Pressureless sintering of Al2O3/Ni nanocomposites

被引:66
|
作者
Chen, RZ [1 ]
Tuan, WH [1 ]
机构
[1] Natl Taiwan Univ, Inst Mat Sci & Engn, Taipei 10764, Taiwan
关键词
sintering; Al2O3; strength; microstructure-final; nanocomposites;
D O I
10.1016/S0955-2219(98)00213-1
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present study, an Al2O3/Ni nanocomposite containing 5 vol% Ni is prepared by pressureless sintering at 1400 degrees C for 2 h. Most nickel inclusions, around 70% in the sintered nanocomposite, locate at the intergranular sites, the triple junctions and Al2O3/Al2O3 grain boundaries. The average size of the nickel inclusions at the triple junctions, grain boundaries and intragranular locations is 145, 131 and 73 nm, respectively. The average size of all nickel inclusions is 118 nm. The presence of nickel inclusions can prohibit the grain growth of matrix grains. The size of Al2O3 grains in the sintered nanocomposite is only 490 nm. The strength of the nanocomposite is thus high for the refined microstructure. The matrix Al2O3 grains and Ni inclusions at triple junctions underwent considerable coarsening during a post-annealing treatment at 1300 degrees C for 2 h. The strength of the annealed composites is thus reduced significantly after annealing. (C) 1999 Elsevier Science Limited. All rights reserved.
引用
收藏
页码:463 / 468
页数:6
相关论文
共 50 条
  • [1] Pressureless sintering the Al2O3/SiC nanocomposites in deoxidized atmosphere
    Peng, ZZ
    Cai, S
    Wang, YW
    Wu, HZ
    HIGH-PERFORMANCE CERAMICS III, PTS 1 AND 2, 2005, 280-283 : 1093 - 1096
  • [2] Processing and mechanical characterization of Al2O3/Ni and Al2O3/Co composites by pressureless sintering of nanocomposite powders
    Yildiz, Betul Kafkaslioglu
    Yilmaz, Huseyin
    Tur, Yahya Kemal
    PROCESSING AND APPLICATION OF CERAMICS, 2018, 12 (02) : 123 - 128
  • [3] Pressureless sintering of Al2O3/Ni nanocomposites produced by heterogeneous precipitation method with varying nickel contents
    Kafkaslioglu, Betul
    Tur, Yahya Kemal
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2016, 57 : 139 - 144
  • [4] Liquid phase sintering of Al2O3/SiC nanocomposites
    Borsa, CE
    Ferreira, HS
    Kiminami, RHGA
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1999, 19 (05) : 615 - 621
  • [5] Preparation of Al2O3-ZrO2-Ni nanocomposite by pulse electric current and pressureless sintering
    Tuan, WH
    Liu, SM
    Ho, CJ
    Lin, CS
    Yang, TJ
    Zhang, DM
    Fu, ZY
    Guo, JK
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (13) : 3125 - 3133
  • [6] Gelcasting process of Al2O3/Ni nanocomposites
    Kim, BS
    Sekino, T
    Yamamoto, Y
    Nakayama, T
    Kusunose, T
    Wada, A
    Niihara, K
    MATERIALS LETTERS, 2004, 58 (1-2) : 17 - 20
  • [7] Pressureless sintering of Al2O3 containing up to 20 vol% zirconium diboride (ZrB2)
    Postrach, S
    Pötschke, J
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2000, 20 (10) : 1459 - 1468
  • [8] Comparison of different alumina powders for the aqueous processing and pressureless sintering of Al2O3-SiC nanocomposites
    Baron, B
    Kumar, CS
    Le Gonidec, G
    Hampshire, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (9-10) : 1543 - 1552
  • [9] Densification behaviour and microstructure evolution of γ-Al2O3 nanoceramics during pressureless sintering
    Li, D.
    Zhu, H. -L.
    Chen, S. -O.
    Shao, W. -Q.
    Ge, X. -H.
    Zhang, Y. -C.
    Zhang, S. -S.
    MATERIALS TECHNOLOGY, 2008, 23 (03) : 145 - 147
  • [10] Low temperature pressureless sintering of α-SiC with Al2O3 and CeO2 as additives
    Liang, Hanqin
    Yao, Xiumin
    Zhang, Jingxian
    Liu, Xuejian
    Huang, Zhengren
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (03) : 831 - 835