATION OF SOME MOLYBDENUM-CONTAINING ALLOYS [J].
BRENNER, SS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1955, 102 (01) :16-21
[4]   OXIDATION OF IRON-MOLYBDENUM AND NICKEL-MOLYBDENUM ALLOYS [J].
BRENNER, SS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1955, 102 (01) :7-15
[5]   Role of molybdenum on the AISI 316L oxidation at 900°C [J].
Buscail, H. ;
El Messki, S. ;
Riffard, F. ;
Perrier, S. ;
Cueff, R. ;
Issartel, C. .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (21) :6960-6966
[6]   Role of Nitrogen Uptake During the Oxidation of 304L and 904L Austenitic Stainless Steels [J].
Cao, Yu ;
Norell, Mats .
OXIDATION OF METALS, 2013, 80 (5-6) :479-491
[7]   Heating modification of an austenitic steel with high-nitrogen content [J].
Carosi, A. ;
Amati, M. ;
Gregoratti, L. ;
Kaciulis, S. ;
Mezzi, A. ;
Montanari, R. ;
Rovatti, L. ;
Ucciardello, N. .
SURFACE AND INTERFACE ANALYSIS, 2010, 42 (6-7) :726-729
[8]   The role of the surface roughness on the integrity of thermally generated oxide scales. Application to the Al2O3/MA956 system [J].
Chao, J ;
GonzalezCarrasco, JL .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 230 (1-2) :39-48
[9]   Mn coating on AISI 430 ferritic stainless steel by pack cementation method for SOFC interconnect applications [J].
Ebrahimifar, Hadi ;
Zandrahimi, Morteza .
SOLID STATE IONICS, 2011, 183 (01) :71-79
[10]   Critical pitting temperature for Type 254 SMO stainless steel in chloride solutions [J].
El Meguid, E. A. Abd ;
El Latif, A. A. Abd .
CORROSION SCIENCE, 2007, 49 (02) :263-275