摘要
It is known that replacing microscopic particles by nano-particles in a composite formulation results in improved physical properties. The authors investigated the possibility adding of nanoparticles SiO2 and TiO2 in an amount of 10-30% in the slurry to produce glass-ceramics. Mechanical strength of the glass-ceramics parts greatly depends on micro-defects of surface and internal structures substantially connected with the factual quality of used production technology, mechanical and heat treatment. There is analyzed a special complex of the destructive and nondestructive methods of strength and quality control of glass-ceramics developed to guarantee the durability of structures used in the usual and extreme service conditions with the temperature up to 1000 degrees C. The methods based on the precise preproduction tests of specimens and real structural elements such as plates and shells were supplemented with the additional non-standard methods for effective use in the working environment which is typical for line production of super thermal-resistant glass-ceramic. As a result of the research found that the adding of nanoparticles in the slurry increases the density of the structure, improves the physical properties and provides high stability of glass-ceramics. (C) 2011 Published by Elsevier Ltd. Selection and peer-review under responsibility of ICM11
引用
收藏
页码:1463 / 1466
页数:4
相关论文
共 50 条
  • [2] Preparation of Nano-Filled Polypropylene Microfibers
    Rezanova, N. M.
    Mel'nik, I. A.
    Tsebrenko, M. V.
    Korshun, A. V.
    FIBRE CHEMISTRY, 2014, 46 (01) : 21 - 27
  • [3] Preparation of Nano-Filled Polypropylene Microfibers
    N. M. Rezanova
    I. A. Mel´nik
    M. V. Tsebrenko
    A. V. Korshun
    Fibre Chemistry, 2014, 46 : 21 - 27
  • [4] Reinforcement in nano-filled PAA hydrogels
    Kalfus, Jan
    Singh, Naveen
    Lesser, Alan J.
    POLYMER, 2012, 53 (13) : 2544 - 2547
  • [5] GLASS AND GLASS-CERAMICS
    SOGA, N
    AMERICAN CERAMIC SOCIETY BULLETIN, 1982, 61 (09): : 935 - 936
  • [6] GLASS-CERAMICS
    ASHBEE, KGH
    BRITISH JOURNAL OF APPLIED PHYSICS, 1965, 16 (05): : 744 - &
  • [7] GLASS-CERAMICS
    MORLEY, JG
    GLASS TECHNOLOGY, 1965, 6 (05): : 172 - +
  • [8] Glass-Ceramics
    Mehulic, Ketij
    ACTA STOMATOLOGICA CROATICA, 2005, 39 (04) : 477 - 486
  • [9] GLASS-CERAMICS
    不详
    JOURNAL OF NUCLEAR MATERIALS, 1965, 17 (01) : 95 - &
  • [10] GLASS-CERAMICS
    GOTTARDI, V
    CHIMICA & L INDUSTRIA, 1965, 47 (08): : 948 - &