Effect of Solidification Conditions on the Deformation Behavior of Pure Copper Castings

被引:2
|
作者
Goto, Ikuzo [1 ]
Aso, Setsuo [1 ]
Ohguchi, Ken-ichi [1 ]
Kurosawa, Kengo [2 ]
Suzuki, Hiroyuki [3 ]
Hayashi, Hiroyuki [3 ]
Shionoya, Jun-ichi [3 ]
机构
[1] Akita Univ, Grad Sch Engn Sci, Dept Mat Sci, Akita 0108502, Japan
[2] Akita Ind Technol Ctr, Akita 0101623, Japan
[3] Sanwa Tekki Corp, Tokyo 1408669, Japan
关键词
pure copper; casting; chill; uniform elongation; dissolved gas; porosity;
D O I
10.2320/jinstmet.J2018031
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The effect of solidification conditions on the tensile deformation behavior of pure copper castings for electrical parts was investigated. Two main types of tensile deformation properties were distinguished on the basis of the difference in uniform elongation. For the castings fabricated under a superheat of 100 degrees C or 150 degrees C, larger and smaller uniform elongation types corresponded to the absence and presence, respectively, of the Cu-Cu2O eutectic phase in the microstructure. Meanwhile, for the castings fabricated under a superheat of 50 degrees C, greater uniform elongation was sometimes obtained when the eutectic phase was present. In addition, irrespective of the presence or absence of the eutectic phase, greater uniform elongation was always obtained when chills were used. Cross-sectional observations showed the existence of considerable nonspherical porosity when the eutectic phase was present; the porosity was reduced when the pouring was conducted under the superheat of 50 degrees C and when the chills were used because of lower hydrogen content in the melt and supersaturation of the hydrogen by rapid cooling, respectively. These results suggest that not only the presence of the eutectic phase but also the inferior casting soundness due to the existence of the porosity is a dominant factor responsible for the decrease in the uniform elongation. The findings presented here indicate that a decrease in the hydrogen content in the melt and/or the rapid cooling during solidification are effective measures to stably achieve practically sufficient deformation properties along with superior casting soundness.
引用
收藏
页码:423 / 430
页数:8
相关论文
共 50 条
  • [1] Effect of Solidification Conditions on the Deformation Behavior of Pure Copper Castings
    Goto, Ikuzo
    Aso, Setsuo
    Ohguchi, Ken-ichi
    Kurosawa, Kengo
    Suzuki, Hiroyuki
    Hayashi, Hiroyuki
    Shionoya, Jun-ichi
    MATERIALS TRANSACTIONS, 2019, 60 (01) : 2 - 9
  • [2] Factor Influencing Deformation Behavior of Pure Copper Castings for Electrical Parts
    Goto, Ikuzo
    Kurosawa, Kengo
    Ohguchi, Ken-ichi
    Aso, Setsuo
    Suzuki, Hiroyuki
    Hayashi, Hiroyuki
    Shionoya, Jun-ichi
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2015, 79 (10) : 511 - 517
  • [3] Deformation Behavior of Pure Copper Castings with As-Cast Surfaces for Electrical Parts
    Ikuzo Goto
    Setsuo Aso
    Ken-ichi Ohguchi
    Kengo Kurosawa
    Hiroyuki Suzuki
    Hiroyuki Hayashi
    Jun-ichi Shionoya
    Journal of Materials Engineering and Performance, 2019, 28 : 3835 - 3843
  • [4] Deformation Behavior of Pure Copper Castings with As-Cast Surfaces for Electrical Parts
    Goto, Ikuzo
    Aso, Setsuo
    Ohguchi, Ken-ichi
    Kurosawa, Kengo
    Suzuki, Hiroyuki
    Hayashi, Hiroyuki
    Shionoya, Jun-ichi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (07) : 3835 - 3843
  • [5] Factors Influencing Deformation Behavior and Electrical Conductivity of Pure Copper Castings Fabricated by Industrial Process
    Goto, Ikuzo
    Aso, Setsuo
    Ohguchi, Ken-ichi
    Oguri, Hayato
    Kurosawa, Kengo
    Suzuki, Hiroyuki
    Hayashi, Hiroyuki
    Shionoya, Jun-ichi
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2017, 81 (03) : 133 - 142
  • [6] Size Effect on Deformation Behavior and Fracture in a Pure Copper Microtensile Test
    Zhang, H. M.
    Chen, R.
    Jing, V
    Li, N.
    Jiang, Z. Y.
    STRENGTH OF MATERIALS, 2021, 53 (04) : 539 - 549
  • [7] Size Effect on Deformation Behavior and Fracture in a Pure Copper Microtensile Test
    H. M. Zhang
    R. Chen
    V. Jing
    N. Li
    Z. Y. Jiang
    Strength of Materials, 2021, 53 : 539 - 549
  • [8] Compression Deformation Behavior and Processing Map of Pure Copper
    S. H. Huang
    S. X. Chai
    X. S. Xia
    Q. Chen
    D. Y. Shu
    Strength of Materials, 2016, 48 : 98 - 106
  • [9] Compression Deformation Behavior and Processing Map of Pure Copper
    Huang, S. H.
    Chai, S. X.
    Xia, X. S.
    Chen, Q.
    Shu, D. Y.
    STRENGTH OF MATERIALS, 2016, 48 (01) : 98 - 106
  • [10] Effect of Initial Grain Size on the Hot Deformation Behavior and Microstructural Evolution of Pure Copper
    Ashtiani, H. R. Rezaei
    Shayanpoor, A. A.
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2022, 35 (04) : 662 - 678