Characterization and Integration Performance of Methyl Silsesquioxane-Based Nano Porous Low-k Dielectric Films

被引:1
作者
Choi, Eunmi [1 ]
Nam, Minwoo [1 ]
Kim, Areum [1 ]
Kang, Keunwon [1 ]
Zheng, Longshou [1 ]
Kwon, Soon Hyeong [1 ]
Yoon, Sung Pil [3 ]
Hahn, Sang June [2 ]
Kim, Soo-Kil [1 ]
Son, Hyungbin [1 ]
Pyo, Sung Gyu [1 ]
机构
[1] Chung Ang Univ, Sch Integrat Engn, Seoul 156756, South Korea
[2] Chung Ang Univ, Dept Phys, Seoul 156756, South Korea
[3] Korea Inst Sci & Technol, Fuel Cell Res Ctr, Seoul 136791, South Korea
关键词
Low-k; Breakdown Strength; Integration; CO2; Plasma Treatment;
D O I
10.1166/jnn.2016.13482
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
We evaluated three kinds of methyl silsesquioxane-based porous spin-on materials with target k values at or below 2.25, prepared under ideal baking and curing conditions. Analysis was carried out to determine the thickness, refractive index, uniformity, chemical signature, k value and mechanical properties (hardness and modulus) of the prepared films. In order to improve the adhesion at the chemical vapor deposited capping layer and porous low-k film interface, plasma treatments were utilized, and modified edge lift-off and chemical mechanical polishing tests were performed to confirm its effectiveness. 1LM integration tests were also carried out to determine metal line resistance, leakage current and breakdown field strength. While the metal line resistance and leakage characteristics were similar, the breakdown field strengths of low k dielectrics were higher than those of nano-porous low-k dielectrics. The evaluation of two kinds of methyl silsesquioxane-based porous low-k dielectrics were achieved with regards to unit processes such as spin coating, etch and chemical mechanical processing, and integration. Adhesion between the porous low-k films and the capping layer was improved by applying CO2 plasma treatment on the low-k material surface before deposition of the capping layer.
引用
收藏
页码:11224 / 11228
页数:5
相关论文
共 50 条
  • [41] Description of the porosity of inhomogeneous porous low-k films using solvent adsorption studied by spectroscopic ellipsometry in the visible range
    Bourgeois, A
    Bruneau, AB
    Jousseaume, V
    Rochat, N
    Fisson, S
    Demarets, B
    Rivory, J
    THIN SOLID FILMS, 2004, 455 : 366 - 369
  • [42] Degradation of the Barrier Integrity of Porous Low-k Dual Damascene Interconnects Using Dual Top Hard Mask Process Integration
    Pyo, Sung Gyu
    Kim, Sang-Young
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 2009, 54 (04) : 1671 - 1674
  • [43] Understanding nitrogen-induced effects on the performance of ultra low-k dielectric systems through ab initio simulations
    Dai, Ling
    Tan, V. B. C.
    Yang, Shuo-Wang
    Wu, Ping
    Chen, Xian-Tong
    SURFACE SCIENCE, 2007, 601 (16) : 3366 - 3371
  • [44] Quantitative mapping of elastic properties of plasma-treated silica-based low-k films
    Jiang, Le
    Geisler, Holm
    Zschech, Ehrenfried
    THIN SOLID FILMS, 2006, 515 (04) : 2230 - 2234
  • [45] Mechanical property determination of thin porous low-k films by twin-transducer laser generated surface acoustic waves
    Xiao, X
    Hata, N
    Yamada, K
    Kikkawa, T
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2004, 43 (02): : 508 - 513
  • [46] Effects of Post-CMP Cleaning on Time Dependent Dielectric Breakdown and Electro-Migration in Porous Low-k/Cu Interconnects
    Hsu, Chia-Lin
    Perng, Dung-Ching
    Lin, Wen-Chin
    Lu, Kuan-Ting
    Tsai, Teng-Chun
    Huang, Climbing
    Wu, J. Y.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2011, 158 (11) : H1133 - H1137
  • [47] Determination of mechanical properties of porous silica low-k films on si substrates using orientation dependence of surface acoustic wave
    Takimura, Toshinori
    Hata, Nobuhiro
    Takada, Syozo
    Yshino, Takenobu
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2008, 47 (07) : 5400 - 5403
  • [48] Variation in process conditions of porogen-based low-k films: A method to improve performance without changing existing process steps in a sub-100 nm Cu damascene integration route
    De Roest, D.
    Travaly, Y.
    Beynet, J.
    Sprey, H.
    Labat, J.
    Huffman, C.
    Verdonck, P.
    Kaneko, S.
    Matsushita, K.
    Kobayashi, N.
    Beyer, G.
    MICROELECTRONIC ENGINEERING, 2010, 87 (03) : 311 - 315
  • [49] Spin coating film transfer and hot-pressing system for uniform dielectric formation and its application to porous low-k film formation
    Kawagoe, Masafumi
    Adachi, Hideki
    Yanagida, Takaaki
    Komura, Tomoyuki
    Saito, Hidenori
    Sato, Norio
    Kudou, Kazuhisa
    Machida, Katsuyuki
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2008, 47 (01) : 113 - 118
  • [50] Quantitative mapping of the elastic properties of electron-beam damaged silica-based low-k films
    Jiang, L
    Geisler, H
    Zschech, E
    MATERIALS SCIENCE-POLAND, 2005, 23 (03): : 643 - 651