Low temperature degradation of single layers of multilayered zirconia in comparison to conventional unshaded zirconia: Phase transformation and flexural strength

被引:47
|
作者
Wille, Sebastian [1 ]
Zumstrull, Paul [1 ]
Kaidas, Victor [2 ]
Jessen, Lea Katharina [2 ]
Kern, Matthias [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, Kiel, Germany
[2] Christian Albrechts Univ Kiel, Fac Engn, Inst Mat Sci, Funct Nanomat, Kiel, Germany
关键词
zirconia; Biaxial flexural strength; Phase transformation; Shading particles; CERAMIC FEMORAL-HEAD; Y-TZP ZIRCONIA; MONOLITHIC ZIRCONIA; DENTAL ZIRCONIA; AIR-ABRASION; SURFACE CHARACTERISTICS; MECHANICAL-PROPERTIES; TRANSLUCENT ZIRCONIA; CATASTROPHIC FAILURE; FRACTURE STRENGTH;
D O I
10.1016/j.jmbbm.2017.09.010
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: The aim of this study was to evaluate the transformation of yttrium stabilized tetragonal zirconia (YTZP) to monoclinic phase and its change in flexural strength of the various layers of multilayered zirconia (enamel layer, transition layer 1, transition layer 2 and body layer) in comparison to two conventional zirconia ceramics. Additionally, the ball-on-three-balls test was compared with a conventional biaxial flexural strength test. Methods: The crystallographic structure of the four layers of Katana Zirconia ML (Kuraray), e.max ZirCAD (Ivoclar Vivadent) and Lava Plus (3M ESPE) was investigated by x-ray-diffraction before and after hydrothermal aging in an autoclave for 5, 10, 15 and 20 h. The biaxial flexural strength was examined with a piston-on-three ball test and a ball-on-three-balls test. Results: There was a significant difference of the ratio of transformation with respect to the tested materials, also between the four different layers of multilayered zirconia. After 20 h of hydrothermal aging the mean ratio of monoclinic phase ranged from 9.9 vol% (LAVA Plus) to 44.2 vol% (Katana Zirconia ML, enamel layer). However, hydrothermal aging had no significant influence on the flexural strength of any material. Furthermore, the flexural strength measured by the ball-on-three-balls test was higher than that measured by the piston-on-three ball test. Conclusion: A ratio of 40% monoclinic phase at the surface did not significantly influence the biaxial flexural strength. Both test methods provide reliable results. However, as the ball-on-three balls test is less dependent on surface roughness, it might be preferred for investigations adapted to clinical reality.
引用
收藏
页码:171 / 175
页数:5
相关论文
共 29 条
  • [1] Effect of sintering condition and low-temperature degradation on the flexural strength and phase transformation of zirconia
    Kong, Moon-Chun
    Park, Mi-Gyoung
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (05) : 692.e1 - 692.e14
  • [2] The effect of surface treatment and low-temperature degradation on flexural strength of additive manufactured zirconia
    Kim, So-Hyun
    Oh, Nam -Sik
    Pang, Nan-Sim
    Jung, Bock-Young
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 148
  • [3] Effects of Silica Coating by Physical Vapor Deposition and Repeated Firing on the Low-Temperature Degradation and Flexural Strength of a Zirconia Ceramic
    Cakir-Omur, Tutku
    Gozneli, Rifat
    Ozkan, Yasemin
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (01): : E186 - E194
  • [4] Effect of low-temperature degradation treatment on hardness, color, and translucency of single layers of multilayered zirconia
    Park, Mi-Gyoung
    JOURNAL OF PROSTHETIC DENTISTRY, 2025, 133 (01) : 258 - 263
  • [5] The effects of surface grinding and polishing on the phase transformation and flexural strength of zirconia
    Lee, Ji-Young
    Jang, Geun-Won
    Park, In-Im
    Heo, Yu-Ri
    Son, Mee-Kyoung
    JOURNAL OF ADVANCED PROSTHODONTICS, 2019, 11 (01) : 1 - 6
  • [6] Effect of low-temperature degradation on the fatigue performance of dental strength-gradient multilayered zirconia restorations
    Li, Qiulan
    Yang, Yunxu
    Chen, Kuangyao
    Jiang, Yingyu
    Swain, Michael, V
    Yao, Mianfeng
    He, Ying
    Liang, Yujie
    Jian, Yutao
    Zhao, Ke
    JOURNAL OF DENTISTRY, 2024, 142
  • [7] Composition, phase analysis, biaxial flexural strength, and fatigue of unshaded versus shaded Procera zirconia ceramic
    Spyropoulou, Panagiota-Eirini
    Kamposiora, Phophi
    Eliades, George
    Papavasiliou, George
    Razzoog, Michael E.
    Thompson, Jeffrey Y.
    Smith, Robert L.
    Bayne, Stephen C.
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 116 (02) : 269 - 276
  • [8] Fatigue strength of bilayer yttria-stabilized zirconia after low-temperature degradation
    Pereira, Raissa Monteiro
    Belli, Renan
    Lohbauer, Ulrich
    Hurle, Katrin
    Campos, Tiago Moreira Bastos
    Thim, Gilmar Patrocinio
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2024, 160
  • [9] Influence of a surface conditioner to pre-sintered zirconia on the biaxial flexural strength and phase transformation
    Sawada, Tomofumi
    Schille, Christine
    Zoldfoldi, Judit
    Schweizer, Ernst
    Geis-Gerstorfer, Juergen
    Spintzyk, Sebastian
    DENTAL MATERIALS, 2018, 34 (03) : 486 - 493
  • [10] Effect of air-abrasion at pre- and/or post-sintered stage and hydrothermal aging on surface roughness, phase transformation, and flexural strength of multilayered monolithic zirconia
    Yilmaz, Ali Dogus
    Okutan, Yener
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2021, 109 (04) : 606 - 616