Spark plasma sintering processed α-SiAlON bonded tungsten carbide: Densification, microstructure and tribomechanical properties

被引:6
|
作者
Sarkar, Soumya [1 ]
Biswas, Mita [1 ]
Halder, Rupa [1 ]
Bandyopadhyay, Siddhartha [1 ]
机构
[1] CSIR, Cent Glass & Ceram Res Inst, 196 Raja SC Mullick Rd, Kolkata 700032, WB, India
关键词
WC; alpha-SiAlON; Microstructure; Mechanical properties; Tribology; SLIDING WEAR BEHAVIOR; MECHANICAL-PROPERTIES; CEMENTED CARBIDES; TRIBOLOGICAL PROPERTIES; COMPOSITES; CERAMICS; SIZE; TEMPERATURE; TOUGHNESS; MGO;
D O I
10.1016/j.matchemphys.2020.122955
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Processing, microstructure and tribomechanical performance of spark plasma sintering (SPS) processed alpha-SiAlON bonded tungsten carbide (WC) have been reported. SPS at 1750 degrees C under 40 MPa for 25 min resulted in almost theoretically dense composites. Microstructure analysis using scanning and transmission electron microscopy revealed formation of principally micron sized, equiaxed WC grains surrounded by sub-micron to micron sized alpha-SiAlON having both equiaxed (higher concentration) and elongated (lower concentration) grain morphology. Sharp and clean WC/alpha-SiAlON interface regions were noticed without any interfacial reaction product. As evidenced from elemental mapping under HAADF-STEM, the alpha-SiAlON grain boundary region was found to be rich in yttrium and oxygen, whereas, presence of characteristics elements were identified in alpha-SiAlON and WC grains. Addition of alpha-SiAlON in WC matrix resulted in progressive improvement in tribomechanical performance of the composites compared to pure WC. The 40 wt% alpha-SiAlON bonded WC matrix composite offered almost 30-33% higher Vickers hardness and toughness than those obtained for pure WC. Three point flexural strength of the 40 wt% alpha-SiAlON/WC composite was found to be around 425 MPa. Unlubricated wear tests also indicated significantly higher damage of hard and tough beta-Si3N4 ball when sliding against the composites compared to pure WC. Formation of progressively thicker and adherent tribolayer containing broken particles of WC and alpha-SiAlON having sharp edges was possibly the primary reason that caused severe abrasive wear of the counterbody. Results indicated the efficacy of SPS processed alpha-SiAlON bonded WC composites having improved tribomechanical performance over conventional monolithic WC.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Spark plasma sintering of ceramic matrix composite of TiC: microstructure, densification, and mechanical properties: a review
    Oguntuyi, Samson D.
    Johnson, Oluwagbenga T.
    Shongwe, Mxolisi B.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 116 (1-2): : 69 - 82
  • [32] Deposition of silicon carbide/titanium carbide laminar ceramics by electrophoresis and densification by spark plasma sintering
    You, C
    Jiang, DL
    Tan, SH
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (04) : 759 - 761
  • [33] Effect of ZrC nano-powder addition on the microstructure and mechanical properties of binderless tungsten carbide fabricated by spark plasma sintering
    Ren, Xiaoyong
    Peng, Zhijian
    Wang, Chengbiao
    Fu, Zhiqiang
    Qi, Longhao
    Miao, Hezhuo
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2015, 48 : 398 - 407
  • [34] Densification of short carbon fiber reinforced silicon carbide by spark plasma sintering
    Shen, Q
    Li, R
    Wang, CB
    Zhang, LM
    COMPOSITE MATERIALS III, 2003, 249 : 133 - 135
  • [35] Ultra-fast densification of boron carbide by flash spark plasma sintering
    Niu, Bo
    Zhang, Fan
    Zhang, Jinyong
    Ji, Wei
    Wang, Weimin
    Fu, Zhengyi
    SCRIPTA MATERIALIA, 2016, 116 : 127 - 130
  • [36] Kinetics of Densification and Grain Growth of Pure Tungsten During Spark Plasma Sintering
    Zhipeng Gao
    Giuseppe Viola
    Ben Milsom
    Iain Whitaker
    Haixue Yan
    Mike J. Reece
    Metallurgical and Materials Transactions B, 2012, 43 : 1608 - 1614
  • [37] Densification and properties of WC-CoCrFeNi/Co cemented carbide fabricated via spark plasma sintering
    Kang, Kejia
    Yu, Bo
    Liu, Shihua
    Wu, Lan
    Hu, Sumeng
    Tu, Rong
    Luo, Guoqiang
    Wei, Ronghan
    CERAMICS INTERNATIONAL, 2024, 50 (24) : 52356 - 52368
  • [38] Kinetics of Densification and Grain Growth of Pure Tungsten During Spark Plasma Sintering
    Gao, Zhipeng
    Viola, Giuseppe
    Milsom, Ben
    Whitaker, Iain
    Yan, Haixue
    Reece, Mike J.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2012, 43 (06): : 1608 - 1614
  • [39] Spark plasma sintering of pure tungsten powder: Densification kinetics and grain growth
    Deng, Shenghua
    Yuan, Tiechui
    Li, Ruidi
    Zeng, Fanhao
    Liu, Guanghong
    Zhou, Xiang
    POWDER TECHNOLOGY, 2017, 310 : 264 - 271
  • [40] The spall strength of silicon carbide and boron carbide ceramics processed by spark plasma sintering
    Paris, V.
    Frage, N.
    Dariel, M. P.
    Zaretsky, E.
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2010, 37 (11) : 1092 - 1099