Evolution of structural properties of iron oxide nano particles during temperature treatment from 250 °C-900 °C: X-ray diffraction and Fe K-shell pre-edge X-ray absorption study

被引:82
作者
Bora, Debajeet K. [1 ,2 ]
Braun, Artur [1 ,3 ]
Erat, Selma [1 ,4 ]
Safonova, Olga [5 ]
Graule, Thomas [1 ,6 ]
Constable, Edwin C. [2 ]
机构
[1] Empa, Swiss Fed Labs Mat Sci & Technol, Lab High Performance Ceram, CH-8600 Dubendorf, Switzerland
[2] Univ Basel, Dept Chem, CH-4056 Basel, Switzerland
[3] Univ Hawaii Manoa, Sch Ocean & Earth Sci & Technol, Hawaii Nat Energy Inst, Honolulu, HI 96822 USA
[4] ETH Zurich Swiss Fed Inst Technol, Dept Nonmetall Inorgan Mat, CH-8037 Zurich, Switzerland
[5] European Synchrotron Radiat Facil, F-38043 Grenoble, France
[6] Tech Univ Bergakad Freiberg, D-09596 Freiberg, Germany
基金
瑞士国家科学基金会;
关键词
Nano particle; Iron oxide; XANES; Fe K-shell; ALPHA-FE2O3; NANOPARTICLES; HEMATITE NANOPARTICLES; CRYSTALLITE SIZE; OXIDATION-STATE; SPECTRA; XANES; WATER; TRANSFORMATION; COORDINATION; FERRIHYDRITE;
D O I
10.1016/j.cap.2011.11.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Iron oxide nano particles with nominal Fe2O3 stoichiometry were synthesized by a wet, soft chemical method with heat treatment temperatures from 250 degrees C to 900 degrees C in air. The variation in the structural properties of the nano particles with the heat treatment temperature was studied by X-ray diffraction and Fe K-shell X-ray absorption spectroscopy. X-ray diffractograms show that at lower annealing temperatures the nano particle comprise both maghemite and hematite phases. With increasing temperature, the remainder of the maghemite phase transforms completely to hematite. Profile analysis of the leading Bragg reflections reveals that the average crystallite size increases from 50 nm to 150 nm with increasing temperature. The mean primary particle size decreases from 105 nm to 90 nm with increasing heat treatment temperature. The X-ray diffraction results are paralleled by systematic changes in the pre-edge structure of the Fe K-edge X-ray absorption spectra, in particular by a gradual decrease of the t(2g)/e(g) peak height ratio of the two leading pre-edge resonances, confirming oxidation of the Fe from Fe2+ towards Fe3+. Transmission electron microscopy (TEM) on the samples treated at temperatures as high as 900 degrees C showed particles with prismatic morphology along with the formation of stacking fault like defects. High resolution TEM with selected area electron diffraction (SAED) of samples heat treated above 350 degrees C showed that the nano particles have well developed lattice fringes corresponding to that of (110) plane of hematite. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:817 / 825
页数:9
相关论文
共 54 条
[1]   X-RAY MICROPROBE ANALYSIS OF IRON OXIDATION-STATES IN SILICATES AND OXIDES USING X-RAY-ABSORPTION NEAR-EDGE STRUCTURE (XANES) [J].
BAJT, S ;
SUTTON, SR ;
DELANEY, JS .
GEOCHIMICA ET COSMOCHIMICA ACTA, 1994, 58 (23) :5209-5214
[2]   XANES calibrations for the oxidation state of iron in a silicate glass [J].
Berry, AJ ;
O'Neill, HS ;
Jayasuriya, KD ;
Campbell, SJ ;
Foran, GJ .
AMERICAN MINERALOGIST, 2003, 88 (07) :967-977
[3]   Fatty Acid Binding Domain Mediated Conjugation of Ultrafine Magnetic Nanoparticles with Albumin Protein [J].
Bora, D. K. ;
Deb, P. .
NANOSCALE RESEARCH LETTERS, 2009, 4 (02) :138-143
[4]   COORDINATION OF IRON IN OXIDE GLASSES THROUGH HIGH-RESOLUTION K-EDGE SPECTRA - INFORMATION FROM THE PRE-EDGE [J].
CALAS, G ;
PETIAU, J .
SOLID STATE COMMUNICATIONS, 1983, 48 (07) :625-629
[5]   Size dependent photocatalytic activity of hydrothermally crystallized titania nanoparticles on poorly adsorbing phenol in absence and presence of fluoride ion [J].
Calza, Paola ;
Pelizzetti, Ezio ;
Mogyorsi, Karoly ;
Kun, Robert ;
Dekany, Imre .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2007, 72 (3-4) :314-321
[6]   Fe2O3 nanoparticle structures investigated by X-ray absorption near-edge structure, surface modifications, and model calculations [J].
Chen, LX ;
Liu, T ;
Thurnauer, MC ;
Csencsits, R ;
Rajh, T .
JOURNAL OF PHYSICAL CHEMISTRY B, 2002, 106 (34) :8539-8546
[7]   Size-dependent structural transformations of hematite nanoparticles. 1. Phase transition [J].
Chernyshova, I. V. ;
Hochella, M. F., Jr. ;
Madden, A. S. .
PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2007, 9 (14) :1736-1750
[8]   Nonaqueous synthesis and characterization of capped α-Fe2O3 nanoparticles from iron(III) hydroxy-oleate precursor [J].
Chikate, Rajeev C. ;
Jun, Ki-Won ;
Rode, Chandrasekhar V. .
POLYHEDRON, 2008, 27 (03) :933-938
[9]  
Cornel R.M., 1996, The iron oxides: structure, properties, reactions, occurrences and uses weinheim, V2
[10]   X-RAY-ABSORPTION SPECTROSCOPY AT THE FE L(2,3) THRESHOLD IN IRON-OXIDES [J].
CROCOMBETTE, JP ;
POLLAK, M ;
JOLLET, F ;
THROMAT, N ;
GAUTIERSOYER, M .
PHYSICAL REVIEW B, 1995, 52 (05) :3143-3150