Influence of matrix property and interfacial reaction on the mechanical performance and fracture mechanism of TiC reinforced Al matrix lamellar composites

被引:32
作者
Guo, Rui-Fen [1 ,2 ,3 ]
Wang, Ya [1 ,2 ]
Shen, Ping [1 ,2 ]
Shaga, Alateng [4 ]
Ma, Yun-Hai [3 ]
Jiang, Qi-Chuan [1 ,2 ]
机构
[1] Jilin Univ, State Key Lab Automot Simulat & Control, Changchun, Peoples R China
[2] Jilin Univ, Sch Mat Sci & Engn, Key Lab Automobile Mat, Minist Educ, Changchun 130022, Peoples R China
[3] Jilin Univ, Coll Biol & Agr Engn, Changchun, Peoples R China
[4] Jilin Jianzhu Univ, Dept Mat Sci & Engn, Changchun 130118, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 775卷
基金
中国国家自然科学基金;
关键词
Freeze casting; Infiltration; Interfacial reaction; Strength and toughness; Fracture mechanism; METAL; CRACKING; TRANSITION; STRENGTH; FABRICATION; TOUGH; AL3TI;
D O I
10.1016/j.msea.2020.138956
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Freeze casting is a versatile approach for the design of lamellar metal-ceramic composites with unique combination of strength and toughness. However, previous studies mainly focused on ceramic factors such as content and lamellae structure, seldom concerning the effects of metal property and interfacial structures, which, in practice, are key factors in determining the mechanical performances of the composites. In this work, we prepared three kinds of Al/TiC lamellar-interpenetrated composites with different matrix compositions (pure Al, 6061Al (Al-0.4Cu-1.0Mg-0.6Si) and ZL107 (Al-7Si-5Cu)) via freeze casting and pressure infiltration, aiming at clarifying the roles of matrix property and interfacial reaction on the mechanical properties and fracture mechanisms of the composites. The flexural strengths of pure Al/TiC, 6061Al/TiC and ZL107/TiC composites reached 355 +/- 10, 415 +/- 15 and 459 +/- 18 MPa, while the toughness values (characterized by crack-growth toughness) were 81.0 +/- 2.0, 57.6 +/- 1.2 and 43.4 +/- 1.5 MPa M-1/2, respectively. The exceptional damage tolerance of these lamellar composites was attributed to multiple toughening mechanisms such as crack deflection, uncracked-ligament bridging of ductile layers and plastic deformation of the metal matrix. However, the presence of Si in the 6061Al and ZL107 alloys weakened the stability of TiC and promoted interfacial reaction, leading to the formation of a certain number of (Al1-n Si-m)(3)Ti and Al4C3, which greatly weakened the toughness of the composites. Due to the combined effects of alloy plasticity, lamellar-interpenetrated structure and interfacial reaction, the fracture of the materials changed from a multiple cracking mode in the Al/TiC composite to a single crack propagating mode in the 6061Al/TiC and ZL107/TiC composites.
引用
收藏
页数:8
相关论文
共 41 条
[1]  
[Anonymous], MAT SCI TECHNOL
[2]  
[Anonymous], ACTA MAT COMPOS SIN
[3]   Mechanics of bioinspired lamellar structured ceramic/polymer composites: Experiments and models [J].
Askarinejad, Sina ;
Rahbar, Nima .
INTERNATIONAL JOURNAL OF PLASTICITY, 2018, 107 :122-149
[4]   Phase equilibria in the α-Ti-Al-Si region of the Ti-Si-Al system [J].
Bulanova, M ;
Tretyachenko, L ;
Golovkova, M ;
Meleshevich, K .
JOURNAL OF PHASE EQUILIBRIA AND DIFFUSION, 2004, 25 (03) :209-229
[5]   Investigation of the interfacial reaction between multi-walled carbon nanotubes and aluminum [J].
Ci, Lijie ;
Ryu, Zhenyu ;
Jin-Phillipp, Neng Yun ;
Ruehle, Manfred .
ACTA MATERIALIA, 2006, 54 (20) :5367-5375
[6]   Solidification orientation relationships between Al3Ti and TiB2 [J].
Cui, Y. ;
King, D. J. M. ;
Horsfield, A. P. ;
Gourlay, C. M. .
ACTA MATERIALIA, 2020, 186 :149-161
[7]   Nacre-mimetics with synthetic nanoclays up to ultrahigh aspect ratios [J].
Das, Paramita ;
Malho, Jani-Markus ;
Rahimi, Khosrow ;
Schacher, Felix H. ;
Wang, Baochun ;
Demco, Dan Eugen ;
Walther, Andreas .
NATURE COMMUNICATIONS, 2015, 6
[8]   Freezing as a path to build complex composites [J].
Deville, S ;
Saiz, E ;
Nalla, RK ;
Tomsia, AP .
SCIENCE, 2006, 311 (5760) :515-518
[9]   Ice-templated porous alumina structures [J].
Deville, Sylvain ;
Saiz, Eduardo ;
Tomsia, Antoni P. .
ACTA MATERIALIA, 2007, 55 (06) :1965-1974
[10]   Different elements-induced destabilisation of TiC and its application on the grain refinement of Mg-Al alloys [J].
Ding, Haimin ;
Li, Hui ;
Liu, Xiangfa .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 485 (1-2) :285-289