Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel

被引:197
作者
Jin, T. Y. [1 ]
Liu, Z. Y. [1 ]
Cheng, Y. F. [1 ]
机构
[1] Univ Calgary, Dept Mech & Mfg Engn, Calgary, AB T2N 1N4, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Microstructure; Inclusions; APISL X100 steel; Pipelines; Hydrogen-induced cracking; MICROSTRUCTURE;
D O I
10.1016/j.ijhydene.2010.05.089
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this work, the type, composition and distribution of inclusions contained in an API5L X100 steel were characterized by scanning electron microscopy and energy-dispersive x-ray analysis. A hydrogen-charging at various current densities was used to introduce hydrogen into the steel, and the correlation between HIC and the inclusions was established. The microstructure of the steel consists of a leather-like bainitic ferrite matrix, with martensite/austenite as the second phase particles. At least four types of inclusions are contained in APISL X100 steel, elongated MnS inclusions and spherical Al-, Si- and Ca-Al-OS-enriched inclusions. In particular, the majority of inclusions in the steel are Al-enriched. Upon hydrogen-charging, hydrogen blisters and HIC could be caused in the steel in the absence of external stress. The cracks are primarily associated with the Al- and Si-enriched inclusions, rather than the elongated MnS inclusion. The critical amount of hydrogen resulting in HIC of the tested API5L X100 steel is determined to be 3.24 ppm under condition in this work. (C) 2010 Professor T. Nejat Veziroglu. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:8014 / 8021
页数:8
相关论文
共 18 条
[1]  
Ciszewski A., 1977, SCC HE IRON BASE ALL
[2]  
Corbett KT, 2004, INT J OFFSHORE POLAR, V14, P75
[3]  
de Abreu L.C., 2009, WELDING INT, V9, P26, DOI [10.1080/09507119509548747, DOI 10.1080/09507119509548747]
[4]   Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking [J].
Dong, C. F. ;
Liu, Z. Y. ;
Li, X. G. ;
Cheng, Y. F. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (24) :9879-9884
[5]   Hydrogen-induced cracking and healing behaviour of X70 steel [J].
Dong, C. F. ;
Li, X. G. ;
Liu, Z. Y. ;
Zhang, Y. R. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 484 (1-2) :966-972
[6]  
Glover A., 2003, P 22 INT C OFFSH MEC
[7]   Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels [J].
Kim, Wan Keun ;
Koh, Seong Ung ;
Yang, Boo Young ;
Kim, Kyoo Young .
CORROSION SCIENCE, 2008, 50 (12) :3336-3342
[8]  
Kudrin VA, 1985, STEELMAKING
[9]  
ORIANI RA, 1984, HYDROGEN DEGRADATION
[10]   Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel [J].
Park, Gyu Tae ;
Koh, Sung Ung ;
Jung, Hwan Gyo ;
Kim, Kyoo Young .
CORROSION SCIENCE, 2008, 50 (07) :1865-1871