Glass welding technology using ultra short laser pulses

被引:7
作者
Roth, Stephan [1 ,4 ]
Cvecek, Kristian [1 ]
Miyamoto, Isamu [2 ,4 ]
Schmidt, Michael [1 ,3 ,4 ]
机构
[1] Bayer Laserzentrum GmbH, Konrad Zuse Str 2-6, D-91052 Erlangen, Germany
[2] Osaka Univ, Suita, Osaka 5650871, Japan
[3] Lehrstuhl Photon Tech, D-91052 Erlangen, Germany
[4] Univ Erlangen Nurnberg, Erlangen Grad Sch Adv Opt Technol, Erlangen, Germany
来源
LASER APPLICATIONS IN MICROELECTRONIC AND OPTOELECTRONIC MANUFACTURING (LAMOM) XVI | 2011年 / 7920卷
关键词
joining; glass welding; material processing; laser processing; ultra-fast lasers;
D O I
10.1117/12.881183
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Glass welding by ultra short laser pulses is a highly promising method to fusion weld glass pieces since it does not need an absorber or pre- and post-heating processes when compared to other laser fusion welding processes. This method utilizes strongly focused ultra short pulses that generate localized plasma which heats and melts the adjacent material. If the plasma region is sufficiently localized the stresses induced by plasma and heat can be tolerated so that defect-free joining of the brittle glass material can be accomplished. This paper gives an overview on the process and shows the advantages and limitations of this joining technology. A method that allows to determine the bonding energy of the welding seams is presented along with measurement results.
引用
收藏
页数:11
相关论文
共 22 条
[1]  
[Anonymous], 2010, PHYS CHEM DENSITY ST
[2]  
[Anonymous], 8505 DIN 1
[3]  
Arata Y, 1976, P 7 INT C ELECT ION, P111
[4]  
Bagdahn J., 1997, ECS ELECTROCHEMICAL, p[97, 285]
[5]  
Banse H., 2005, THESIS U JENA
[6]  
Cvecek K., 2010, GLASS WELDING ULTRAS
[7]   Defect formation in glass welding by means of ultra short laser pulses [J].
Cvecek, Kristian ;
Alexeev, Ilya ;
Miyamoto, Isamu ;
Schmidt, Michael .
LASER ASSISTED NET SHAPE ENGINEERING 6, PROCEEDINGS OF THE LANE 2010, PART 1, 2010, 5 :495-502
[8]   Laser-matter interaction in the bulk of a transparent solid: Confined microexplosion and void formation [J].
Gamaly, Eugene G. ;
Juodkazis, Saulius ;
Nishimura, Koichi ;
Misawa, Hiroaki ;
Luther-Davies, Barry .
PHYSICAL REVIEW B, 2006, 73 (21)
[9]   Optical contact and van der Waals interactions: the role of the surface topography in determining the bonding strength of thick glass plates [J].
Greco, V ;
Marchesini, F ;
Molesini, G .
JOURNAL OF OPTICS A-PURE AND APPLIED OPTICS, 2001, 3 (01) :85-88
[10]  
Grunwald F., 1985, FERTIGUNGSVERFAHREN