Effects of postbake on the microstructure and whisker growth of matte Sn finish

被引:0
|
作者
Yu, C. H. [1 ]
Kang, H. S. [1 ]
Kim, K. S. [2 ]
Han, S. W. [3 ]
Yang, K. C. [3 ]
机构
[1] Elect & Telecommun Res Inst, Opt Commun Res Ctr, Kwangju 500480, South Korea
[2] Yeojoo Inst Tech, Yeojoo 469, South Korea
[3] Chung Ang Univ, Sch Mech Engn, Seoul 156756, South Korea
来源
2007 12TH INTERNATIONAL SYMPOSIUM ON ADVANCED PACKAGING MATERIALS: PROCESSES, PROPERTIES, AND INTERFACES | 2007年
关键词
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of postbake treatment on a pure matte Sn-plated copper leadframes under high temperature and humidity conditions were investigated. The samples were divided into two categories: those without postbake treatment (WOPB) and those with postbake treatment (WPB), which exposed at 125 square for 1 hour. The X-ray intensity decreased through all crystal orientations after the postbake treatment. For matte Sn-plated Cu leadframes stored at 55 degrees C/85%RH for 1800 hours, nodule-shaped whiskers were observed on samples WOPB, while none were on samples WPB. The WPB samples have a regular layer of IMCs approximately 27% narrower than the WOPB samples. The IMCs had two distinct layers divided into large-grains and small-grains. The large-grain layers located on the Sri side grew before the small-grain layers. The IMCs in the WOPB and WPB samples were identified as Cu6Sn5 and eta-CU6.26Sn5. IMC precipitates were also observed at the grain boundaries and some IMC precipitates were embedded at the Sri matrix. No Cu3Sn or Kirkendall voids were observed at the interface between the Sri and Cu.
引用
收藏
页码:65 / +
页数:3
相关论文
共 50 条
  • [21] Characteristics of tin whisker growth on matte tin surface finishes by acceleration conditions
    Zhao, Fang
    Wang, Qian
    Lee, Taekoo
    ICEPT: 2007 8TH INTERNATIONAL CONFERENCE ON ELECTRONICS PACKAGING TECHNOLOGY, PROCEEDINGS, 2007, : 254 - 257
  • [22] Optimum Thickness of Sn Film for Whisker Growth
    Jing Cheng
    Fuqian Yang
    Paul T. Vianco
    Bei Zhang
    James C.M. Li
    Journal of Electronic Materials, 2011, 40 : 2069 - 2075
  • [23] Stress analysis of spontaneous Sn whisker growth
    K. N. Tu
    Chih Chen
    Albert T. Wu
    Journal of Materials Science: Materials in Electronics, 2007, 18 : 269 - 281
  • [24] Sn corrosion and its influence on whisker growth
    Osenbach, J. W.
    DeLucca, J. M.
    Potteiger, B. D.
    Amin, A.
    Shook, R. L.
    Baiocchi, F. A.
    IEEE TRANSACTIONS ON ELECTRONICS PACKAGING MANUFACTURING, 2007, 30 (01): : 23 - 35
  • [25] Whisker Growth From Sn Solder Alloys
    Crandall, E. R.
    Flowers, G. T.
    Lan, P.
    Bozack, M. J.
    PROCEEDINGS OF THE 2012 IEEE 14TH ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE, 2012, : 671 - 675
  • [26] Sn whisker growth during thermal cycling
    Suganuma, Katsuaki
    Baated, Alongheng
    Kim, Keun-Soo
    Hamasaki, Kyoko
    Nemoto, Norio
    Nakagawa, Tsuyoshi
    Yamada, Toshiyuki
    ACTA MATERIALIA, 2011, 59 (19) : 7255 - 7267
  • [27] Tin whisker growth on electroplated Sn multilayers
    Ting Liu
    Dongyan Ding
    Yu Hu
    Yihua Gong
    Journal of Materials Science: Materials in Electronics, 2015, 26 : 6411 - 6418
  • [28] Tin Whisker Growth on Electroplating Sn Bilayer
    Liu, Ting
    Ding, Dongyan
    Hu, Yu
    Gong, Yihua
    2013 14TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2013, : 931 - +
  • [29] Tin whisker growth on electroplated Sn multilayers
    Liu, Ting
    Ding, Dongyan
    Hu, Yu
    Gong, Yihua
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2015, 26 (09) : 6411 - 6418
  • [30] Stress analysis of spontaneous Sn whisker growth
    Tu, K. N.
    Chen, Chih
    Wu, Albert T.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2007, 18 (1-3) : 269 - 281