Investigation of the performance decay of anodic PtRu catalyst with working time of direct methanol fuel cells

被引:35
作者
Wang, Zhen-Bo [1 ]
Wang, Xin-Peng [2 ]
Zuo, Peng-Jian [1 ]
Yang, Bo-Qian [2 ]
Yin, Ge-Ping [1 ]
Feng, Xian-Ping [2 ]
机构
[1] Harbin Inst Technol, Dept Appl Chem, Harbin 150001, Peoples R China
[2] Univ Puerto Rico, Dept Phys, San Juan, PR 00931 USA
基金
中国国家自然科学基金;
关键词
direct methanol fuel cell; life test; anodic catalyst degradation; electrochemically active surface area; in situ cyclic voltammetry;
D O I
10.1016/j.jpowsour.2008.03.042
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Life tests of direct methanol fuel cells (DMFC) were carried out with three individual single cells at a current density of 100 mA cm(-2) for three different times under ambient pressure and at a cell temperature of 60 degrees C. X-ray diffraction (XRD) and X-ray photoelectron spectra (XPS) were used to characterize the anodic PtRu catalysts before and after the life tests. XRD results showed that the particle sizes of anodic catalysts increased from an original value of 2.8 to 3.0, 3.2, and 3.3 nm, whereas their lattice parameters first increased and then decreased from an original value of 3.8761 to 3.8879, 3.8777, and 3.8739 A before and after 117, 210, and 312 working hours, respectively. XPS results indicated that during cells' working the contents of Pt and Ru oxides in anodic catalysts increased, but the metal content gradually decreased with test times. Polarization curves, power density curves, and in situ CO-stripping cyclic voltammetric (CV) curves were also plotted to evaluate the performances of fuel cells and electrochemically active surface areas (SEAS) of anodic catalysts before and after life tests. After different time tests, the performances of DMFC lowered to different extents and could not recover their initial performances. The SEAS of anodic catalyst decreased slightly by 4.78 and 9.03 m(2) g(-1) after 117 and 312 working hours, respectively. The utilization of anodic catalysts lowered slightly. This indicates that the change of (SEAS) and utilization of anodic catalysts are not the main factors affecting the performance degradation of DMFC. The dissolution of Ru metal from anodic catalysts surface could be one of the main factors for the performance degradation of the PtRu black catalyst. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:93 / 100
页数:8
相关论文
共 50 条
  • [1] Durability studies of unsupported Pt cathodic catalyst with working time of direct methanol fuel cells
    Wang, Zhen-Bo
    Shao, Yu-Yan
    Zuo, Peng-Jian
    Wang, Xin-Peng
    Yin, Ge-Ping
    JOURNAL OF POWER SOURCES, 2008, 185 (02) : 1066 - 1072
  • [2] Effect of the solvent in the catalyst ink preparation on the properties and performance of unsupported PtRu catalyst layers in direct methanol fuel cells
    Alcaide, Francisco
    Alvarez, Garbine
    Cabot, Pere L.
    Genova-Koleva, Radostina
    Grande, Hans-Juergen
    Miguel, Oscar
    ELECTROCHIMICA ACTA, 2017, 231 : 529 - 538
  • [3] Synthesis and optimization of PtRu/TiO2-CNF anodic catalyst for direct methanol fuel cell
    Abdullah, N.
    Kamarudin, S. K.
    Shyuan, L. K.
    Karim, N. A.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (58) : 30543 - 30552
  • [4] A durable PtRu/C catalyst with a thin protective layer for direct methanol fuel cells
    Shimazaki, Yuzuru
    Hayasaka, Sho
    Koyama, Tsubasa
    Nagao, Daisuke
    Kobayashi, Yoshio
    Konno, Mikio
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2010, 351 (02) : 580 - 583
  • [5] Electrocatalysis in direct methanol fuel cells: in-situ probing of PtRu anode catalyst surfaces
    Dinh, HN
    Ren, XM
    Garzon, FH
    Zelenay, P
    Gottesfeld, S
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2000, 491 (1-2): : 222 - 233
  • [6] Supported PtRu on mesoporous carbons for direct methanol fuel cells
    Arbizzani, Catia
    Beninati, Sabina
    Soavi, Francesca
    Varzi, Alberto
    Mastragostino, Marina
    JOURNAL OF POWER SOURCES, 2008, 185 (02) : 615 - 620
  • [7] Polyol-synthesized PtRu/C and PtRu black for direct methanol fuel cells
    Guo, Junsong
    Sun, Gongquan
    Sun, Shiguo
    Yan, Shiyou
    Yang, Weiqian
    Qi, Jing
    Yan, Yushan
    Xin, Qin
    JOURNAL OF POWER SOURCES, 2007, 168 (02) : 299 - 306
  • [8] Preparation and characterization of a PtRu/C nanocatalyst for direct methanol fuel cells
    Guo, JW
    Zhao, TS
    Prabhuram, J
    Chen, R
    Wong, CW
    ELECTROCHIMICA ACTA, 2005, 51 (04) : 754 - 763
  • [9] Preparation of supported PtRu/C electrocatalyst for direct methanol fuel cells
    Jiang, LH
    Sun, GQ
    Zhao, XS
    Zhou, ZH
    Yan, SY
    Tang, SH
    Wang, GX
    Zhou, B
    Xin, Q
    ELECTROCHIMICA ACTA, 2005, 50 (12) : 2371 - 2376
  • [10] Optimized CeO2 content of the carbon nanofiber support of PtRu catalyst for direct methanol fuel cells
    Kunitomo, Hikari
    Ishitobi, Hirokazu
    Nakagawa, Nobuyoshi
    JOURNAL OF POWER SOURCES, 2015, 297 : 400 - 407